journal article·1982-03

Fracture Behavior of Low‐Density Fibrous Ceramics

D. J. GREEN, J. E. RITTER, F. F. LANGE

Publisher page

Abstract

It was established that subcritical crack growth occurs in the silica fiber‐based tiles that are currently in use as part of the thermal protection system (TPS) of the Space Shuttle. By measuring the tensile strength distribution and the subcritical crack‐growth parameters, it was possible to predict the material's behavior during proof‐testing. A similar time dependence of dynamic strength was also found for structural systems using this ceramic tile, suggesting that the ceramic is controlling their strength behavior. It was possible, therefore, to predict the influence of the proof testing currently in use for the Shuttle. These predictions were found to be in reasonable agreement with the experimentally determined strength distributions after proof‐testing. This study confirmed that proof‐testing and tile densification should lead to improved reliability of the TPS. The research further suggests that the subcritical crack‐growth behavior in these fibrous tiles is simiilar to that observed in bulk glass of similar composition and that failure occurs by the tensile fracture and fragmentation of individual fibers.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Structural Analysis of Composite Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Symposium on Reusable Surface Insulations for the Space Shuttle · NASA TMX · 1973 · 1 · 2719
2. Rusert E. L. · 1971 · 403
3. S.Musikant F. P.MaginIII andJ. I.Gebhardt “Development of REI Mullite (Reusable External Insulation) for Application to the Space Shuttle”; pp.413–15in Ref. 2.
4. R. C.Thuss H. G.Thibault andA. A.Hiltz “Utilization of Silica‐Based Surface Insulation for Space Shuttle Thermal Protection System”; pp.453–65in Ref. 2.
5. Final Report for Improvement of Reusable Surface Insulation Material LMSC D265204 Contract No. NAS9–12137 March 1972.
6. The Shuttle Tile Story
7. Ritter J. E. · 1978 · 667
8. 10.1520/STP36639S10.1520/STP36639S ↗
9. J. E.Ritter Jr. S. M.Wiederhorn N. J.Tighe andE. R.Fuller Jr. “Application of Fracture Mechanics in Assuring Against Fatigue Failure of Ceramic Components ” NBSIR 80–2047 June 1980.10.6028/NBS.IR.80-2047 ↗
10. D. J.GreenandF. F.Lange “Micromechanical Model for Fibrous Ceramic Bodies”;this issue pp.138–41.10.1111/j.1151-2916.1982.tb10381.x ↗
11. Materials Properties Handbook · 1979
12. Ambartsumya S.A. · 1970 · 11
13. D. J.Green;unpublished work.
14. Crack Propagation in Ceramic Materials Under Cyclic Loading Conditions10.1007/BF02642921 ↗
15. 10.1007/BF0055231710.1007/BF00552317 ↗
16. 1980
17. “Effect of Load Rate on Flatwise Tensile Strength of LI 900/.160 SIP ” Laboratory Test Report TR S107075 ibid. Feb. 1980.
18. “Effect of Load Rate on Flatwise Tensile Strength of Densified LI 900/.160 SIP ”LabRept. TRS134381.
19. 10.1098/rspa.1976.010610.1098/rspa.1976.0106 ↗
20. 10.1007/978-1-4615-7014-1_1210.1007/978-1-4615-7014-1_12 ↗
21. J. W.SawyerandP. A.Cooper “Fatigue Properties of Shuttle Thermal Protection System ”NASA Technical Memorandum 81899 Jan. 1981.
22. 10.1111/j.1151-2916.1971.tb16013.x10.1111/j.1151-2916.1971.tb16013.x ↗