Minimum time heating cycles for diffusion‐ versus permeability‐controlled binder removal from ceramic green bodies
Source abstract
Abstract
Abstract A comparison of minimum time heating cycles ( MTHC s) was conducted for binder removal from ceramic green bodies for two mass transfer mechanisms: diffusion and gas permeability. The MTHC s were determined by combining approximate analytic solutions to the governing reaction‐diffusion and reaction‐gas permeability equations with a variational calculus algorithm containing a constraint on pressure buildup within the green body. Both the temperature‐time profile and duration of the MTHC s were sensitive to the operative transport process as well as to a number of model parameters including the pressure constraint, the total furnace pressure, the reaction kinetics, the gas permeability, and the diffusivity as described by the free volume theory. Strategies were identified which are most effective for decreasing the cycle time for each mass transfer mechanism.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Injection Molding Process and Properties · Epoxy Resin Curing Processes · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical and Aerospace Engineering Department of Chemical Engineering University of Missouri Columbia Missouri
References (37)
Show source-provided references
1. Theory of thermal debinding
2. 10.1146/annurev.matsci.27.1.14710.1146/annurev.matsci.27.1.147 ↗
3. 10.1016/0009-2509(90)87050-310.1016/0009-2509(90)87050-3 ↗
4. 10.1002/aic.69037040810.1002/aic.690370408 ↗
5. 10.1098/rspa.1991.002010.1098/rspa.1991.0020 ↗
6. 10.1557/JMR.1993.061710.1557/JMR.1993.0617 ↗
7. 10.1557/JMR.1996.010110.1557/JMR.1996.0101 ↗
8. 10.1111/j.1151-2916.1996.tb07938.x10.1111/j.1151-2916.1996.tb07938.x ↗
9. 10.1016/S1359-6454(02)00036-810.1016/S1359-6454(02)00036-8 ↗
10. 10.1016/S0955-2219(97)00193-310.1016/S0955-2219(97)00193-3 ↗
11. 10.1016/S1385-8947(98)00098-910.1016/S1385-8947(98)00098-9 ↗
12. 10.1111/j.1151-2916.2003.tb00005.x10.1111/j.1151-2916.2003.tb00005.x ↗
13. 10.1557/JMR.2001.033410.1557/JMR.2001.0334 ↗
14. 10.1007/s11663-002-0058-610.1007/s11663-002-0058-6 ↗
15. 10.1111/j.1151-2916.2002.tb00172.x10.1111/j.1151-2916.2002.tb00172.x ↗
16. 10.1557/JMR.2002.021310.1557/JMR.2002.0213 ↗
17. 10.1557/JMR.2003.037810.1557/JMR.2003.0378 ↗
18. 10.1016/j.ces.2007.08.05110.1016/j.ces.2007.08.051 ↗
19. 10.1016/j.ces.2009.03.00610.1016/j.ces.2009.03.006 ↗
20. 10.1179/174367508X30650510.1179/174367508X306505 ↗
21. Development of a heating schedule for rapid thermal debinding of green multilayer ceramic capacitors
22. 10.1111/jace.1245510.1111/jace.12455 ↗
23. 10.1111/jace.1328410.1111/jace.13284 ↗
24. 10.1016/0955-2219(93)90055-V10.1016/0955-2219(93)90055-V ↗
25. A catalogue of ceramic injection moulding defects and their causes
26. 10.1007/BF0114879510.1007/BF01148795 ↗
27. 10.1007/BF0054917110.1007/BF00549171 ↗
28. 10.1111/j.1551-2916.2005.00697.x10.1111/j.1551-2916.2005.00697.x ↗
29. Effect of green body size and heating rate on failure during thermal debinding and on debinding cycle time
30. Methods for introducing safety factors into minimum time heating cycles for binder removal from green ceramic bodies
31. 10.1002/aic.69028021710.1002/aic.690280217 ↗
32. 10.1002/aic.69038030910.1002/aic.690380309 ↗
33. 10.1111/j.1551-2916.2005.00859.x10.1111/j.1551-2916.2005.00859.x ↗
34. Rumpf H · 1962 · 379
35. 10.1111/j.1151-2916.1976.tb10942.x10.1111/j.1151-2916.1976.tb10942.x ↗
36. 10.1016/B978-0-12-395695-8.50008-210.1016/B978-0-12-395695-8.50008-2 ↗
37. Modeling of the green body strength, internal pressure, and stress in porous ceramic bodies during thermal debinding