journal article·2016Open access

Analysis of sintering behavior of silicon nitride based on master sintering curve theory of liquid phase sintering

Junichi TATAMI, Daisuke HIRATSUKA, Shigefumi OKADA, Katsutoshi KOMEYA, Toru WAKIHARA

Abstract

We propose a new master sintering curve (MSC) theory for liquid phase sintering in consideration of grain rearrangement and solution-precipitation in order to analyze the sintering behaviors of silicon nitride (Si3N4) powder compacts. We found that the MSC for liquid phase sintering is theoretically the same expression as that for solid-state sintering. Very fine high-purity powders of Si3N4 Y2O3, Al2O3, AlN, and TiO2 were used as the raw materials to make powder compacts. The degree of sintering shrinkages of the powder compacts, which contained different amounts of the sintering aids, were measured directly by the laser displacement measurement method using a dilatometer. Based on the displacements and the specimen dimensions, the shrinkage ratios and rates could be calculated. The sintering shrinkage behavior depended on the sintering aid used and the heating rate. The MSCs were obtained for shrinkage ratios of 0–2 and 2–15% corresponding to grain rearrangement and the solution-precipitation process, respectively. Finally, the apparent activation energies of sintering of Si3N4 for grain rearrangement and the solution-precipitation process were found to be 251–294 and 345–430 kJ/mol, respectively, depending on the sintering aid used.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Graduate School of Environment and Information Sciences, Yokohama National University

References (47)

Show source-provided references
1. 1) G. C. Deeley, J. M. Herbert and N. C. Moore, Pow.Met., 8, 145–151 (1961).10.1179/pom.1961.4.8.011 ↗
2. 2) K. Komeya and F. Noda, “Aluminum Nitride and Silicon Nitride for High Temperature Gas Turbine Engines”, SAE Paper No. 740237 (1974).10.4271/740237 ↗
3. 3) M. Mitomo, J. Mater. Sci., 11, 1103–1107 (1976).10.1007/BF02396645 ↗
4. 4) G. R. Terwillinger and F. F. Lange, J. Mater. Sci., 10, 1169–1174 (1975).10.1007/BF00541399 ↗
5. 5) K. Komeya, M. Komatsu, T. Kameda, Y. Goto and A. Tsuge, J. Mater. Sci., 26, 5513–5516 (1991).10.1007/BF02403951 ↗
6. 6) M. Matsuoka, J. Tatami, T. Wakihara, K. Komeya and T. Meguro, J. Asian Ceram. Soc., 2, 199–203 (2014).10.1016/j.jascer.2014.02.005 ↗
7. 7) I.-W. Chen and A. Rosenflanz, Nature, 389, 701–704 (1997).10.1038/39542 ↗
8. 8) S. G. Guo, N. Hirosaki, Y. Yamamoto, T. Nishimura and M. Mitomo, J. Am. Ceram. Soc., 85, 1607–1609 (2002).10.1111/j.1151-2916.2002.tb00319.x ↗
9. 9) C. H. Lin, K. Komeya, T. Meguro, J. Tatami, Y. Abe and M. Komatsu, J. Ceram. Soc. Japan, 111, 452–456 (2003).10.2109/jcersj.111.452 ↗
10. 10) J. Tatami, I. W. Chen, Y. Yamamoto, M. Komastu, K. Komeya, D. K. Kim, T. Wakihara and T. Meguro, J. Ceram. Soc. Japan, 114, 1049–1053 (2006).10.2109/jcersj.114.1049 ↗
11. 11) J. Tatami, E. Kodama, H. Watanabe, H. Nakano, T. Wakihara, K. Komeya, T. Meguro and A. Azushima, J. Ceram. Soc. Japan, 116, 749–754 (2008).10.2109/jcersj2.116.749 ↗
12. 12) H. Kawamura and S. Yamamoto, “Improvement of Diesel Engine Startability by Ceramic Glow Plug Start System”, SAE Paprer No. 830580 (1983).10.4271/830580 ↗
13. 13) S. Kamiya, M. Murachi, H. Kawamoto, S. Kato, S. Kawakami and Y. Suzuki, “Silicon Nitride Swirl Chambers for High Power Charged Diesel Engines”, SAE No. 850523 (1985).10.4271/850523 ↗
14. 14) K. Komeya and H. Kotani, JSAE Rev., 7, 72–79 (1986).
15. 15) K. Kijima and S. Shirasaki, J. Chem. Phys., 65, 2668–2671 (1976).10.1063/1.433464 ↗
16. 16) A. Tsuge, K. Nishida and M. Komatsu, J. Am. Ceram. Soc., 58, 323–326 (1975).10.1111/j.1151-2916.1975.tb11488.x ↗
17. 17) K. Komeya, Am. Ceram. Soc. Bull., 63, 1158–1159, 1164 (1984).
18. 18) S. Watanabe, T. Kodera and T. Ogihara, J. Ceram. Soc. Japan, 123, 345–350 (2015).10.2109/jcersj2.123.345 ↗
19. 19) S. K. Choi, S. W. Ui, I. S. Choi and S. C. Choi, J. Ceram. Soc. Japan, 122, 198–203 (2014).10.2109/jcersj2.122.198 ↗
20. 20) Q. H. Yang, H. P. Wang, Z. P. He, D. H. Li, Q. H. Wang and S. Q. Xu, J. Ceram. Soc. Japan, 122, 125–128 (2014).10.2109/jcersj2.122.125 ↗
21. 21) T. Shimonosono, S. Ikeyama, Y. Hirata and S. Sameshima, J. Asian Ceram. Soc., 2, 422–428 (2014).10.1016/j.jascer.2014.09.002 ↗
22. 22) H. Su and D. L. Johnson, J. Am. Ceram. Soc., 79, 3211–3217 (1996).10.1111/j.1151-2916.1996.tb08097.x ↗
23. 23) A. J. Rayner, R. M. C. Clemmer and S. F. Corbin, J. Am. Ceram. Soc., 98, 1060–1065 (2015).10.1111/jace.13405 ↗
24. 24) V. Pouchly, K. Maca and Z. J. Shen, J. Eur. Ceram. Soc., 33, 2275–2283 (2013).10.1016/j.jeurceramsoc.2013.01.020 ↗
25. 25) K. G. Ewsuk, D. T. Ellerby and C. B. DiAntonio, J. Am. Ceram. Soc., 89, 2003–2009 (2006).10.1111/j.1551-2916.2006.00990.x ↗
26. 26) M. Mazaheri, A. Simchi, M. Dourandish and F. Golestani-Fard, Ceram. Int., 35, 547–554 (2009).10.1016/j.ceramint.2008.01.008 ↗
27. 27) J. Tatami, Y. Suzuki, T. Wakihara, T. Meguro and K. Komeya, Key Eng. Mater., 317–318, 11–14 (2006).10.4028/www.scientific.net/KEM.317-318.11 ↗
28. 28) R. Bollina, S. J. Park and R. M. German, POWDER METALLURGY, 53, 20–26 (2010).10.1179/174329009X409688 ↗
29. 29) D. Choron, S. Marinel, B. Pintault, S. Beaudet-Savignat and R. Macaigne, J. Eur. Ceram. Soc., 35, 4195–4202 (2015).10.1016/j.jeurceramsoc.2015.07.014 ↗
30. 30) K. Rozenburg, I. E. Reimanis, H. J. Kleebe and R. L. Cook, J. Am. Ceram. Soc., 91, 444–450 (2008).10.1111/j.1551-2916.2007.02185.x ↗
31. 31) S. J. Park, R. M. German, J. M. Martin, J. F. Guo and J. L. Johnson, Metall. Mater. Trans., A, 37, 2837–2848 (2006).10.1007/BF02586116 ↗
32. 32) L. Wang, V. Pouchly, K. Maca, Z. J. Shen and Y. Xiong, J. Asian Ceram. Soc., 3, 183–187 (2015).10.1016/j.jascer.2015.02.004 ↗
33. 33) W. D. Kingery, J. Appl. Phys., 30, 301–306 (1959).10.1063/1.1735155 ↗
34. 34) R. M. German, “Liquid Phase Sintering”, Plemium, New York (1985) p. 74.10.1007/978-1-4899-3599-1 ↗
35. 35) J. D. Hansen, R. P. Rusin, M.-H. Teng and D. L. Johnson, J. Am. Ceram. Soc., 75, 1129–1135 (1992).10.1111/j.1151-2916.1992.tb05549.x ↗
36. 36) R. T. DeHoff, “A Cell Model for Microstructural Evolution during Sintering”, in Material Science Research, Vol. 16, Sintering and Heterogeneous Catalysis, Ed. by G. C. Kuczynski, A. E. Miller and G. A. Sargent, Plenum Press, New York (1984) pp. 23–34.10.1007/978-1-4613-2761-5_2 ↗
37. 37) J. Tatami, M. Toyama, K. Noguchi, K. Komeya, T. Meguro and M. Komatsu, Ceram. Trans., 247, 83–86 (2003).10.4028/www.scientific.net/KEM.247.83 ↗
38. 38) T. Wakihara, M. Yabuki, J. Tatami, K. Komeya, T. Meguro, H. Hyuga and H. Kita, J. Am. Ceram. Soc., 91, 3413–3415 (2008).10.1111/j.1551-2916.2008.02594.x ↗
39. 39) K. Koga, Ceramics, 25, 107–111 (1990).10.1163/24689300_0250108 ↗
40. 40) O. Abe, J. Mater. Sci., 25, 4018–4026 (1990).10.1007/BF00582475 ↗
41. 41) M. Mitomo, M. Tsutsumi, H. Tanaka, S. Uenosono and F. Saito, J. Am. Ceram. Soc., 73, 2441–2445 (1990).10.1111/j.1151-2916.1990.tb07610.x ↗
42. 42) L. J. Bowen, R. J. Weston, T. G. Carruthers and J. Brook, J. Mater. Sci., 13, 341–350 (1978).10.1007/BF00647779 ↗
43. 43) K. H. Jack, “The Role of Additives in the Densification of Nitrogen Ceramics”, in Final Technical Report, DAERO-78-G-012. European Research Office, U.S. Army, London (1978) pp. 3–14.
44. 44) C. M. Hwang, T. Y. Tien and I-Wei Chen, “Anisotropic Grain Growth During Final Stage Sintering of Silicon Nitride Ceramics”, in Sintering, Ed. by S. Somiya, M. Shimada, M. Yoshimura, and R. Watanabe. Elsevier Applied Science, London (1988) pp. 1034–1039.
45. 45) K. R. Lai and Y. Y. Tien, J. Am. Ceram. Soc., 76, 91–96 (1993).10.1111/j.1151-2916.1993.tb03693.x ↗
46. 46) G. Ziegler, J. Heinrich and G. Wötting, J. Mater. Sci., 22, 3041–3086 (1987).10.1007/BF01161167 ↗
47. 47) M. Kitayama, K. Hirao and S. Kanzaki, J. Am. Ceram. Soc., 89, 2612–2618 (2006).10.1111/j.1551-2916.2006.01106.x ↗