Low temperature sintering of polycrystalline yttria by transition metal ion doping
Source abstract
Abstract
Sintering of (1 mol%Ni2+-1 mol%Er3+) or (1 mol%Mn2+-1 mol%Er3+) -doped Y2O3 polycrystal was investigated by conventional sintering at the sintering temperature in a range from 1200 to 1600°C. The sintering temperature required for full-densification decreased from 1600 to 1300°C by the doping. The average grain size in Ni2+ or Mn2+-doped Y2O3 is twice as large as that in undoped Y2O3 at the examined sintering temperature. HRTEM observations and EDS analyses with a nano-sized probe indicated that the doped transition metal ions segregated along the grain boundaries without amorphous layers and secondary phase particles. The segregated transition metal ions probably enhance the grain boundary diffusion, and the sinterability of Y2O3 was accordingly improved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Technology, Tokyo University of Science
National Institute for Materials Science
Department of Advanced Materials Science, The University of Tokyo
References (25)
Show source-provided references
1. 1) M. Foex, High Temp.-High Press., 9, 269-282 (1997).
2. 2) T. Yamada, M. Yoshimura and S. Sōmiya, High Temp.-High Press., 18, 377-388 (1986).
3. TSUKUDA YASUO · 1988 · 23 · 456
4. 4) K. A. Wickersheim and R. A. Lefever, J. Electrochem. Soc., 111, 47-51 (1964).10.1149/1.2426061 ↗
5. 10.1111/j.1151-2916.1990.tb09784.x10.1111/j.1151-2916.1990.tb09784.x ↗
6. 6) R. A. Lefever and J. Matsko, Mat. Res. Bull., 2, 865-869 (1967).10.1016/0025-5408(67)90096-7 ↗
7. 1993 · 193 · 280
8. 8) S. K. Dutta and G. E. Gazza, Mat. Res. Bull., 4, 791-796 (1969).10.1016/0025-5408(69)90001-4 ↗
9. 9) Y. Tsukuda and A. Muta, J. Ceram. Soc. Japan, 84, 585-589 (1976).10.2109/jcersj1950.84.976_585 ↗
10. 10) P. J. Jorgensen and R. C. Anderson, J. Am. Ceram. Soc., 50, 553-558 (1967).10.1111/j.1151-2916.1967.tb14997.x ↗
11. 11) C. Grescovich and K. N. Woos, Am. Ceram. Soc. Bull., 52, 473-478 (1973).
12. SAITO N · 1998 · 81 · 202310.1111/j.1151-2916.1998.tb02583.x ↗
13. IKEGAMI T · 2002 · 85 · 172510.1111/j.1151-2916.2002.tb00342.x ↗
14. 1990 · 25 · 1503
15. 10.1111/j.1551-2916.2005.00763.x10.1111/j.1551-2916.2005.00763.x ↗
16. 10.1111/j.1151-2916.1996.tb07998.x10.1111/j.1151-2916.1996.tb07998.x ↗
17. 10.1002/crat.217024060910.1002/crat.2170240609 ↗
18. 18) R. L. Fullman, Trans. AIME, 197, 447-452 (1953).10.1007/BF03398971 ↗
19. 19) E. N. Timofeeva, N. I. Timofeeva, L. N. Drozdova, and O. A. Mordovin, Inorg. Mater. (Engl. Transl.), 5, 983-984 (1969).
20. 10.1557/JMR.1998.036210.1557/JMR.1998.0362 ↗
21. 10.1007/s10853-005-2674-410.1007/s10853-005-2674-4 ↗
22. 1997 · 80 · 63710.1111/j.1151-2916.1997.tb02879.x ↗
23. 10.1016/0022-4596(80)90500-910.1016/0022-4596(80)90500-9 ↗
24. SAITO N · 2001 · 16 · 236210.1557/JMR.2001.0324 ↗
25. 25) R. D. Shannon and C. T. Prewitt, Acta Cryst. Sect. B: Structural Science, 25, 925-946 (1969).10.1107/S0567740869003220 ↗