journal article·1992-10

Strength of Bottles as Affected by Limitations of Manufacturing Processes *

F. W. Preston

Publisher page

Abstract

L etter of T ransmittal This paper is part of the proceedings of the Standard Testing Procedure Committee of the Glass Container Association of America. The reasons that caused the Committee to ask for a more or less formal statement of what was known on this subject will be apparent from the paper itself. The members of the Committee, namely, Mr. Bowes, Mr. Flint, Mr. Hiller, Mr. Lyon, and Mr. Roche, as well as Mr. Hendrickson, Mr. Lester, myself, and various others associated with the Committee, have read the paper and offered criticisms. Although we do not necessarily, either as individuals or as a Committee, concur in all that is said, we believe that the paper offers a new approach to some difficult problems connected with strength, a primary concern of the Committee, and that it may act as a basis for industrial advances or for further contributions by others outside the Committee. V. L. H all , Secretary , G lass C ontainer A ssociation
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Material Properties and Processing · Structural Analysis of Composite Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (4)

Show source-provided references
1. Philip Arbogast of Pittsburgh Pa. U. S. Pat. 260 879 July 11 1882; Arbogast's method is essentially the modern press‐and‐blow operation pressing the blank solidly in a blank mold transferring it quickly by means of a two‐piece neck mold (ring mold) to a blow mold and blowing to size and shape. The significance and importance of each fundamental element of apparatus and of timing is fully realized by Arbogast and what was true then is still true today. There is only one claim at the end of the patent which is “pressing the mouth or neck to finished from with a dependent mass of glass withdrawing the plunger removing the article from the press mold inserting it in a separate mold and blowing to from the body.”
2. Average 1‐minute sustained pressure strength; Hydrostatic Pressure Test on Glass Containers A.S.T.M. designation C147‐40T. American Society for Testing Materials 260 South Broad St. Philadelphia Pa.
3. Resistance of Bottles to Abuse
4. See star footnote p.432.