journal article·1979-09

Multibarrier Kinetics of Brittle Fracture: I, Stress Dependence of the Subcritical Crack Velocity

S. D. BROWN

Publisher page

Abstract

A general equation for the subcritical crack velocity in brittle materials is derived using steady‐state, multibarrier kinetics. It provides a basis from which specialized expressions can be developed for the crack velocity in specific cases. One social equation for v=v(K) at constant temperature, derived from the general expression, has a mathematic form that fits data representative of a wide variety of specific cases. Examples are presented and the equation is discussed in terms of its physical foundations.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-pressure geophysics and materials · Concrete and Cement Materials Research · Thermal and Kinetic Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (82)

Show source-provided references
1. Charles R. J. · 1962 · 511
2. Hillig W. B. · 1965 · 682
3. Wiederhorn S. M. · 1966 · 503
4. 10.1111/j.1151-2916.1967.tb15145.x10.1111/j.1151-2916.1967.tb15145.x ↗
5. Fracture of Glass in vacuum
6. Freiman S. W. · “Effect of Alcohol on Crack Propagation in Glass · 20 · 350
7. 10.1098/rspa.1964.021010.1098/rspa.1964.0210 ↗
8. Plastic Flow‐Slow Crack Propagation and Static Fatigue in Glass
9. 10.1111/j.1151-2916.1970.tb15962.x10.1111/j.1151-2916.1970.tb15962.x ↗
10. Effect of Electrolyte pH on Crack Propagation in Glass
11. 10.1007/978-1-4615-7014-1_1710.1007/978-1-4615-7014-1_17 ↗
12. 10.1111/j.1151-2916.1974.tb10910.x10.1111/j.1151-2916.1974.tb10910.x ↗
13. Highlight of Progress in the Science of Fracture of Ceramics and Glass
14. 10.1016/0022-3093(75)90083-610.1016/0022-3093(75)90083-6 ↗
15. 'The Charles‐Hillig Subcritical Velocity Reconsidered
16. 10.1063/1.172381210.1063/1.1723812 ↗
17. 10.1111/j.1151-2916.1951.tb11637.x10.1111/j.1151-2916.1951.tb11637.x ↗
18. Dependence of Ultimate Strength of Glass Under Constant Load on Temperature. Ambient Atmosphere, and Time
19. Bartemev G. M. · 1955 · 53
20. Theory of Spontaneous Dispersion of Solid
21. Barteney G. M. · 1966 · 1871
22. Kinetic Concept of the Strength of Solids10.1007/BF03545562 ↗
23. 10.1063/1.304810210.1063/1.3048102 ↗
24. Krausz A. S. · 1975
25. 10.1007/978-1-4684-2643-4_1410.1007/978-1-4684-2643-4_14 ↗
26. 10.1016/0025-5416(71)90076-010.1016/0025-5416(71)90076-0 ↗
27. R.Duttonpp647–57in Ref 10.
28. 10.1063/1.166069910.1063/1.1660699 ↗
29. Lattice Theory of Fracture and Crack Creep
30. Thomson R. · 1974 · 283
31. 10.1007/BF0054369210.1007/BF00543692 ↗
32. 10.1007/BF0003698110.1007/BF00036981 ↗
33. 10.1111/j.1151-2916.1976.tb10952.x10.1111/j.1151-2916.1976.tb10952.x ↗
34. Schoenert K. · 1969 · 474
35. Growth Kinetics in Cracks in Glass
36. Ree F. H. · 1962 · 1
37. Eyring H. · 1962 · 1
38. Eyring H. · 1962
39. Rodiguin N. M. · 1964
40. Condit R. H · 1969 · 284
41. 10.1007/BF0060339010.1007/BF00603390 ↗
42. 10.1007/978-1-4615-8723-1_1510.1007/978-1-4615-8723-1_15 ↗
43. Churchill S. W. · 1974
44. 10.1007/BF0003238110.1007/BF00032381 ↗
45. A. S.Krausz “The Theory of the Thermally Activated Processes of Stress Corrosion Cracking”: submitted to Engineering; Fracture Mechanics..
46. Glasstone S. · 1941
47. Jeans J. H. · 1921
48. Chapman S. · 1929
49. Sherwood T. K. · 1952
50. Hirschfelder J. O. · 1954 · 539
51. Samaras D. G. · 1962 · 318
52. Stresses in a Plate Due to the Presence of Cracks and Sharp Corners
53. 10.1115/1.401154710.1115/1.4011547 ↗
54. Fracture Toughness Testing and Its Applications
55. Brown S.D. · 1978 · 597
56. Shewmon P. G. · 1963
57. Bardeen J. · 1951 · 87
58. 10.1103/PhysRev.37.40510.1103/PhysRev.37.405 ↗
59. 10.1111/j.1151-2916.1976.tb10938.x10.1111/j.1151-2916.1976.tb10938.x ↗
60. Strength and Static Fatigue of Abraded Glass Under Controlled Ambient Condition
61. Sedlacek R. · 1968 · 211
62. 10.1007/BF0055019610.1007/BF00550196 ↗
63. Swann P. R. · 1965 · 327
64. Static Fatigue of Glass: I
65. 10.1111/j.1151-2916.1972.tb11215.x10.1111/j.1151-2916.1972.tb11215.x ↗
66. Chang R. · 1967
67. 10.6028/jres.048.01310.6028/jres.048.013 ↗
68. Holland L. · 1966
69. Emsberger F. M. · 1972 · 529
70. Mullins W. W. · 1963 · 17
71. 10.1007/BF0018894510.1007/BF00188945 ↗
72. 10.1007/BF0264321910.1007/BF02643219 ↗
73. 10.1111/j.1151-2916.1973.tb12419.x10.1111/j.1151-2916.1973.tb12419.x ↗
74. Slow Crack Propagation in Glass
75. Scarborough J. B. · 1962 · 516
76. Schmitz G. K. · 1968
77. Spontaneous Cracking of Glass Filaments
78. Mechanism of Stress Corrosion in E Glass Filaments
79. 10.1111/j.1151-2916.1973.tb12374.x10.1111/j.1151-2916.1973.tb12374.x ↗
80. Handbook of Chemistry and Physics · 1966 · F‐85
81. 10.1111/j.1151-2916.1956.tb15619.x10.1111/j.1151-2916.1956.tb15619.x ↗
82. W. H.Gitzen “Alumina Ceramics.” Tech. Rept No. AFML‐TR‐66‐13 USAF Contract No. AF 33 (657)‐8741. Air Force Materials Laboratory Wright‐Patterson AFB Ohio 1966.