Structure and oxidation behavior of high temperature ZrB2–SiBCN ceramics with polyborosilazane as a sintering additive
Source abstract
Abstract
The polyborosilazane (PBSZ) was employed as the sintering additive and the dense ZrB2 ultra-high temperature ceramic samples were fabricated by hot pressing at 1900°C. The relative density of sintered ceramics is 96.4%. The PBSZ was converted to amorphous SiBCN ceramics after sintering. Mass transfer process was significantly improved in the amorphous region among the ZrB2 grains. Densification temperature was reduced. The mechanical properties and high temperature oxidation resistance were also enhanced. The bending strength and fracture toughness of the ZrB2 ceramics were 241 ± 10 MPa and 4.47 ± 0.5 MPa m1/2, respectively. The crack was deflected along the grain boundaries. During high-temperature oxidation process, the grain boundary at SiBCN ceramic was oxidized into borosilicate glass and the low viscous glass was extruded out and spread over the surface quickly. The continuous oxide coating formed on the ZrB2 ceramics surface prevented further oxidation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Aerospace Materials and Performance (Ministry of Education), School of Materials Science and Engineering, Beihang University
School of Materials Science and Engineering, Georgia Institute of Technology Atlanta
References (15)
Show source-provided references
1. 1) S. Zhou, Z. Wang and W. Zhang, J. Alloys Compd., 485, 181–185 (2009).10.1016/j.jallcom.2009.05.126 ↗
2. 2) Q. Liu, W. Han, X. Zhang, S. Wang and J. Han, Mater. Lett., 63, 1323–1325 (2009).10.1016/j.matlet.2009.02.054 ↗
3. 3) W. Zhi, W. Zhanjun and S. Guodong, Mater. Sci. Eng., A, 528, 2870–2874 (2011).10.1016/j.msea.2010.12.079 ↗
4. 4) S. Zhu, W. G. Fahrenholtz, G. E. Hilmas, S. C. Zhang, E. J. Yadlowsky and M. D. Keitz, Compos. Part A:Appls, 39, 449–453 (2008).
5. 5) X. Sun, W. B. Han, Q. Liu, P. Hu and C. Q. Hong, Mater. Des., 31, 4427–4431 (2010).10.1016/j.matdes.2010.04.020 ↗
6. 6) X. Sun, W. Han, P. Hu, Z. Wang and X. Zhang, Int. J. Refract. Met. H, 28, 472–474 (2010).10.1016/j.ijrmhm.2009.12.005 ↗
7. 7) F. Monteverde and A. Bellosi, J. Electrochem. Soc., 150, B552–B559 (2003).10.1149/1.1618226 ↗
8. 8) X.-J. Zhou, G.-J. Zhang, Y.-G. Li, Y.-M. Kan and P.-L. Wang, Mater. Lett., 61, 960–963 (2007).10.1016/j.matlet.2006.06.024 ↗
9. 9) R. Riedel, A. Kienzle, W. Dressler, L. Ruwisch, J. Bill and F. Aldinger, Nature, 382, 796–798 (1996).10.1038/382796a0 ↗
10. 10) M. K. Cinibulk and T. A. Parthasarathy, J. Am. Ceram. Soc., 84, 2197–2202 (2001).10.1111/j.1151-2916.2001.tb00987.x ↗
11. 11) H. Jüngermann and M. Jansen, Mater. Res. Innovations, 2, 200–206 (1999).10.1007/s100190050085 ↗
12. 12) P. Chantikul, B. R. Lawn and D. B. Marshall, J. Am. Ceram. Soc., 64, 322–325 (1981).10.1111/j.1151-2916.1981.tb10295.x ↗
13. 13) F. Monteverde, S. Guicciardi and A. Bellosi, Mater. Sci. Eng., A, 346, 310–319 (2003).10.1016/S0921-5093(02)00520-8 ↗
14. 14) F. Monteverde and A. Bellosi, Adv. Eng. Mater., 5, 508–512 (2003).10.1002/adem.200300349 ↗
15. 15) S. R. Levine, E. J. Opila, M. C. Halbig, J. D. Kiser, M. Singh and J. A. Salem, J. Eur. Ceram. Soc., 22, 2757–2767 (2002).10.1016/S0955-2219(02)00140-1 ↗