journal article·2024-02

Effects of chemical corrosion and thermal shock on the properties of mullite- and cordierite-bonded porous SiC ceramics prepared using waste fly ash

Nilanjan Santra, Dulal Das, Nijhuma Kayal

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Miwa, S., Abe, F., Hamanaka, T., Yamada, T., Miyairi, Y.: Diesel particulate filters made of newly developed SiC. SAE Int. J. Fuels Lubr. 110(4), 190–195 (2001). https://www.jstor.org/stable/4474263210.4271/2001-01-0192 ↗
2. Gómez-Martín, A., Orihuela, M.P., Becerra, J.A., Martínez-Fernández, J., Ramírez-Rico, J.: Permeability and mechanical integrity of porous biomorphic SiC ceramics for application as hot-gas filters. Mater. Des. 107, 450–460 (2016). https://doi.org/10.1016/j.matdes.2016.06.06010.1016/j.matdes.2016.06.060 ↗
3. Dhiman, R., Johnson, E., Skou, E.M., Morgen, P., Andersen, S.M.: SiC nanocrystals as Pt catalyst supports for fuel cell applications. J. Mater. Chem. A 1(19), 6030–6036 (2013). https://doi.org/10.1039/C3TA10238F10.1039/C3TA10238F ↗
4. Bukhari, S.Z.A., Ha, J.H., Lee, J., Song, I.H.: Oxidation-bonded SiC membrane for microfiltration. J. Eur. Ceram. Soc. 38(4), 1711–1719 (2018). https://doi.org/10.1016/j.jeurceramsoc.2017.10.01910.1016/j.jeurceramsoc.2017.10.019 ↗
5. Wang, F., Hao, S., Dong, B., Ke, N., Khan, N.Z., Hao, L., Yin, L., Xu, X., Agathopoulos, S.: Porous-foam mullite-bonded SiC-ceramic membranes for high-efficiency high-temperature particulate matter capture. J. Alloys. Compd. 893, 162231 (2022). https://doi.org/10.1016/j.jallcom.2021.16223110.1016/j.jallcom.2021.162231 ↗
6. Chen, C.Y., Chung, C.J., Wu, B.H., Li, W.L., Chien, C.W., Wu, P.H., Cheng, C.W.: Microstructure and lubricating property of ultra-fast laser pulse textured silicon carbide seals. Appl. Phys. A 107, 345–350 (2012). https://doi.org/10.1007/s00339-012-6822-910.1007/s00339-012-6822-9 ↗
7. Valdez, B., Schorr, M., Zlatev, R., Carrillo, M., Stoytcheva, M., Alvarez, L., Rosas, N.: Corrosion Control in Industry. InTech. (2012). https://doi.org/10.5772/5198710.5772/51987 ↗
8. Fayomi, O.S.I., Akande, I.G., Odigie, S.: Economic impact of corrosion in oil sectors and prevention: an overview. J. Phys. (2007). https://doi.org/10.1088/1742-6596/1378/2/02203710.1088/1742-6596/1378/2/022037 ↗
9. Eliaz, N., Shemesh, G., Latanision, R.M.: Hot corrosion in gas turbine components. Eng. Fail. Anal. 9(1), 31–43 (2002). https://doi.org/10.1016/S1350-6307(00)00035-210.1016/S1350-6307(00)00035-2 ↗
10. Baxter, D., Bellosi, A., Monteverde, F.: Oxidation and burner rig corrosion of liquid phase sintered SiC. J. Eur. Ceram. Soc. 20(3), 367–382 (2000). https://doi.org/10.1016/S0955-2219(99)00160-010.1016/S0955-2219(99)00160-0 ↗
11. Wu, S., Cheng, L., Zhang, L., Xu, Y., Luan, X., Mei, H.: Corrosion of SiC/SiC composite in Na2SO4 vapor environments from 1000 to 1500°C. Compos. A Appl. Sci. Manuf. 37(9), 1396–1401 (2006). https://doi.org/10.1016/j.compositesa.2005.07.01010.1016/j.compositesa.2005.07.010 ↗
12. Cheng, S., Zhao, X., Yang, G., Wang, Y.: Salt-fog corrosion behavior of C/SiC and its effect on ablation resistance. J. Mat. Sci. Technol. 35(12), 2772–2777 (2019). https://doi.org/10.1016/j.jmst.2019.04.03710.1016/j.jmst.2019.04.037 ↗
13. Ip, S.Y., McNallan, M.J., Park, D.S.: Active oxidation of SiC-based ceramics in Ar–2%, Cl2 and O2 gas mixtures at 1000° C. J. Am. Ceram. Soc. 75(7), 1942–1948 (1992). https://doi.org/10.1111/j.1151-2916.1992.tb07221.x10.1111/j.1151-2916.1992.tb07221.x ↗
14. Butt, D.P., Tressler, R.E., Spear, K.E.: Durability of SiC materials in gaseous N2-H2-CO Heat treatment environments. Center. Adv. Mater. Newslett. 5(1), 1–12 (1991)
15. Park, D.J., Jung, Y.I., Kim, H.G., Park, J.Y., Koo, Y.H.: Oxidation behavior of silicon carbide at 1200°C in both air and water–vapor-rich environments. Corros. Sci. 88, 416–422 (2014). https://doi.org/10.1016/j.corsci.2014.07.05210.1016/j.corsci.2014.07.052 ↗
16. Kim, H.E., Moorhead, A.J.: Effect of hydrogen water atmospheres on corrosion and flexural strength of sintered α-silicon carbide. J. Am. Ceram. Soc. 73(3), 694–699 (1990). https://doi.org/10.1111/j.1151-2916.1990.tb06574.x10.1111/j.1151-2916.1990.tb06574.x ↗
17. Zhang, L., Zhang, M., He, X., Tang, W.: Chemical corrosion of liquid-phase sintered SiC in acidic/alkaline solutions part 1. Corrosion in HNO3 solution. J. Mater. Eng. Perform. 25, 839–844 (2016). https://doi.org/10.1007/s11665-016-1916-810.1007/s11665-016-1916-8 ↗
18. Carruth, M., Baxter, D., Oliveira, F., Coley, K.: Hot-corrosion of silicon carbide in combustion gases at temperatures above the dew point of salts. J. Eur. Ceram. Soc. 18(16), 2331–2338 (1998). https://doi.org/10.1016/S0955-2219(98)00239-810.1016/S0955-2219(98)00239-8 ↗
19. Graziani, T., Baxter, D. J., Nannetti, C. A.: Degradation of silicon carbide-based materials in a high temperature combustion environment. Key Eng. Mater. 113, 153–166 (1995). https://www.scientific.net/KEM.113.15310.4028/www.scientific.net/KEM.113.153 ↗
20. More, K.L., Tortorelli, P.F., Walker, L.R., Miriyala, N., Price, J.R., van Roode, M.: High temperature stability of SiC based composites in highwater vapour pressure environments. J. Am. Ceram. Soc. 86(8), 1272–1281 (2003). https://doi.org/10.1111/j.1151-2916.2003.tb03463.x10.1111/j.1151-2916.2003.tb03463.x ↗
21. Lvping, F., Huazhi, Gu., Ao, Huang, Siu, W., Yang, Z., Yongshun, Z., Meijie, Z.: Design, fabrication and properties of lightweight wear lining refractories: a review. J. Euro. Ceram. Soc. 42(3), 744–763 (2022). https://doi.org/10.1016/j.jeurceramsoc.2021.11.01910.1016/j.jeurceramsoc.2021.11.019 ↗
22. Han, F., Xu, C., Wei, W., Zhang, F., Xu, P., Zhong, Z., Xing, W.: Corrosion behaviors of porous reaction-bonded silicon carbide ceramics incorporated with CaO. Ceram. Int. 44(11), 12225–12232 (2018). https://doi.org/10.1016/j.ceramint.2018.04.00410.1016/j.ceramint.2018.04.004 ↗
23. Liu, Z., Zhang, H., Yan, Y., Wu, H., Yang, B., Li, Y., Huang, Z.: Corrosion of sintered SiC ceramics in mixed acid solution: temperature and time dependences. Corros. Eng. Sci. Technol. 52(1), 38–45 (2017). https://doi.org/10.1080/1478422X.2016.117996510.1080/1478422X.2016.1179965 ↗
24. Jiang, Q., Zhou, J., Miao, Y., Yang, S., Zhou, M., Zhong, Z., Xing, W.: Lower-temperature preparation of SiC ceramic membrane using zeolite residue as sintering aid for oil-in-water separation. J. Memb. Sci. 610, 118238 (2020). https://doi.org/10.1016/j.memsci.2020.11823810.1016/j.memsci.2020.118238 ↗
25. Ding, S., Zeng, Y.P., Jiang, D.: Thermal shock resistance of in situ reaction bonded porous silicon carbide ceramics. Mat. Sci. Eng. A. 425(1–2), 326–329 (2006). https://doi.org/10.1016/j.msea.2006.03.07510.1016/j.msea.2006.03.075 ↗
26. Jin, X., Dong, L., Xu, H., Liu, L., Li, N., Zhang, X., Han, J.: Effects of porosity and pore size on mechanical and thermal properties as well as thermal shock fracture resistance of porous ZrB2–SiC ceramics. Ceram. Int. 42(7), 9051–9057 (2016). https://doi.org/10.1016/j.ceramint.2016.02.16410.1016/j.ceramint.2016.02.164 ↗
27. Parvanian, A.M., Salimijazi, H.R., Fathi, M., Saadatfar, M.: Synthesis and thermal shock evaluation of porous SiC ceramic foams for solar thermal applications. J. Am. Ceram. Soc. 102(4), 2009–2020 (2019). https://doi.org/10.1111/jace.1600710.1111/jace.16007 ↗
28. Xu, X., Song, J., Wu, J., Zhang, Y., Zhou, Y., Zhang, Q.: Preparation and thermal shock resistance of mullite and corundum Co-bonded SiC ceramics for solar thermal storage.J. Wuhan Univ. Technol.-Mat. Sci. Ed. 35, 16–25 (2020). https://doi.org/10.1007/s11595-020-2221-910.1007/s11595-020-2221-9 ↗
29. Ding, S., Zeng, Y.P., Jiang, D.: Thermal shock behaviour of mullite-bonded porous silicon carbide ceramics with yttria addition. J. Phys. D Appl. Phys. 40(7), 2138–2142 (2007). https://doi.org/10.1088/0022-3727/40/7/04210.1088/0022-3727/40/7/042 ↗
30. Baitalik, S., Kayal, N.: Thermal shock and chemical corrosion resistance of oxide bonded porous SiC ceramics prepared by infiltration technique. J. of Alloys and Comp. 781, 289 (2019)10.1016/j.jallcom.2018.12.046 ↗
31. Das, D., Kayal, N.: Influence of additive contents on the properties of SiC ceramic membranes and their performance in oil-water separation. Int. J. appl. Ceram. Technol. 20(3), 1715–1729 (2023). https://doi.org/10.1111/ijac.1433410.1111/ijac.14334 ↗
32. Das, D., Kayal, N.: Properties and performance of cordierite bonded porous silicon carbide membrane prepared using waste fly ash and other oxide additives. Bull Mat Sci. 46, 169 (2023). https://doi.org/10.1007/s12034-023-03004-310.1007/s12034-023-03004-3 ↗
33. Tressler, R.E., Meiser, M.D., Yonushonis, T.: Molten salt corrosion of SiC and Si3N4 ceramics. J. Am. Ceram. Soc. 59(5–6), 278–279 (1976). https://doi.org/10.1111/j.1151-2916.1976.tb10962.x10.1111/j.1151-2916.1976.tb10962.x ↗
34. Jacobson, N.S., Smialek, J.L.: Hot corrosion of sintered α-SiC at 1000° C. J. Am. Ceram. Soc. 68(8), 432–439 (1985). https://doi.org/10.1111/j.1151-2916.1985.tb10170.x10.1111/j.1151-2916.1985.tb10170.x ↗
35. Fielder, W. L.: Oxidation and hot corrosion of hot-pressed Si3N4 at 1000°C. (1985). https://ntrs.nasa.gov/api/citations/19850013048/downloads/19850013048
36. Richet, P., Bottinga, Y., Denielou, L., Petitet, J.P., Tequi, C.: Thermodynamic properties of quartz, cristobalite and amorphous SiO2: drop calorimetry measurements between 1000 and 1800 K and a review from 0 to 2000 K. Geochim. Cosmochim. Acta 46(12), 2639–2658 (1982). https://doi.org/10.1016/0016-7037(82)90383-010.1016/0016-7037(82)90383-0 ↗
37. Ringdalen, E.: Changes in quartz during heating and the possible effects on Si production. J. Met. Mater. Miner. 67, 484–492 (2015). https://doi.org/10.1007/s11837-014-1149-y10.1007/s11837-014-1149-y ↗
38. Holmquist, S.B.: Conversion of quartz to tridymite. J. Am. Ceram. Soc. 44(2), 82–86 (1961). https://doi.org/10.1111/j.1151-2916.1961.tb15355.x10.1111/j.1151-2916.1961.tb15355.x ↗
39. Polyakova, I.G.: The main silica phases and some of their properties. In: Schmelzer, J.W.P. (ed.) Glass: selected properties and crystallization, pp. 197–268. De Gruyter, Berlin (2014)10.1515/9783110298581.197 ↗
40. Jacobson, N.S., Fox, D.S., Smialek, J.L., Deliacorte, C., Lee, K.N.: Performance of ceramics in severe environments. Patent No. E-14992. (2005). https://ntrs.nasa.gov/api/citations/20050060620/downloads/20050060620
41. Swainson, I.P., Dove, M.T.: On the thermal expansion of β-cristobalite. Phys. Chem. Miner. 22(1), 61–65 (1995). https://doi.org/10.1007/BF0020268110.1007/BF00202681 ↗
42. Bianco, R., Jacobson, N.: Corrosion of cordierite ceramics by sodium sulphate at 1000°C. J. Mater. Sci. 24, 2903–2910 (1989). https://doi.org/10.1007/BF0238564510.1007/BF02385645 ↗
43. Takahashi, J., Kawai, Y., Shimada, S.: Hot corrosion of cordierite/mullite composites by Na-salts. J. Eur. Ceram. Soc. 22(12), 1959–1969 (2002). https://doi.org/10.1016/S0955-2219(01)00529-510.1016/S0955-2219(01)00529-5 ↗
44. She, J., Ohji, T., Deng, Z.Y.: Thermal shock behavior of porous silicon carbide ceramics. J. Am. Ceram. Soc. 85(8), 2125–2127 (2002). https://doi.org/10.1111/j.1151-2916.2002.tb00418.x10.1111/j.1151-2916.2002.tb00418.x ↗
45. Jin, X., Zhang, X., Han, J., Hu, P., He, R.: Thermal shock behavior of porous ZrB2–SiC ceramics. Mater. Sci. Eng. A.588, 175–180 (2013). https://doi.org/10.1016/j.msea.2013.09.04610.1016/j.msea.2013.09.046 ↗
46. Wang, C., Jiand, Y. S.: Thermal shock damage evaluation of porous refractory by finite element method. In Defect and Diffusion Forum, vol. 312–315, pp. 1032–1037. Trans. Tech. Publications Ltd. (2011). https://doi.org/10.4028/www.scientific.net/ddf.312-315.103210.4028/www.scientific.net/ddf.312-315.1032 ↗
47. Kingery, W.D.: Factors affecting thermal stress resistance of ceramic materials. J. Am. Ceram. Soc. 38(1), 3–15 (1955). https://doi.org/10.1111/j.1151-2916.1955.tb14545.x10.1111/j.1151-2916.1955.tb14545.x ↗
48. Lu, T.J., Fleck, N.A.: The thermal shock resistance of solids. Acta Mater. 46(13), 4755–4768 (1998). https://doi.org/10.1016/S1359-6454(98)00127-X10.1016/S1359-6454(98)00127-X ↗