Effect of the Ca 2+ ‐substitution on the Microwave Dielectric Properties of M 3 (PO 4 ) 2 (M = Ba, Sr)
Source abstract
Abstract
ABSTRACT We investigated structures, sintering behaviors, and microwave dielectric properties of (A (1‐ x ) Ca x ) 3 (PO 4 ) 2 (A═Ba, Sr; 0≤ x ≤0.03). XRD and BSEM investigations confirmed the formation of limited solid solutions, accompanied by cell volume contraction as the Ca 2+ ‐doping concentration increases. A trace amount of (Sr,Ca) 2 P 2 O 7 secondary phase appears in the x = 0.03 composition of (Sr (1‐ x ) Ca x ) 3 (PO 4 ) 2 . The under‐bonded P–O bond valences increase, while those of the over‐bonded A‐O bonds decrease with increasing the Ca 2+ ‐doping concentration for both solid solutions. The Ca 2+ ‐doping induces a phase transition accompanied by volume expansion around 1200°C for the (Ba (1‐ x) Ca x ) 3 (PO 4 ) 2 , leading to a decrease in relative density with increasing doping concentration when the sintering temperature is ≥ 1200°C/2 h. The (Sr (1‐ x ) Ca x ) 3 (PO 4 ) 2 and (Ba (1‐ x) Ca x ) 3 (PO 4 ) 2 sintered at 1250°C/2 h have relative dielectric permittivities ( ε r ) of ∼13.5 and ∼11.8, respectively, changing little with Ca 2+ ‐doping concentration. The Q × f value decreases for the (Ba (1‐ x) Ca x ) 3 (PO 4 ) 2 , while increases for the (Sr (1‐ x ) Ca x ) 3 (PO 4 ) 2 solid solutions with increasing the Ca 2+ ‐doping level. The temperature coefficient of resonant frequency τ f of the (Ba (1‐ x) Ca x ) 3 (PO 4 ) 2 could be tuned to a near‐zero value of ∼1 ppm/°C coupled with a high Q × f value of ∼ 60 000 GHz at the x = 0.025 composition after sintering at 1250 C/2 h.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Nuclear materials and radiation effects · Microwave-Assisted Synthesis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Shanghai University Shanghai China
References (23)
Show source-provided references
1. 10.1143/JJAP.43.352110.1143/JJAP.43.3521 ↗
2. 10.1016/j.mssp.2022.10679310.1016/j.mssp.2022.106793 ↗
3. 10.1016/j.ceramint.2022.07.01610.1016/j.ceramint.2022.07.016 ↗
4. Sintering Behavior, Microwave Dielectric Properties, and Chemical Bond Features of Novel Low‐permittivity Cu3(PO4)2 Ceramic With Low‐loss
5. 10.1524/zkri.1991.196.1-4.31210.1524/zkri.1991.196.1-4.312 ↗
6. 10.1016/S0022-4596(05)80072-610.1016/S0022-4596(05)80072-6 ↗
7. 10.1021/ja00212a02310.1021/ja00212a023 ↗
8. 10.1016/0022-4596(81)90299-110.1016/0022-4596(81)90299-1 ↗
9. Microwave Dielectric Properties of AZn2(PO4)3 (A= Sr, Ba) Ceramics
10. 10.1016/j.ceramint.2024.07.00610.1016/j.ceramint.2024.07.006 ↗
11. 10.1149/1.240822510.1149/1.2408225 ↗
12. 10.1149/1.242796410.1149/1.2427964 ↗
13. Empirical Bond‐strength‐bond‐length Curves for Oxides
14. 10.1107/S056773947600155110.1107/S0567739476001551 ↗
15. 10.1039/JR961000444210.1039/JR9610004442 ↗
16. 10.1016/0040-6031(90)80206-E10.1016/0040-6031(90)80206-E ↗
17. 10.1143/JJAP.46.299910.1143/JJAP.46.2999 ↗
18. Chiang Y. M. · 1997
19. Maxwell J. C. · 1954
20. 10.1063/1.35385610.1063/1.353856 ↗
21. 10.1111/ijac.1323310.1111/ijac.13233 ↗
22. 10.1111/j.1551-2916.2011.04717.x10.1111/j.1551-2916.2011.04717.x ↗
23. 10.1016/j.stam.2004.08.00210.1016/j.stam.2004.08.002 ↗