Low-temperature hydrothermal synthesis and characterization of SrTiO3 photocatalysts for NOx degradation
Source abstract
Abstract
SrTiO3 is an excellent photocatalyst due to its high photocorrosion resistance and thermal stability. In this study, we synthesized SrTiO3 nanoparticles with high specific surface areas by the hydrothermal method at reduced temperature. Titanium(IV) bis(ammonium lactato)dihydroxide (TALH) solution and strontium hydroxide octahydrate [Sr(OH)2·8H2O] were used as starting materials. SrTiO3 nanoparticles were directly synthesized by hydrothermal heating at 150°C for 72–120 h. The synthesized nanoparticles had diameters of 20–40 nm, and the SrTiO3 powder heated for 72 h exhibited the highest specific surface area of 33.1 m2/g. This sample also showed the highest degradation rate for NO gas.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Photocatalysis Techniques · Electronic and Structural Properties of Oxides · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Graduate School of Pure and Applied Sciences, University of Tsukuba
Faculty of Pure and Applied Sciences, University of Tsukuba
The Institute of Scientific and Industrial Research (ISIR), Osaka University
Institute of Multidisciplinary Research for Advanced Materials, Tohoku University
References (15)
Show source-provided references
1. 1) A. Fujishima and K. Honda, Nature, 238, 37–38 (1972).
2. 2) M. Miyauchi, M. Takashio and H. Tobimatsu, Langmuir, 20, 232–236 (2004).
3. 3) T. Ohno, T. Tsubota, Y. Nakamura and K. Sayama, Appl. Catal. A-Gen., 288, 74–79 (2005).
4. 4) T. Puangpeth, T. Sreethawong, S. Yoshikawa and S. Chavadej, J. Mol. Catal. A-Chem., 287, 70–79 (2008).
5. 5) J. Xu, Y. Wei, Y. Huang, J. Wang, X. Zheng, Z. Sun, L. Fan and J. Wu, Ceram. Int., 40, 10583–10591 (2014).
6. 6) G. Wu, P. Li, D. Xu, B. Luo, Y. Hong, W. Shi and C. Liu, Appl. Surf. Sci., 333, 39–47 (2015).
7. 7) H. Kato and A. Kudo, J. Phys. Chem. B, 106, 5029–5034 (2002).
8. 8) R. Konta, T. Ishii, H. Kato and A. Kudo, J. Phys. Chem. B, 108, 8992–8995 (2004).
9. 9) T. Puangpetch, S. Chavadej and T. Sreethawong, Energ. Convers. Manage., 52, 2256–2261 (2011).
10. 10) H. Yu, S. Ouyang, S. Yan, Z. Li, T. Yu and Z. Zou, J. Mater. Chem., 21, 11347–11351 (2011).
11. 11) E. Garcia-Lopez, G. Marci, B. Megna, F. Parisi, L. Armelao, A. Trovarelli, M. Boaro and L. Palmisano, J. Catal., 321, 13–22 (2015).
12. 12) N. Wang, D. Kong and H. He, Powder Technol., 207, 470–473 (2011).
13. 13) Y. Zhang, L. Zhong and D. Duan, J. Mater. Sci., 51, 1142–1152 (2016).
14. 14) S. Yin, D. Maeda, M. Ishitsuka, J. Wu and T. Sato, Solid State Ionics, 151, 377–383 (2002).