Electrical and mechanical properties of glass and glass-ceramic electrolytes in the system Li3BO3–Li2SO4
Source abstract
Abstract
Low-melting oxide glasses are promising as electrolytes for all-solid-state lithium rechargeable batteries. Glasses in the pseudobinary system Li3BO3–Li2SO4 were prepared by a mechanochemical technique. Raman spectra revealed that the glasses contained no macroanions which form networks but consisted only of Li+ ions and two discrete ortho-oxoanions, BO33− and SO42−. The density and molar volume increased and elastic moduli decreased with an increase in the Li2SO4 content in the glasses. The heat treatment of the Li3BO3–Li2SO4 glasses at around 300°C brought about the crystallization to form ion conducting glass-ceramics. Electrical conductivities of the glasses and glass-ceramics in this system were maximized with the mixing of Li3BO3 and Li2SO4. The conductivities were higher in the glass-ceramics of the compositions with small amounts of Li2SO4, ranging from 3 × 10−6 to 1 × 10−5 S cm−1 at room temperature, compared to the corresponding glasses. This conductivity enhancement by the heat treatment is probably due to the precipitation of solid solutions with a high temperature Li3BO3 phase.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Applied Chemistry, Graduate School of Engineering, Osaka Prefecture University
Department of Energy and Environment, Research Institute of Electrochemical Energy, National Institute of Advanced Industrial Science and Technology (AIST)
Department of Materials Chemistry, Faculty of Engineering, Hokkaido University
References (16)
Show source-provided references
1. 1) K. Takada, Acta Mater., 61, 759–770 (2013).10.1016/j.actamat.2012.10.034 ↗
2. 2) M. Ribes, B. Barrau and J. L. Souquet, J. Non-Cryst. Solids, 38–39, 271–276 (1980).10.1016/0022-3093(80)90430-5 ↗
3. 3) F. Mizuno, A. Hayashi, K. Tadanaga and M. Tatsumisago, Adv. Mater., 17, 918–921 (2005).10.1002/adma.200401286 ↗
4. 4) Y. Seino, T. Ota, K. Takada, A. Hayashi and M. Tatsumisago, Energy Environ. Sci., 7, 627–631 (2014).10.1039/C3EE41655K ↗
5. 5) N. Kamaya, K. Homma, Y. Yamakawa, M. Hirayama, R. Kanno, M. Yonemura, T. Kamiyama, Y. Kato, S. Hama, K. Kawamoto and A. Matsui, Nat. Mater., 10, 682–686 (2011).10.1038/nmat3066 ↗
6. 6) A. Sakuda, A. Hayashi and M. Tatsumisago, Sci. Rep., 3, 2261 (2013).10.1038/srep02261 ↗
7. 7) M. Tatsumisago, N. Machida and T. Minami, J. Ceram. Soc. Japan, 95, 197–201 (1987).10.2109/jcersj1950.95.1098_197 ↗
8. 8) M. Tatsumisago, H. Narita, T. Minami and M. Tanaka, J. Am. Ceram. Soc., 66, C210–C211 (1983).10.1111/j.1151-2916.1983.tb10576.x ↗
9. 9) A. Hayashi, D. Furusawa, Y. Takahashi, K. Minami and M. Tatsumisago, Phys. Chem. Glasses, 54, 109–114 (2013).
10. 10) M. He, H. Okudera, J. Fleig, A. Simon, X. L. Chen and J. Maier, J. Solid State Chem., 178, 680–687 (2005).10.1016/j.jssc.2004.12.017 ↗
11. 11) E. A. Secco, J. Solid State Chem., 96, 366–375 (1992).10.1016/S0022-4596(05)80270-1 ↗
12. 12) M. Tatsumisago, R. Takano, K. Tadanaga and A. Hayashi, J. Power Sources, 270, 603–607 (2014).10.1016/j.jpowsour.2014.07.061 ↗
13. 13) W. L. Konijnendijk and J. M. Stevels, J. Non-Cryst. Solids, 18, 307–331 (1975).10.1016/0022-3093(75)90137-4 ↗
14. 14) K. Nakamoto, “Infrared and Raman spectra of inorganic and coordination compounds”, 3rd ed., Wiley, New York (1978).
15. 15) K. Takahashi and A. Osaka, J. Ceram. Soc. Japan, 91, 116–120 (1983).10.2109/jcersj1950.91.1051_116 ↗
16. 16) B. Raguenet, G. Tricot, G. Silly, M. Ribes and A. Pradel, Solid State Ionics, 208, 25–30 (2012).10.1016/j.ssi.2011.11.034 ↗