Due to the unique three-dimensional spatial network structure formed by SiO2 nanoparticles and high surface aera, silica aerogel is a high-profile material in many fields. In the present study, by adopting the industrial water glass as the silicon source, silica aerogels had been prepared via the sol–gel approach followed by the ambient pressure drying process. The effects of different alkaline catalysts in terms of LiOH, NaOH, KOH, and NH3·H2O on the formation of silica aerogels were investigated. It was found that with the introduction of alkaline catalysts, the gel aging time dramatically decreased from 5840 to 31 min during the sol–gel process. Compared with the silica aerogels prepared without any catalyst, accordingly, the thermal stability was significantly improved, and the decomposition temperature increased from 375 to above 410 °C. Furthermore, the silica aerogels prepared with alkaline catalysts were featured in a distinctive double-pore structure. It was shown that the alkali metal ions might have an alkaline dissolution effect in the weakly acidic environment during the sol–gel process. Moreover, this effect might increase the contact area between different SiO2 nanoparticles, which was benefit to maintain the three-dimensional spatial network structure and resulted in the silica aerogels with higher thermal stability. The alkaline dissolution effect had an influence on the pore size distribution of silica aerogels with a double pore structure at 1.7 and 32 nm as well as retained large pore volume at about 2.60–3.35 cm3/g.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aerogels and thermal insulation · Mesoporous Materials and Catalysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Civil Engineering, Dalian University of Technology
References (40)
Show source-provided references
1. 1) S. S. Kistler, Nature, 127, 741 (1931).10.1038/127741a0 ↗
2. 2) N. Hã Sing and U. Schubert, Angew. Chem. Int. Edit., 37, 22–45 (2010).
3. 3) C. Zhao, Y. Yan, Z. Hu, L. Li and X. Fan, Constr. Build. Mater., 93, 309–316 (2015).
4. 4) J. P. Randall, M. A. B. Meador and S. C. Jana, ACS Appl. Mater. Interfaces, 3, 613–626 (2011).
5. 5) J. E. Amonette and J. Matyáš, Micropor. Mesopor. Mat., 250, 100–119 (2017).
6. 6) A. Veronovski, G. Tkalec, Ž. Knez and Z. Novak, Carbohyd. Polym., 113, 272–278 (2014).
7. 7) T. W. Hamann, A. B. F. Martinson, J. W. Elam, M. J. Pellin and J. T. Hupp, Adv. Mater., 20, 1560–1564 (2008).
8. 8) M. Schmidt, J. Non-Cryst. Solids, 225, 364–368 (1998).
9. 9) J. Xu, X. Zhou, M. Chen, S. Shi and Y. Cao, Micropor. Mesopor. Mat., 265, 258–265 (2018).
10. 10) D. Sun, K. Li, X. Sui, C. Zhou and F. Liu, J. Porous Mat., 25, 341–349 (2018).
11. 11) A. Venkateswara Rao, S. D. Bhagat, H. Hirashima and G. M. Pajonkc, J. Colloid Interf. Sci., 300, 279–285 (2006).
12. 12) Z. Li, X. Cheng, S. He, X. Shi, H. Yang and H. Zhang, Mater. Lett., 171, 91–94 (2016).
13. 13) A. Venkateswara Rao, A. Parvathy Rao and M. M. Kulkarni, J. Non-Cryst. Solids, 350, 224–229 (2004).
14. 14) C. J. Brinker, K. D. Keefer, D. W. Schaefer, R. A. Assink, B. D. Kay and C. S. Ashley, J. Non-Cryst. Solids, 63, 45–59 (1984).
15. 15) S. Iswar, W. J. Malfait, S. Balog, F. Winnefeld, M. Lattuada and M. M. Koebel, Micropor. Mesopor. Mat., 241, 293–302 (2017).
16. 16) C. Lei, J. Li, C. Sun, H. Yang, T. Xia, Z. Hu and Y. Zhang, Micropor. Mesopor. Mat., 267, 107–114 (2018).
17. 17) C. Lei, Z. Hu, Y. Zhang, H. Yang, J. Li, S. Hu, Micropor. Mesopor. Mat., 258, 236–243 (2018).
18. 18) A. Venkateswara Rao and N. N. Parvathy, J. Mater. Sci., 28, 3021–3026 (1993).
19. 19) S. Zhao, H. Xu, L. Wang and S. J. William, J. Wuhan Univ. Technol., 28, 476–482 (2013).
20. 20) R. B. Torres, J. P. Vareda, A. Lamy-Mendes and L. Durães, J. Supercrit. Fluid., 147, 81–89 (2019).
21. 21) P. B. Wagh, R. Begag, G. M. Pajonk, A. V. Rao and D. Haranath, Mater. Chem. Phys., 57, 214–218 (1999).
22. 22) S. D. Bhagat, Y.-H. Kim, Y.-S. Ahn and J.-G. Yeo, Appl. Surf. Sci., 253, 3231–3236 (2007).
23. 23) P. B. Sarawade, J.-K. Kim, A. Hilonga and H. T. Kim, Solid State Sci., 12, 911–918 (2010).
24. 24) P. B. Sarawade, J.-K. Kim, A. Hilonga and H. T. Kim, Korean J. Chem. Eng., 27, 1301–1309 (2010).
25. 25) P. B. Sarawade, J.-K. Kim, H.-K. Kim and H.-T. Kim, Appl. Surf. Sci., 254, 574–579 (2007).
26. 26) M. A. Aegerter, N. Leventis and M. M. Koebel, “Aerogels Handbook” (2011) pp. 449–498.
27. 27) F. He, J. Cheng, J.-Y. Wu, Y.-H. Huang, X.-H. Zhu and Z.-T. Qi, J. Sol-Gel Sci. Techn., 90, 323–329 (2019).
28. 28) F. Shi, L. Wang, J. Liu and M. Zheng, J. Mater. Sci. Technol., 23, 402–406 (2007).
29. 29) P. B. Sarawade, J.-K. Kim, A. Hilonga and H.-T. Kim, Powder Technol., 197, 288–294 (2010).
30. 30) S. Lee, Y. C. Cha, H. J. Hwang, J.-W. Moon and I. S. Han, Mater. Lett., 61, 3130–3133 (2007).
31. 31) J. Li, J. Cao, L. Huo and X. He, Mater. Lett., 87, 146–149 (2012).
32. 32) V. G. Parale, D. B. Mahadik, M. S. Kavale, A. V. Rao, P. B. Wagh and S. C. Gupta, Soft Nanosci. Lett., 1, 97–104 (2011).
33. 33) A. Hilonga, J.-K. Kim, P. B. Sarawade and H. T. Kim, J. Alloy. Compd., 487, 744–750 (2009).
34. 34) M. V. Khedkar, S. B. Somvanshi, A. V. Humbe and K. M. Jadhav, J. Non-Cryst. Solids, 511, 140–146 (2019).
35. 35) A. Y. Jeong, S. Koo and D. Kim, J. Sol-Gel Sci. Techn., 19, 483–487 (2000).
36. 36) X. Tang, A. Sun, C. Chu, M. Yu, S. Ma, Y. Cheng, J. Guo and G. Xu, Mater. Design, 115, 415–421 (2017).
37. 37) M. Thommes, K. Kaneko, A. V. Neimark, J. P. Olivier, F. Rodriguez-Reinoso, J. Rouquerol and K. S. W. Sing, Pure Appl. Chem., 87, 1051–1069 (2015).
38. 38) S. Chatterji, N. Thaulow and A. D. Jensen, Cement Concrete Res., 18, 363–366 (1988).
39. 39) H. Wang and J. E. Gillott, Cement Concrete Res., 21, 647–654 (1991).
40. 40) E. Garcia-Diaz, J. Riche, D. Bulteel and C. Vernet, Cement Concrete Res., 36, 395–400 (2006).