Densification and microstructure of Al2O3-cBN composites prepared by spark plasma sintering
Source abstract
Abstract
Al2O3-cubic boron nitride (cBN) composites were prepared from Al2O3 and cBN powders by spark plasma sintering (SPS) at temperatures of 1200 to 1600°C for 600 s under a pressure of 100 MPa. Densification, phase transformation, microstructure and mechanical properties of the Al2O3-cBN composites were investigated. Fully dense Al2O3-cBN composites containing 10 to 20 vol% cBN with a relative density of more than 98% were obtained at 1300°C for 600 s without the phase transformation from cBN to hexagonal BN (hBN). The transformation of cBN was more greatly accelerated in the Al2O3-cBN composite than in cBN. The cBN phase to Al2O3 inhibited the grain growth of Al2O3 in the Al2O3-cBN composite. Vickers hardness of dense Al2O3-cBN composites containing 10 to 20 vol% cBN sintered at 1300°C showed the maximum value of 26 GPa. The Al2O3-cBN composite containing 20 vol% cBN sintered at 1300°C had the highest fracture toughness of 4.1 MPa·m1/2.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute for Materials Research, Tohoku University
References (22)
Show source-provided references
1. 1) P. A. Dearnley, Transactions of the ASME. Series H, J. Eng. Mater. Technol., 107, 68-82 (1985).10.1115/1.3225773 ↗
2. 2) R. H. Wentorf, R. C. DeVries and F. P. Bundy, Science, 208, 873-880 (1980).10.1126/science.208.4446.873 ↗
3. 3) F. P. Bundy and R. H. Wentorf, J. Chem. Phys., 38, 1144-1149 (1963).10.1063/1.1733815 ↗
4. 10.1063/1.43187410.1063/1.431874 ↗
5. 5) V. L. Solozhenko, V. Z. Turkevich and W. B. Holzapfel, J. Phys. Chem. B, 103, 2903-2905 (1999).10.1021/jp984682c ↗
6. 6) X. Z. Rong and O. Fukunaga, Advanced Materials '93, I / B, Ed. by M. Homma et al., Elsevier Science B.V., Trans. Mater. Res. Soc. Jpn., 14B, 1455-1458 (1994).
7. 10.1023/B:JMSC.0000034176.85765.4010.1023/B:JMSC.0000034176.85765.40 ↗
8. 10.1016/S0925-9635(01)00692-610.1016/S0925-9635(01)00692-6 ↗
9. KLIMCZYK P · 2004 · 382 · 19510.1016/j.jallcom.2004.04.140 ↗
10. 10) H. Moriguchi, K. Tsuduki and A. Ikegaya, Metal Powder Report, 59, 26-30 (2004).10.1016/S0026-0657(04)00110-9 ↗
11. 10.1111/j.1551-2916.2006.01426.x10.1111/j.1551-2916.2006.01426.x ↗
12. TOKITA MASAO · 1993 · 30 · 79010.4164/sptj.30.11_790 ↗
13. 13) J. Tatami, M. Iguchi, M. Hotta, C. Zhang, K. Komeya, T. Meguro, M. Omori, T. Hirai, M. E. Brito and Y.-B. Cheng, "Key Engineering Materials," 237, 105-110 (2003).10.4028/www.scientific.net/KEM.237.105 ↗
14. 14) D. Hiratsuka, J. Tatami, T. Meguro, K. Komeya, I. Hayashi, J. F. Yang and M. Omori, Key Engineering Materials, 317-318, 633-636 (2006).10.4028/www.scientific.net/KEM.317-318.633 ↗
15. ZHOU Y · 2000 · 83 · 65410.1111/j.1151-2916.2000.tb01249.x ↗
16. SHEN Z · 2002 · 85 · 192110.1111/j.1151-2916.2002.tb00381.x ↗
17. SUGANUMA M · 2003 · 86 · 38710.1111/j.1151-2916.2003.tb03310.x ↗
18. 18) JCPDS, International Centre for Diffraction Data, No.10-173.
19. 19) JCPDS, International Centre for Diffraction Data, No.25-1033.
20. 10.1007/BF0055747910.1007/BF00557479 ↗
21. 10.1016/S0925-9635(99)00131-410.1016/S0925-9635(99)00131-4 ↗
22. 1991 · 2 · 233