Abstract

TiN-cubic boron nitride (cBN) composites were prepared from TiN and cBN powders by spark plasma sintering at temperatures from 1600 to 1800°C for 600 s under a uniaxial pressure of 100 MPa. The densification, phase transformation, microstructure and mechanical properties of the TiN-cBN composites were investigated. TiN-BN composites originally containing 10 to 30 vol% cBN without a phase transformation from cBN to hexagonal BN (hBN) were obtained at a sintering temperature of 1600°C. The densification of the TiN-BN composites was retarded with increasing cBN content. The phase transformation from cBN to hBN in the TiN-BN composites started at 1650°C and was completed at 1800°C. The Vickers hardness and fracture toughness of TiN-BN composite, originally containing 10 vol% cBN, prepared at 1600°C were 17 GPa and 3.6 MPa·m1/2, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute for Materials Research, Tohoku University

References (26)

Show source-provided references
1. 10.1126/science.208.4446.87310.1126/science.208.4446.873 ↗
2. 10.1021/jp984682c10.1021/jp984682c ↗
3. 10.1063/1.43187410.1063/1.431874 ↗
4. 4) F. P. Bundy and R. H. Wentorf Jr., J. Chem. Phys., 38, 1144-1149 (1963).10.1063/1.1733815 ↗
5. 10.1016/j.jallcom.2004.04.14010.1016/j.jallcom.2004.04.140 ↗
6. 10.1023/B:JMSC.0000034176.85765.4010.1023/B:JMSC.0000034176.85765.40 ↗
7. 10.1016/S0925-9635(01)00692-610.1016/S0925-9635(01)00692-6 ↗
8. 8) X. Z. Rong and O. Fukunaga, Advanced Materials '93, I / B, Ed. by M. Homma et al., Elsevier Science B. V., Trans. Mater. Res. Soc. Jpn., 14B, 1455-1458 (1994).
9. 10.1111/j.1551-2916.2006.01426.x10.1111/j.1551-2916.2006.01426.x ↗
10. 10) H. Moriguchi, K. Tsuduki and A. Ikegaya, Metal Powder Report, 59, 26-30 (2004).10.1016/S0026-0657(04)00110-9 ↗
11. 10.1016/S0272-8842(99)00109-110.1016/S0272-8842(99)00109-1 ↗
12. TOKITA MASAO · 1993 · 30 · 79010.4164/sptj.30.11_790 ↗
13. 10.2109/jcersj2.116.74410.2109/jcersj2.116.744 ↗
14. 14) M. Hotta and T. Goto, Mater. Sci. Forum, 561-565, 599-602 (2007).10.4028/www.scientific.net/MSF.561-565.599 ↗
15. 15) D. Hiratsuka, J. Tatami, T. Meguro, K. Komeya, I. Hayashi, J. F. Yang and M. Omori, Key Eng. Mater., 317-318, 633-636 (2006).10.4028/www.scientific.net/KEM.317-318.633 ↗
16. 16) J. Tatami, M. Iguchi, M. Hotta, C. Zhang, K. Komeya, T. Meguro, M. Omori, T. Hirai, M. E. Brito and Y.-B. Cheng, Key Eng. Mater., 237, 105-110 (2003).10.4028/www.scientific.net/KEM.237.105 ↗
17. 10.1111/j.1151-2916.2003.tb03310.x10.1111/j.1151-2916.2003.tb03310.x ↗
18. GROZA J R · 2000 · 83 · 128110.1111/j.1151-2916.2000.tb01369.x ↗
19. ZHOU Y · 2000 · 83 · 65410.1111/j.1151-2916.2000.tb01249.x ↗
20. 10.1007/BF0055747910.1007/BF00557479 ↗
21. 10.1016/S0925-9635(99)00131-410.1016/S0925-9635(99)00131-4 ↗
22. 1991 · 2 · 233
23. 23) J. Martín, J.García, R. Gonzáles, I. Iturriza and F. Castro, Advances in Powder Metallurgy and Particulate Materials, Washington, MPIF, 11, 209-220 (1996).
24. 10.1111/j.1551-2916.2009.03098.x10.1111/j.1551-2916.2009.03098.x ↗
25. 10.1016/j.diamond.2004.05.00410.1016/j.diamond.2004.05.004 ↗
26. 10.1016/j.matlet.2009.01.08610.1016/j.matlet.2009.01.086 ↗