journal article·2013-02

Nanocomposite Derived from Core–Shell Nanoparticles via Creep Deformation of an Amorphous Silica Layer Below its Glass Transition Temperature

Yoshiaki Kinemuchi, Atsuya Towata, Masaki Yasuoka

Publisher page

Abstract

The microstructural design of ceramics is relevant to tune their properties. Nanostructuring can drastically modify ceramic properties because of enhanced interfacial effects, although the creation of such structures in ceramics is still challenging because of the interfacial reaction and grain growth at elevated temperatures during sintering. Here, we demonstrate densification of core – shell nanoparticles consisting of Fe 3 O 4 (core particle, 20 nm diameter) and SiO 2 (shell layer, 2 nm thick) with over 90% of theoretical density below 500°C, which was achieved by facilitating plastic flow of amorphous SiO 2 under high pressure below its glass transition temperature. Thus, grain growth of the core nanoparticles was strongly suppressed, and the core nanoparticles remained separated by an amorphous layer in the final microstructure reflecting the original core–shell nanostructure. We also analyzed the densification behavior on the basis of a power law creep model, and estimated the pressures required to attain full density.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Material Dynamics and Properties · Glass properties and applications · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Institute of Advanced Industrial Science and Technology 2266‐98 Anagahora, Shimoshidami Moriyama Nagoya 463‐8560 Japan

Funding

New Energy and Industrial Technology Development Organization

References (29)

Show source-provided references
1. 10.1038/3500454810.1038/35004548 ↗
2. 10.1063/1.347565010.1063/1.3475650 ↗
3. 10.1063/1.366939210.1063/1.3669392 ↗
4. 10.1111/j.1151-2916.1991.tb06863.x10.1111/j.1151-2916.1991.tb06863.x ↗
5. 10.1016/0001-6160(82)90028-110.1016/0001-6160(82)90028-1 ↗
6. 10.1016/0001-6160(75)90136-410.1016/0001-6160(75)90136-4 ↗
7. 10.1007/BF0265161810.1007/BF02651618 ↗
8. 10.1111/j.1551-2916.1986.tb00026.x10.1111/j.1551-2916.1986.tb00026.x ↗
9. 10.1063/1.165692710.1063/1.1656927 ↗
10. Hardness‐Temperature Characteristics of Some Simple Glasses
11. 10.1111/j.1151-2916.1960.tb13606.x10.1111/j.1151-2916.1960.tb13606.x ↗
12. 10.1103/PhysRevB.54.728410.1103/PhysRevB.54.7284 ↗
13. 10.1111/j.1551-2916.2009.02928.x10.1111/j.1551-2916.2009.02928.x ↗
14. 10.1016/j.jcis.2011.01.05810.1016/j.jcis.2011.01.058 ↗
15. 10.1016/0021-9797(68)90272-510.1016/0021-9797(68)90272-5 ↗
16. 10.1016/j.jeurceramsoc.2008.02.00310.1016/j.jeurceramsoc.2008.02.003 ↗
17. Sintering Temperature of Porous Glass and Transition Temperature of High Silica Glass
18. Morey G. W. · 1954 · 275
19. 10.1016/0022-3093(85)90190-510.1016/0022-3093(85)90190-5 ↗
20. 10.1111/j.1151-2916.1986.tb07448.x10.1111/j.1151-2916.1986.tb07448.x ↗
21. 10.1111/j.1151-2916.1984.tb19165.x10.1111/j.1151-2916.1984.tb19165.x ↗
22. Brinker C. J. · 1989
23. 10.1088/0370-1301/62/12/31010.1088/0370-1301/62/12/310 ↗
24. 10.1111/j.1151-2916.1977.tb14114.x10.1111/j.1151-2916.1977.tb14114.x ↗
25. 10.1111/j.1151-2916.1963.tb13776.x10.1111/j.1151-2916.1963.tb13776.x ↗
26. Tabor D. · 1951
27. 10.1038/217733a010.1038/217733a0 ↗
28. Practical and Theoretical Aspects of hot Pressing of Refractory Oxides
29. 10.1021/ja01186a01910.1021/ja01186a019 ↗