Fabrication and properties of U-shaped NiFe2O4 ceramic tube produced by slip casting and pressureless sintering
Source abstract
Abstract
To explore the production of ceramic sleeves to protect the thermocouple in aluminum electrolysis, a U-shaped NiFe2O4 ceramic tube was produced by slip casting and pressureless sintering. The slurry stability, thermal shock resistance of NiFe2O4 ceramic tube, and temperature measurement performance of assembled thermocouple with NiFe2O4 ceramic tube were investigated in detail. The slurry stability was enhanced for the narrower size distribution and smaller particles of slurry. The highest average thermal shock of 9.2 was obtained for the samples sintered at 1350 °C for 6 h, resulted from the high binding force of the grains and low linear thermal expansion coefficient. Temperature tests showed that the thermocouple assembled with the U-shaped NiFe2O4 ceramic tube was highly responsive and accurate. In addition, its good resistance to thermal shock and corrosion by molten salts make it a potential candidate for industrial temperature measurement applications in an aluminum reduction cell.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thermal properties of materials · Advanced Sensor Technologies Research · Thermodynamic and Structural Properties of Metals and Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Cassayre, L., Palau, P., Chamelot, P., Massot, L.: Properties of low-temperature melting electrolytes for the aluminum electrolysis process: a review. J Chem Eng Data. 55(11), 4549–4560 (2010)10.1021/je100214x ↗
2. Híveš, J., Thonstad, J.: Electrical conductivity of low-melting electrolytes for aluminium smelting. Electrochim Acta. 49(28), 5111–5114 (2004)10.1016/j.electacta.2004.06.022 ↗
3. Kubiňáková, E., Danielik, V., Híveš, J.: Electrochemical characterization of multicomponent sodium cryolite electrolytes with high content of aluminium fluoride. Electrochim Acta. 265, 474–479 (2018)10.1016/j.electacta.2018.01.174 ↗
4. Kolås, S., Støre, T.: Bath temperature and AlF3 control of an aluminium electrolysis cell. Control Eng Pract. 17(9), 1035–1043 (2009)10.1016/j.conengprac.2009.03.008 ↗
5. Constantin, V.: Influence of the operating parameters over the current efficiency and corrosion rate in the Hall-Heroult aluminum cell with tin oxide anode substrate material. Chin J Chem Eng. 23(4), 722–726 (2015)10.1016/j.cjche.2014.03.003 ↗
6. Taylor, M.P., Zhang, W.D., Wills, V., Schmid, S.: A dynamic model for the energy balance of an electrolysis cell. Chem Eng Res Des. 74(8), 913–933 (1996)10.1205/026387696523094 ↗
7. Safa, Y., Flueck, M., Rappaz, J.: Numerical simulation of thermal problems coupled with magneto hydrodynamic effects in aluminium cell. Appl Math Model. 33(3), 1479–1492 (2009)10.1016/j.apm.2008.02.011 ↗
8. Olsen, E., Thonstad, J.: Nickel ferrite as inert anodes in aluminum electrolysis: part I material fabrication and preliminary testing. J Appl Electrochem. 29(3), 293–299 (1999)10.1023/A:1003460220418 ↗
9. Ma, J., Bao, L., Yao, G.C., Liu, Y.H., Zhang, X., Zhang, Z.G., Liang, L.S.: Effect of MnO2 addition on properties of NiFe2O4-based cermets. Ceram Int. 37(8), 3381–3387 (2011)10.1016/j.ceramint.2011.05.140 ↗
10. Zarrabian, P., Kalantar, M., Ghasemi, S.S.: Fabrication and characterization of nickel ferrite based inert anodes for aluminum electrolysis. J Mater Eng Perform. 23(5), 1656–1664 (2014)10.1007/s11665-014-0914-y ↗
11. Carles, V.B., Pasquet, I., Laurent, V., Gabriel, A., Tailhades, P.: Preparation and electrical properties of dense micro-cermets made of nickel ferrite and metallic copper. Solid State Sci. 11(8), 1503–1506 (2009)10.1016/j.solidstatesciences.2009.05.016 ↗
12. Zhang, Z.G., Yao, G.C., Luo, H.J., Zhang, X., Ma, J.F., Xu, J.R.: Sintering behavior and properties of NiFe2O4 ceramic inert anode toughened by adding NiFe2O4 nanopowder. J Inorg Mater. 31(7), 761–768 (2016)10.15541/jim20180493 ↗
13. Rahaman, M.N.: Ceramic processing and sintering, 2nd edn. Marcel Dekker, New York (2003)
14. Ortiz, A.L., Candelario, V.M., Moreno, R., Guiberteau, F.: Near-net shape manufacture of B4C-Co and ZrC-Co composites by slip casting and pressureless sintering. J Eur Ceram Soc. 37(15), 4577–4584 (2017)10.1016/j.jeurceramsoc.2017.07.024 ↗
15. Sun, Y.H., Xiong, W.H., Li, C.H., Yuan, L.: Effect of dispersant concentration on preparation of an ultrahigh density ZnO-Al2O3 target by slip casting. J Am Ceram Soc. 92(9), 2168–2171 (2009)10.1111/j.1551-2916.2009.03178.x ↗
16. Shafeiey, A., Enayati, M.H., Alhaji, A.: The effect of slip casting and spark plasma sintering (SPS) temperature on the transparency of MgAl2O4 spinel. Ceram Int. 44(4), 3536–3540 (2018)10.1016/j.ceramint.2017.10.228 ↗
17. Talimian, A., Galusek, D.: Aqueous slip casting of translucent magnesium aluminate spinel: effects of dispersant concentration and solid loading. Ceram Int. 45(8), 10646–10653 (2019)10.1016/j.ceramint.2019.02.134 ↗
18. Sun, X.N., Wu, H.K., Zhu, G.Z., Shan, Y.C., Xu, J.J., Li, J.T., Olevsky, E.A.: Direct coarse powder aqueous slip casting and pressureless sintering of highly transparent AlON ceramics. Ceram Int. 46(4), 4850–4856 (2020)10.1016/j.ceramint.2019.10.219 ↗
19. Yi, H.L., Wang, Z.J., Zhou, G.H., Zhang, J., Wang, S.W.: Highly transparent LaYZr2O7 ceramic fabricated by slip casting. Ceram Int. 42(1 Part B), 2070–2073 (2016)10.1016/j.ceramint.2015.09.070 ↗
20. Brouczek, D., Konegger, T.: Open-porous silicon nitride-based ceramics in tubular geometry obtained by slip-casting and gelcasting. Adv Eng Mater. 19(10), 1700434 (2017)10.1002/adem.201700434 ↗
21. Tatar, I., Ediz, N., Aydm, A.: Optimum parameters for the production of porous ceramic materials. J Aust Ceram Soc. 53(2), 253–263 (2017)10.1007/s41779-017-0031-0 ↗
22. Medri, V., Capiani, C., Bellosi, A.: Properties of slip-cast and pressureless-sintered ZrB2-SiC composites. Int J Appl Ceram Technol. 8(2), 351–359 (2011)10.1111/j.1744-7402.2009.02484.x ↗
23. Sornlar, W., Choeycharoen, P., Wannagon, A.: Characterization of alumina crucible made from aluminum industrial waste. J Aust Ceram Soc. 56(2), 771–779 (2020)10.1007/s41779-019-00395-7 ↗
24. Liu, Y., Shu, Y.C., Zeng, X.Y., Sun, B.S., Liang, P., Zhang, Y., Qiu, C., Yi, J.H., He, J.L.: Study on the sintering behavior and characterization of the IGZO ceramics by slip casting. Int J Appl Ceram Technol. 16(2), 585–594 (2019)10.1111/ijac.13100 ↗
25. Tarhan, B.: Usage of fired wall tile wastes into fireclay sanitaryware products. J Aust Ceram Soc. 55(3), 737–746 (2019)10.1007/s41779-018-0285-1 ↗
26. Zhang, Z.G., Xu, J.R., Cao, Z.K., Yao, G.C.: Fabrication of high-density NiFe2O4 ceramics by slip casting and pressureless sintering. Int J Appl Ceram Technol. (2020). https://doi.org/10.1111/ijac.1351410.1111/ijac.13514 ↗
27. Zhang, Z.G., Yao, G.C., Zhang, X., Ma, J.F., Lin, H.: Synthesis and characterization of nickel ferrite nanoparticles via planetary ball milling assisted solid-state reaction. Ceram Int. 41(3 Part B), 4523–4530 (2015)10.1016/j.ceramint.2014.11.147 ↗
28. Kingery, W.D.: Factors affecting thermal stress resistance of ceramic materials. J Am Ceram Soc. 38(1), 3–15 (1955)10.1111/j.1151-2916.1955.tb14545.x ↗
29. Munz, D., Fett, T.: Ceramics, mechanical properties, failure behaviour, material selection, 2nd edn. Springer Series in Materials Science, New York (2001)
30. Zhou, K.C., Li, Z.Y., Zhang, L.: Cermet inert anode for aluminum electrolysis. Central South University Press, Changsha (2012)
31. Makarian, K., Santhanam, S., Wing, Z.N.: Thermal shock resistance of refractory composites with zirconia and silicon-carbide inclusions and alumina binder. Ceram Int. 44(11), 12055–12064 (2018)10.1016/j.ceramint.2018.03.217 ↗
32. Makarian, K., Santhanam, S., Wing, Z.N.: Coefficient of thermal expansion of particulate composites with ceramic inclusions. Ceram Int. 42(15), 17659–17665 (2016)10.1016/j.ceramint.2016.08.082 ↗
33. Kovalčíková, A., Dusza, J., Šajglík, P.: Thermal shock resistance and fracture toughness of liquid-phase-sintered SiC-based ceramics. J Eur Ceram Soc. 29(11), 2387–2394 (2009)10.1016/j.jeurceramsoc.2009.01.021 ↗
34. Liang, T.X., Qi, L., Ma, Z.L., Xiao, Z.L., Wang, Y., Liu, H., Zhang, J.X., Guo, Z.H., Liu, C.T., Xie, W., Ding, T., Lu, N.: Experimental study on thermal expansion coefficient of composite multilayered flaky gun propellants. Compos Part B. 166, 428–435 (2019)10.1016/j.compositesb.2019.02.024 ↗
35. Son, M.A., Chae, K.W., Kim, J.S., Kim, S.H.: Structural origin of negative thermal expansion of cordierite honeycomb ceramics and crystal phase evolution with sintering temperature. J Eur Ceram Soc. 39(7), 2484–2492 (2019)10.1016/j.jeurceramsoc.2019.02.017 ↗
36. Kim, I.J., Cao, G.Z.: Low thermal expansion behavior and thermal durability of ZrTiO4–Al2TiO5–Fe2O3 ceramics between 750 and 1400 °C. J Eur Ceram Soc. 22(14–15), 2627–2632 (2002)
37. Wu, J.F., Liu, M., Xu, X.H., Zhang, Y.X., Lao, X.B.: A novel Si3N4–SiC ceramic used for volumetric receivers. Int J Appl Ceram Technol. 11(2), 246–253 (2014)10.1111/ijac.12094 ↗
38. Xi, J.H., Xie, Y.J., Yao, G.C., Liu, Y.H.: Effect of additive on corrosion resistance of NiFe2O4 ceramics as inert anodes. Trans Nonferrous Met Soc China. 18(2), 356–360 (2008)10.1016/S1003-6326(08)60062-X ↗
39. Nightingale, S.A., Longbottom, R.J., Monaghan, B.J.: Corrosion of nickel ferrite refractory by Na3AlF6–AlF3–CaF2–Al2O3 bath. J Eur Ceram Soc. 33(13–14), 2761–2765 (2013)10.1016/j.jeurceramsoc.2013.04.022 ↗