Effect of water-based electrolyte on surface, mechanical and tribological properties of ZrO2 nanotube arrays produced on zirconium
Source abstract
Abstract
Abstract In this work, highly ordered ZrO2 nanotube arrays were fabricated on commercial pure Zr substrates through anodic oxidation in the water-based electrolyte at various voltages (30 V, 40 V and 50 V) for 1 h. The monoclinic- and tetragonal-ZrO2 phases were obtained on ZrO2 nanotubes through anodic oxidation. 13 vibration modes have been observed for the samples grown at low voltages (30 V and 40 V), which are assigned to monoclinic symmetry (7Ag + 6Bg), while—with the increasing growth voltage, the dominant phonon peak intensities associated with the monoclinic symmetry 6 times are decreased, and Eg (268 and 645 cm − 1) mode corresponding to tetragonal symmetry is observed. The nanotube array surfaces exhibited hydrophilic and super-hydrophilic behavior compared to the bare Zr surface. The elastic modulus values of ZrO2 nanotube surfaces (14.41 GPa) were highly similar to those of bone structure (10–30 GPa) compared to bare Zr substrate (120.5 GPa). Moreover, hardness values of ZrO2 nanotube surfaces were measured between ∼76.1 MPa and ∼ 283.0 MPa. The critical load values required to separate the nanotubes from the metal surface were measured between ∼1.6 N and ∼26.3 N. The wear resistance of the ZrO2 nanotube arrays was improved compared to that of plain Zr substrate.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Anodic Oxide Films and Nanostructures · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Osman, R.B., Swain, M.V.: A critical review of dental implant materials with an emphasis on titanium versus zirconia. Materials (Basel) 8, 932–958 (2015). https://doi.org/10.3390/ma803093210.3390/ma8030932 ↗
2. Sollazzo, V., Pezzetti, F., Scarano, A., et al.: Zirconium oxide coating improves implant osseointegration in vivo. Dent. Mater. 24, 357–361 (2008). https://doi.org/10.1016/j.dental.2007.06.00310.1016/j.dental.2007.06.003 ↗
3. Sanchez, A.G., Schreiner, W., Duffo, G., Cere, S.: Surface characterization of anodized zirconium for biomedical applications. Appl. Surf. Sci. 257, 6397–6405 (2011). https://doi.org/10.1016/j.apsusc.2011.02.00510.1016/j.apsusc.2011.02.005 ↗
4. Sanchez, A.G., Ballarre, J., Orellano, J.C., Duffo, G., Cere, S.: Surface modification of zirconium by anodisation as material for permanent implants: in vitro and in vivo study. J. Mater. Sci-Mater. Med. 24, 161–169 (2013). https://doi.org/10.1007/s10856-012-4770-810.1007/s10856-012-4770-8 ↗
5. Hosseini, M.G., Daneshvari-Esfahlan, V., Maleki-Ghaleh, H.: Effect of water and fluoride content of anodizing electrolyte on morphology and corrosion behavior of ZrO2-nanotubes developed on zirconium implant. J. Mater. Eng. Perform. 25, 1129–1135 (2016). https://doi.org/10.1007/s11665-016-1904-z10.1007/s11665-016-1904-z ↗
6. Tsutsumi, Y., Nishimura, D., Doi, H., Nomura, N., Hanawa, T.: Difference in surface reactions between titanium and zirconium in Hanks’ solution to elucidate mechanism of calcium phosphate formation on titanium using XPS and cathodic polarization. Mater. Sci. Eng. C 29, 1702–1708 (2009). https://doi.org/10.1016/j.msec.2009.01.01610.1016/j.msec.2009.01.016 ↗
7. Katunar, M.R., Sanchez, A.G., Ballarre, J., et al.: Can anodised zirconium implants stimulate bone formation? Preliminary study in rat model. Prog. Biomater. 3, 1–10 (2014). https://doi.org/10.1007/s40204-014-0024-910.1007/s40204-014-0024-9 ↗
8. Hanawa, T.: In vivo metallic biomaterials and surface modification. Mater. Sci. Eng. A-Struct. Mater. Prop. Microstruct. Process. 267, 260–266 (1999). https://doi.org/10.1016/s0921-5093(99)00101-x10.1016/s0921-5093(99)00101-x ↗
9. Yildiz, T., Durdu, S., Ozcan, K., Usta, M.: Characterization and investigation of biological properties of silver nanoparticle-doped hydroxyapatite-based surfaces on zirconium. Sci. Rep. 13, 6773 (2023). https://doi.org/10.1038/s41598-023-33992-510.1038/s41598-023-33992-5 ↗
10. Chopra, D., Jayasree, A., Guo, T., Gulati, K., Ivanovski, S.: Advancing dental implants: Bioactive and therapeutic modifications of zirconia. Bioactive Materials 13, 161–178 (2022). https://doi.org/10.1016/j.bioactmat.2021.10.01010.1016/j.bioactmat.2021.10.010 ↗
11. Molaei, M., Attarzadeh, N., Fattah-alhosseini, A.: Tailoring the biological response of zirconium implants using zirconia bioceramic coatings: A systematic review. J. Trace Elem. Med. Biol. 66, 1–8 (2021). https://doi.org/10.1016/j.jtemb.2021.12675610.1016/j.jtemb.2021.126756 ↗
12. Fidan, S., Muhaffel, F., Riool, M., et al.: Fabrication of oxide layer on zirconium by micro-arc oxidation: Structural and antimicrobial characteristics. Mater. Sci. Eng. C-Mater. Biol. Appl. 71, 565–569 (2017). https://doi.org/10.1016/j.msec.2016.11.03510.1016/j.msec.2016.11.035 ↗
13. Zhang, L., Wang, S., Han, Y.: Interfacial structure and enhanced adhesion between anodized ZrO2 nanotube films and Zr substrates by sedimentation of fluoride ions. Surf. Coat. Technol. 212, 192–198 (2012). https://doi.org/10.1016/j.surfcoat.2012.09.04910.1016/j.surfcoat.2012.09.049 ↗
14. Shanmugavelayutham, G., Yano, S., Kobayashi, A.: Microstructural characterization and properties of ZrO2/Al2O3 thermal barrier coatings by gas tunnel-type plasma spraying. Vacuum 80, 1336–1340 (2006). https://doi.org/10.1016/j.vacuum.2006.01.05610.1016/j.vacuum.2006.01.056 ↗
15. Leushake, U., Krell, T., Schulz, U., Peters, M., Kaysser, W.A., Rabin, B.H.: Microstructure and phase stability of EB-PVD alumina and alumina/zirconia for thermal barrier coating applications. Surf. Coat. Technol. 94–95, 131–136 (1997). https://doi.org/10.1016/S0257-8972(97)00490-810.1016/S0257-8972(97)00490-8 ↗
16. Brenier, R., Mugnier, J., Mirica, E.: XPS study of amorphous zirconium oxide films prepared by sol-gel. Appl. Surf. Sci. 143, 85–91 (1999). https://doi.org/10.1016/s0169-4332(98)00901-510.1016/s0169-4332(98)00901-5 ↗
17. Li, P., Wang, H., Ni, Y., et al.: Unraveling the six stages of the current-time curve and the bilayer nanotubes obtained by one-step anodization of Zr. Nanoscale Adv. 4, 582–589 (2022). https://doi.org/10.1039/d1na00692d10.1039/d1na00692d ↗
18. Durdu, S., Cihan, G., Yalcin, E., Altinkok, A.: Characterization and mechanical properties of TiO2 nanotubes formed on titanium by anodic oxidation. Ceram. Int. 47, 10972–10979 (2021). https://doi.org/10.1016/j.ceramint.2020.12.21810.1016/j.ceramint.2020.12.218 ↗
19. Durdu, S., Sancak, M., Yalcin, E., Usta, M., Akagunduz, E., Altinkok, A.: Surface characterization of TiO2 nanotube arrays produced on Ti6Al4V alloy by anodic oxidation. Surf. Coat. Technol. 428, 127903 (2021). https://doi.org/10.1016/j.surfcoat.2021.12790310.1016/j.surfcoat.2021.127903 ↗
20. Bashirom, N., Tan, W.K., Kawamura, G., Matsuda, A., Lockman. Z.: Comparison of ZrO2, TiO2, and alpha-Fe2O3 nanotube arrays on Cr(VI) photoreduction fabricated by anodization of Zr, Ti, and Fe foils. Mater. Res. Express 7, 1–9 (2020). https://doi.org/10.1088/2053-1591/ab8ee310.1088/2053-1591/ab8ee3 ↗
21. Wang, C., Wang, Y., Zhang, G., et al.: Preparation of a novel transplant material, zirconium oxide (ZrO2) nanotubes, and characterizations research. Ann. Transplant. 25, e924272 (2020). https://doi.org/10.12659/aot.92427210.12659/aot.924272 ↗
22. Stępień, M., Handzlik, P., Fitzner, K.: Synthesis of ZrO2 nanotubes in inorganic and organic electrolytes by anodic oxidation of zirconium. J. Solid State Electrochem. 18, 3081–3090 (2014). https://doi.org/10.1007/s10008-014-2422-210.1007/s10008-014-2422-2 ↗
23. Raghu, S.N.V., Hartwich, P., Patalas, A., et al.: Nanodentistry aspects explored towards nanostructured ZrO2: Immobilizing zirconium-oxide nanotube coatings onto zirconia ceramic implant surfaces. Open Ceram. 14, 100340 (2023). https://doi.org/10.1016/j.oceram.2023.10034010.1016/j.oceram.2023.100340 ↗
24. Ni, Y.L., Li, C.Y., Chen, J.D., et al.: Formation process of zirconia nanotubes and porous structures and model of oxygen bubble growth. Ceram. Int. 48, 495–502 (2022). https://doi.org/10.1016/j.ceramint.2021.09.12510.1016/j.ceramint.2021.09.125 ↗
25. Zalnezhad, E., Hamouda, A.M.S., Jaworski, J., Do Kim, Y.: From zirconium nanograins to zirconia nanoneedles. Sci. Rep. 6, 33282 (2016). https://doi.org/10.1038/srep3328210.1038/srep33282 ↗
26. Sarcan, F., Dönmez, Ö., Kara, K., et al.: Bismuth-induced effects on optical, lattice vibrational, and structural properties of bulk GaAsBi alloys. Nanoscale Res. Lett. 9, 119 (2014). https://doi.org/10.1186/1556-276X-9-11910.1186/1556-276X-9-119 ↗
27. Sarcan, F., Fairbairn, N.J., Zotev, P., et al.: Understanding the impact of heavy ions and tailoring the optical properties of large-area monolayer WS2 using focused ion beam. npj 2D Mater. Appl. 7, 23 (2023). https://doi.org/10.1038/s41699-023-00386-010.1038/s41699-023-00386-0 ↗
28. Erol, A., Akalin, E., Sarcan, F., et al.: Excitation energy-dependent nature of Raman scattering spectrum in GaInNAs/GaAs quantum well structures. Nanoscale Res. Lett. 7, 656 (2012). https://doi.org/10.1186/1556-276X-7-65610.1186/1556-276X-7-656 ↗
29. Zhao, X., Vanderbilt, D.: Phonons and lattice dielectric properties of zirconia. Phys. Rev. B 65, 075105 (2002). https://doi.org/10.1103/PhysRevB.65.07510510.1103/PhysRevB.65.075105 ↗
30. Ciszak, C., Mermoux, M., Gutierrez, G., et al.: Raman spectra analysis of ZrO2 thermally grown on Zircaloy substrates irradiated with heavy ion: Effects of oxygen isotopic substitution. J. Raman Spectrosc. 50, 425–435 (2019). https://doi.org/10.1002/jrs.551310.1002/jrs.5513 ↗
31. Singh, F., Rawat, M., Gautam, S.K., Ojha, S.: Micro-Raman investigations on zirconium oxide film during swift heavy ion irradiation to study crystalline-to-crystalline phase transformation kinetics by cascade overlap model. J. Appl. Phys. 126, 1–7 (2019). https://doi.org/10.1063/1.509030910.1063/1.5090309 ↗
32. Rawat, M., Das, A., Shukla, D.K., et al.: Micro-Raman and electronic structure study on kinetics of electronic excitations induced monoclinic-to-tetragonal phase transition in zirconium oxide films. RSC Adv. 6, 104425–104432 (2016). https://doi.org/10.1039/c6ra14199d10.1039/c6ra14199d ↗
33. Chauhan, V., Gupta, D., Upadhyay, S., et al.: Influence of high dose gamma radiation on optical, physico-chemical and surface morphology properties of nanocrystalline ZrO2 thin films. Opt. Mater. 126, 112125 (2022). https://doi.org/10.1016/j.optmat.2022.11212510.1016/j.optmat.2022.112125 ↗
34. Emeline, A., Kataeva, G.V., Litke, A.S., Rudakova, A.V., Ryabchuk, V.K., Serpone, N.: Spectroscopic and photoluminescence studies of a wide band gap insulating material: powdered and colloidal ZrO2 sols. Langmuir 14, 5011–5022 (1998). https://doi.org/10.1021/la980083l10.1021/la980083l ↗
35. Sowa, M., Łastówka, D., Kukharenko, A.I., et al.: Characterisation of anodic oxide films on zirconium formed in sulphuric acid: XPS and corrosion resistance investigations. J. Solid State Electrochem. 21, 203–210 (2017). https://doi.org/10.1007/s10008-016-3369-210.1007/s10008-016-3369-2 ↗
36. Noothongkaew, S., Ariyachaokun, K., Pansri, S.: Enhanced bioactivity and antibacterial properties of anodized ZrO2 implant coatings via optimized nanoscale morphology and timed antibiotic release through PLGA overcoat. Ceram. Int. 47, 33775–33787 (2021). https://doi.org/10.1016/j.ceramint.2021.08.28910.1016/j.ceramint.2021.08.289 ↗
37. Wang, L.N., Luo, J.L.: Electrochemical behaviour of anodic zirconium oxide nanotubes in simulated body fluid. Appl. Surf. Sci. 258, 4830–4833 (2012). https://doi.org/10.1016/j.apsusc.2012.01.04310.1016/j.apsusc.2012.01.043 ↗
38. Yu, M.S., Li, C., Yang, Y.B., et al.: Cavities between the double walls of nanotubes: Evidence of oxygen evolution beneath an anion-contaminated layer. Electrochem. Commun. 90, 34–38 (2018). https://doi.org/10.1016/j.elecom.2018.03.00910.1016/j.elecom.2018.03.009 ↗
39. Zhu, X.F., Song, Y., Liu, L., et al.: Electronic currents and the formation of nanopores in porous anodic alumina. Nanotechnology 20, 1–7 (2009). https://doi.org/10.1088/0957-4484/20/47/47530310.1088/0957-4484/20/47/475303 ↗
40. Zhu, X.F., Song, Y., Yu, D.L., Zhang, C.S., Yao, W.: A novel nanostructure fabricated by an improved two-step anodizing technology. Electrochem. Commun. 29, 71–74 (2013). https://doi.org/10.1016/j.elecom.2013.01.01810.1016/j.elecom.2013.01.018 ↗
41. Deen, K.M., Farooq, A., Raza, M.A., Haider, W.: Effect of electrolyte composition on TiO2 nanotubular structure formation and its electrochemical evaluation. Electrochim. Acta 117, 329–335 (2014). https://doi.org/10.1016/j.electacta.2013.11.10810.1016/j.electacta.2013.11.108 ↗
42. Li, X., Li, C.Y., Gong, T.L., et al.: Comparative study on the anodizing process of Ti and Zr and oxide morphology. Ceram. Int. 47, 23332–23337 (2021). https://doi.org/10.1016/j.ceramint.2021.05.04610.1016/j.ceramint.2021.05.046 ↗
43. Zhang, S.Y., Yu, D.H., Li, D.D., et al.: Forming Process of Anodic TiO2 Nanotubes under a Preformed Compact Surface Layer. J. Electrochem. Soc. 161, E135–E141 (2014). https://doi.org/10.1149/2.0661410jes10.1149/2.0661410jes ↗
44. Sulka, G.D., Kapusta-Kolodziej, J., Brzozka, A., Jaskula, M.: Anodic growth of TiO2 nanopore arrays at various temperatures. Electrochim. Acta 104, 526–535 (2013). https://doi.org/10.1016/j.electacta.2012.12.12110.1016/j.electacta.2012.12.121 ↗
45. Chen, C.Y., Ozasa, K., Kitamura, F., et al.: Self-organization of TiO2 Nanobamboos by Anodization with Deep Eutectic Solvent. Electrochim. Acta 153, 409–415 (2015). https://doi.org/10.1016/j.electacta.2014.11.08410.1016/j.electacta.2014.11.084 ↗
46. Kwon, Y.S., Park, J.W.: Osteogenic differentiation of mesenchymal stem cells modulated by a chemically modified super-hydrophilic titanium implant surface. J. Biomater. Appl. 33, 205–215 (2018). https://doi.org/10.1177/088532821878687310.1177/0885328218786873 ↗
47. Nie, Y., Kalapos, C., Nie, X., Murphy, M., Hussein, R., Zhang, J.: Superhydrophilicity and antibacterial property of a Cu-dotted oxide coating surface. Ann. Clin. Microbiol. Antimicrob. 9, 25 (2010). https://doi.org/10.1186/1476-0711-9-2510.1186/1476-0711-9-25 ↗
48. Nezhad, E.Z., Sarraf, M., Musharavati, F., et al.: Effect of zirconia nanotube coating on the hydrophilicity and mechanochemical behavior of zirconium for biomedical applications. Surf. Interfaces 28, 101623 (2022). https://doi.org/10.1016/j.surfin.2021.10162310.1016/j.surfin.2021.101623 ↗
49. Vakamulla Raghu, S.N., Killian, M.S.: Wetting behavior of zirconia nanotubes. RSC Adv. 11, 29585–29589 (2021). https://doi.org/10.1039/D1RA04751E10.1039/D1RA04751E ↗
50. Raghu, S.N.V., Chuluunbandi, K., Killian, M.S.: Zirconia nanotube coatings - UV-resistant superhydrophobic surfaces. Surf. Interfaces 26, 101357 (2021). https://doi.org/10.1016/j.surfin.2021.10135710.1016/j.surfin.2021.101357 ↗
51. Wang, L.N., Shen, C., Shinbine, A., Luo, J.L.: Variation on wettability of anodic zirconium oxide nanotube surface. Thin. Solid Films 531, 277–283 (2013). https://doi.org/10.1016/j.tsf.2013.01.06610.1016/j.tsf.2013.01.066 ↗
52. Zhao, Y., Zhang, J., Pantea, C., et al.: Thermal equations of state of the $\ensuremath{\alpha}$, $\ensuremath{\beta}$, and $\ensuremath{\omega}$ phases of zirconium. Phys. Rev. B 71, 184119 (2005). https://doi.org/10.1103/PhysRevB.71.18411910.1103/PhysRevB.71.184119 ↗
53. Shiraishi, T., Yubuta, K., Shishido, T., Shinozaki, N.: Elastic Properties of As-Solidified Ti-Zr Binary Alloys for Biomedical Applications. Mater. Trans. 57, 1986–1992 (2016). https://doi.org/10.2320/matertrans.MI20150110.2320/matertrans.MI201501 ↗
54. Fogaing, E.Y., Lorgouilloux, Y., Huger, M., Gault, C.P.: Young’s modulus of zirconia at high temperature. J. Mater. Sci. 41, 7663–7666 (2006). https://doi.org/10.1007/s10853-006-0593-710.1007/s10853-006-0593-7 ↗
55. Wheeler, D.W., Zekonyte, J., Wood, R.J.K.: Mechanical properties of cerium and a cerium–5wt% lanthanum alloy by nanoindentation and ultrasonic velocity measurements. Mater. Sci. Eng. A 578, 294–302 (2013). https://doi.org/10.1016/j.msea.2013.04.08310.1016/j.msea.2013.04.083 ↗
56. Patel, N.R.G.P.P.: A review on biomaterials: Scope, applications & human anatomy significance. Int. J. Emerg. Technol. Adv. Eng. 2, 91–101 (2012)
57. Rho, J.Y., Ashman, R.B., Turner, C.H.: Young’s modulus of trabecular and cortical bone material: ultrasonic and microtensile measurements. J. Biomech. 26, 111–119 (1993). https://doi.org/10.1016/0021-9290(93)90042-d10.1016/0021-9290(93)90042-d ↗
58. Long, M., Rack, H.J.: Titanium alloys in total joint replacement - a materials science perspective. Biomaterials 19, 1621–1639 (1998). https://doi.org/10.1016/s0142-9612(97)00146-410.1016/s0142-9612(97)00146-4 ↗
59. Almeida, A.C.C., Fontes, L.S., Laurindo, C.A.H., Torres, R.D., Popat, K.C., Soares, P.: Annealing temperature efect on tribocorrosion and biocompatibility properties of TiO2 nanotubes. J. Bio. Tribo-Corros. 64, 1–12 (2020)
60. Sarraf, M., Zalnezhad, E., Bushroa, A.R., et al.: Structural and mechanical characterization of Al/Al2O3 nanotube thin film on TiV alloy. Appl. Surf. Sci. 321, 511–519 (2014). https://doi.org/10.1016/j.apsusc.2014.10.04010.1016/j.apsusc.2014.10.040 ↗
61. Durdu, S., Usta, M.: Characterization and mechanical properties of coatings on magnesium by micro arc oxidation. Appl. Surf. Sci. 261, 774–782 (2012). https://doi.org/10.1016/j.apsusc.2012.08.09910.1016/j.apsusc.2012.08.099 ↗
62. Polat, A., Makaraci, M., Usta, M.: Influence of sodium silicate concentration on structural and tribological properties of microarc oxidation coatings on 2017A aluminum alloy substrate. J. Alloy. Compd. 504, 519–526 (2010). https://doi.org/10.1016/j.jallcom.2010.06.00810.1016/j.jallcom.2010.06.008 ↗
63. Sekler, J., Steinmann, P.A., Hintermann, H.E.: The scratch test: Different critical load determination techniques. Surf. Coat. Technol. 36, 519–529 (1988). https://doi.org/10.1016/0257-8972(88)90179-X10.1016/0257-8972(88)90179-X ↗
64. Rus, D., Capitanu, L., Badita, L.-L.: A qualitative correlation between friction coefficient and steel surface wear in linear dry sliding contact to polymers with SGF. Friction 2, 47–57 (2014). https://doi.org/10.1007/s40544-014-0038-210.1007/s40544-014-0038-2 ↗