Preparation of ZrB2-SiC composites by arc melting and their properties
Source abstract
Abstract
ZrB2-SiC composites were prepared by arc melting using ZrB2 and β-SiC powders as raw materials and their Vickers micro-hardness, electrical conductivity and thermal conductivity were investigated. The eutectic composition of the ZrB2-SiC system was ZrB2-58.5 mol%SiC with a labyrinthine microstructure 100 nm in width and several μm in length. The hardness of the ZrB2-SiC composites increased with increasing SiC content and showed the highest value of 24 GPa at an indenter load of 4.9 N around the eutectic composition. The ZrB2-SiC eutectic composite had the highest fracture hardness of 6 MPa m1/2. The electrical conductivity of ZrB2-SiC composites ranged from 3.2×104 to 5.0×106 S m-1 at room temperature and decreased with increasing temperature. Their thermal conductivity at room temperature was 70 to 95 W m-1 K-1 and decreased with increasing temperature. The eutectic composite had the lowest thermal conductivity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute for Materials Research, Tohoku University
References (26)
Show source-provided references
1. 10.1016/0364-5916(88)90021-110.1016/0364-5916(88)90021-1 ↗
2. 10.1007/BF0055361610.1007/BF00553616 ↗
3. R. A. Cutler · Ceramics and Glasses, Engineered Materials Handbook · 1991 · 4 · 787
4. T. M. Branscomb and O. Hunter, JR. · J. Appl. Phys. · 1971 · 42 · 230910.1063/1.1660541 ↗
5. C. Mroz · Am. Ceram. Soc. Bull. · 1994 · 73 · 141
6. K. Upadhya, J. Yang and W. Hoffman · Am. Ceram. Soc. Bull. · 1997 · 76 · 51
7. 10.1023/A:100452952716210.1023/A:1004529527162 ↗
8. CHAMBERLAIN A L · J. Am. Ceram. Soc. · 2004 · 87 · 117010.1111/j.1551-2916.2004.01170.x ↗
9. 10.1111/j.1551-2916.2006.01329.x10.1111/j.1551-2916.2006.01329.x ↗
10. 10.1007/s10853-006-0719-y10.1007/s10853-006-0719-y ↗
11. 10.1111/j.1551-2916.2006.01270.x10.1111/j.1551-2916.2006.01270.x ↗
12. J. Marschall, D. C. Erlich, H. Mann · J. Mater. Sci. · 2004 · 39 · 595910.1023/B:JMSC.0000041692.72915.e8 ↗
13. ZHANG G-J · J. Am. Ceram. Soc. · 2000 · 83 · 233010.1111/j.1151-2916.2000.tb01558.x ↗
14. 10.1016/j.jeurceramsoc.2006.11.07410.1016/j.jeurceramsoc.2006.11.074 ↗
15. 10.2320/matertrans.43.230910.2320/matertrans.43.2309 ↗
16. 10.2320/matertrans.46.250410.2320/matertrans.46.2504 ↗
17. 10.2320/matertrans.46.206710.2320/matertrans.46.2067 ↗
18. 10.2320/matertrans.47.119310.2320/matertrans.47.1193 ↗
19. R. Tu and T. Goto · Mater. Sci. Forum · 2006 · 534-536 · 1057
20. Izv. Akad. Nauk SSSR, Neorg. Mater. · 1989 · 25 · 1752
21. 21) “Testing Methods for Fracture Toughness of Fine Ceramics,” Japanese Industrial Standard No. JIS R 1607, (1995).
22. K. Niihara, R. Morena and D. P. H. · J. Am. Ceram. Soc. · 1982 · 65 · c11610.1111/j.1151-2916.1982.tb10482.x ↗
23. 10.1007/BF0055747910.1007/BF00557479 ↗
24. R. W. Olesinski and G. J. Abbaschia · Bull. Alloy Phase Diagrams · 1984 · 5 · 48610.1007/BF02872902 ↗
25. 10.1111/j.1151-2916.1995.tb08498.x10.1111/j.1151-2916.1995.tb08498.x ↗
26. KOIWA MASAHIRO · Bull. Jpn. Inst. Metal. · 1988 · 27 · 52510.2320/materia1962.27.525 ↗