journal article·2025-07

The influence of mechanical activation and sintering process on the formation of the spinel phase of MgAl2O4

Adriana Peleš Tadić, Jelena Živojinović, Vladimir Pavlović, Ana Stanković, Suzana Filipović, Nina Obradović, Frank Kern

Publisher page

Abstract

Magnesium aluminate has the spinel structure and, due to good mechanical, chemical, and thermal properties, has a wide range of applications including refractory ceramics, optically transparent ceramic windows, and armors. Calcined MgO and Al2O3 powders were mixed in a one-to-one molar ratio to produce phase-pure spinel. The MgO powder was calcined at 1000 oC for 1 h prior to mechanical activation to avoid presence of hydroxide and carbonate at the powder surface. The powders were mechanically activated for 15, 30, and 60 min in a high-energy planetary ball mill in air atmosphere. The mechanically activated powders were pressed into pellets and heated to 1300 oC at 10 oC/min and held for 1 h for the reaction. Afterwards pellets were ground and sieved. Synthesized powders were sintered at 1450 oC at 10 oC/min for 2 h and examined for phase composition, crystal structure, and morphology. The results showed that mechanical activation and sintering led to formation of pure spinel phase. Mechanical activation times of 30 min and 60 min led to spinel that was more highly crystalline and phase-pure. Raman spectroscopy showed the presence of all five Raman active modes (A1g + Eg +3T2g), and their positions were in a good agreement with previous investigations. Powder morphology analysis showed that particles were comminuted, but that agglomerates formed for longer activation times. The maximum in the particle size distribution curves decreased from 14.7 μm for non-activated powder to 9.1 μm after 15 min of mechanical activation and 8.1 μm after 30 min of mechanical activation, but increased to10.5 μm after 60 min of activation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Nuclear materials and radiation effects · Magnetic Properties and Synthesis of Ferrites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Zegadi, A., Kolli, Hamidouche, M.M., Fantozzi, G.: Transparent MgAl2O4 spinel fabricated by spark plasma sintering from commercial powders. Ceram. Int. 44, 18828–18835 (2018). https://doi.org/10.1016/j.ceramint.2018.07.11710.1016/j.ceramint.2018.07.117 ↗
2. Carniglia, S.C., Barna, G.L.: Handbook of Industrial Refractories Technology: Principles, Types, Properties and Applications, pp. 135–188. Noyes, Park Ridge, NJ (1992)
3. Weast, D.R. (ed.): CRC Handbook of Chemistry and Physics. 71st Ed.; pp. 5-1-5-117. CRC Press, Boca Raton, FL (1990)
4. Urita, Y., Yamaguchi, K., Takita, I., Furuta, K., Natsuo, Y.: Properties of alumina–magnesia refractories for steel ladles. Taikabutsu. 45, 664–672 (1993)
5. Baudin, C., Martinez, R., Pena, P.: High-temperature mechanical behavior of stoichiometric magnesium spinel. J. Am. Ceram. Soc. 78, 1857–1862 (1995). https://doi.org/10.1111/j.1151-2916.1995.tb08900.x10.1111/j.1151-2916.1995.tb08900.x ↗
6. Ruh, E.: The refractory industry today — Japan and the United States. Am. Ceram. Soc. Bull. 63, 1140–1142 (1984)
7. Cunha-Duncan, F.N., Bradt, R.C.: Synthesis of magnesium aluminate spinels from bauxites and magnesias. J. Am. Ceram. Soc. 85, 2995–3003 (2002). https://doi.org/10.1111/j.1151-2916.2002.tb00569.x10.1111/j.1151-2916.2002.tb00569.x ↗
8. Kingery, W.D.: Introduction to Ceramics, vol. 64, 2nd edn. Wiley, New York and London (1976)
9. Sickafus, K.E., Wills, J.M., Grimes, N.W.: Structure of spinel. J. Am. Ceram. Soc. 82, 3279–3292 (1999). https://doi.org/10.1111/j.1151-2916.1999.tb02241.x10.1111/j.1151-2916.1999.tb02241.x ↗
10. Liu, C., Lu, Y., Peng, Q., Xu, C., Yang, K., Li, X., Su, D., Li, Yuhong, Gao, F.: The effect of Sr doping on the structural, mechanical, electronic properties and radiation tolerance of MgAl2O4 spinel: A first-principles study. J. Alloys Compd. 889, 161614 (2021). https://doi.org/10.1016/j.jallcom.2021.16161410.1016/j.jallcom.2021.161614 ↗
11. Khalaf, K.A.M.: Influence of the inversion factor on madelung constants in spinel systems. Solid State Commun. 324, 114134 (2021). https://doi.org/10.1016/j.ssc.2020.11413410.1016/j.ssc.2020.114134 ↗
12. Shannon, R.D.: Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides. Acta Crystallogr. Sect. A. 32, 751–767 (1976). https://doi.org/10.1107/S056773947600155110.1107/S0567739476001551 ↗
13. O’Quinn, E.C., Shamblin, J.B., Perlov, Ewing, R.C., Neuefeind, J., Feygenson, M., Gussev, J., Long, M.: Inversion in Mg1-xNixAl2O4 spinel: New Insight into local structure. J. Am. Chem. Soc. 139, 10395–10402 (2017). https://doi.org/10.1021/jacs.7b0437010.1021/jacs.7b04370 ↗
14. Fukumoto, K.-I., Kinoshita, C., Garner, F.A.: Void formation in magnesium aluminate spinel heavily irradiated with fast neutrons. J. Nucl. Sci. Technol. 32, 773–778 (1995). https://doi.org/10.1080/18811248.1995.973177210.1080/18811248.1995.9731772 ↗
15. Wang, L., Gong, W., Bordes, N., Ewing, R., Feit, Y.: Effects of Ion Dose and Irradiation Temperature on the Microstructure of Three Spinel Compositions, MRS Online Proceedings Library Archive, p. 373. (1994)10.1557/PROC-373-407 ↗
16. Sickafus, K., Larson, A., Yu, N., Nastasi, M., Hollenberg, G., Garner, F., Bradt, R.: Cation disorder in high dose, neutron-irradiated spinel. J. Nucl. Mater. 219, 128–134 (1995). https://doi.org/10.1016/0022-3115(94)00386-610.1016/0022-3115(94)00386-6 ↗
17. Bordes, N., Wang, L., Ewing, R., Sickafus, K.: Ion-beam induced disordering and onset of amorphization in spinel by defect accumulation. J. Mater. Res. 10, 981–985 (1995). https://doi.org/10.1557/JMR.1995.098110.1557/JMR.1995.0981 ↗
18. Raghu, R., Nampoothiri, J., Satish Kumar, T.: In-situ generation of MgAl2O4 particles in Al–Mg alloy using H3BO3 addition for grain refinement under ultrasonic treatment. Measure. 129, 389–394 (2018). https://doi.org/10.1016/j.measurement.2018.07.05610.1016/j.measurement.2018.07.056 ↗
19. Shahbazi, H., Tataei, M.: A novel technique of gel-casting for producing dense ceramics of spinel (MgAl2O4). Ceram. Int. 45, 8727–8733 (2019). https://doi.org/10.1016/j.ceramint.2019.01.19610.1016/j.ceramint.2019.01.196 ↗
20. Ewais, E.M.M., El-Amir, A.A.M., Besisa, D.H.A., Esmat, M., Anadouli, B.E.H.: Synthesis of nanocrystalline MgO/MgAl2O4 spinel powders from industrial wastes. J. Alloys Compd. 691, 822–833 (2017). https://doi.org/10.1016/j.jallcom.2016.08.27910.1016/j.jallcom.2016.08.279 ↗
21. Rahmat, N., Yaakob, Z., Pudukudy, M., Abdul Rahman, N., Jahaya, S.: Single step solid-state fusion for MgAl2O4 spinel synthesis and its influence on the structural and textural properties. Powder Technol. 329, 409–419 (2018). https://doi.org/10.1016/j.powtec.2018.02.00710.1016/j.powtec.2018.02.007 ↗
22. Obradović, N., Filipović, S., Fahrenholtz, W., Marinkovic, B., Rogan, J., Lević, S., Đorđević, A., Pavlović, V.B.: Morphological and structural characterization of MgAl2O4 spinel. Sci. Sinter. 55, 1–10 (2023). https://doi.org/10.2298/SOS2301001O10.2298/SOS2301001O ↗
23. Ceganac, Z., Acimovic, Z., Andric, L., Petrov, M., Mihajlovic, S.: Mechanical activation of ceramic powders and its influence on the quality of the refractory linings, Proceedings of 3rd BMC-2003-Ohnd, R. Macedonia
24. Filipović, S., Pavlović, V.P., Obradović, N., Paunović, V., Maca, K., Pavlović, V.B.: The impedance analysis of sintered MgTiO3 ceramics. J. Alloys Comp. 701, 107–115 (2017). https://doi.org/10.1016/j.jallcom.2017.01.11710.1016/j.jallcom.2017.01.117 ↗
25. Peleš, A., Đorđević, N., Obradović, N., Tadić, N., Pavlović, V.B.: Influence of prolonged sintering time on density and electrical properties of isothermally sintered cordierite-based ceramics. Sci. Sinter. 45, 157–164 (2013). https://doi.org/10.2298/SOS1302157P10.2298/SOS1302157P ↗
26. Filipović, S., Obradović, N., Pavlović, V.B., Mitrić, M., Đorđević, A., Kachlik, M.M.: Effect of consolidation parameters on structural, microstructural and electrical properties of magnesium titanate ceramics. Ceram. Int. 42, 9887–9898 (2016). https://doi.org/10.1016/j.ceramint.2016.03.08810.1016/j.ceramint.2016.03.088 ↗
27. Minh, N.V., Yang, I.-S.: A Raman study of cation-disorder transition temperature of natural MgAl2O4 spinel. Vib. Spectrosc. 35, 93–96 (2004). https://doi.org/10.1016/j.vibspec.2003.12.01310.1016/j.vibspec.2003.12.013 ↗
28. Evarestov, R.A., Platonenko, A., Zhukovskii, Y.: Site symmetry approach applied to the supercell model of MgAl2O4 spinel with oxygen interstitials: Ab initio calculations. Comput. Mater. Sci. 150, 517–523 (2018). https://doi.org/10.1016/j.commatsci.2018.04.00710.1016/j.commatsci.2018.04.007 ↗
29. O’Horo, M.P., Frisillo, A.L., White, W.B.: Lattice vibrations of MgAl2O4 spinel. J. Phys. Chem. Solids. 34, 23–28 (1973). https://doi.org/10.1016/0022-3697(73)90058-910.1016/0022-3697(73)90058-9 ↗
30. Lazzeri, M., Thibaudeau, P.: Ab initio Raman spectrum of the normal and disordered MgAl2O4 spinel. Phys. Rev. B: 74, 140301(R) (2006). https://doi.org/10.1103/PhysRevB.74.14030110.1103/PhysRevB.74.140301 ↗
31. Muche, D.N.F., Marple, M.A.T., Hung, I., Gan, Z., Castro, R.H.R., Sen, S.: Size-induced structural disorder enables ultrahard oxides. J. Phys. Chem. C. 121, 13898–13905 (2017). https://doi.org/10.1021/acs.jpcc.7b0332310.1021/acs.jpcc.7b03323 ↗
32. Obradović, N., Fahrenholtz, W.G., Filipović, S., Marković, S., Blagojević, V., Lević, S., Savić, S., Ðorđević, A., Pavlović, V.: Formation kinetics and cation inversion in mechanically activated, MgAl2O4 spinel ceramics. J. Therm. Anal. Calorim. 140, 95–107 (2020). https://doi.org/10.1007/s10973-019-08846-w10.1007/s10973-019-08846-w ↗
33. Cynn, H., Sharma, S.K., Cooney, T.F., Nicol, M.: High-temperature Raman investigation of order-disorder behavior in the MgAl2O4 spinel. Phys. Rev. B 45, 500 (R) (1992). https://doi.org/10.1103/PhysRevB.45.50010.1103/PhysRevB.45.500 ↗