Abstract

We studied the effects of crystallization conditions on the conduction properties of the Na5YSi4O12-type sodium ion conducting glass-ceramics. Crystallization process was controlled by varying annealing parameters of nucleation time (0–200 h) and crystal growth temperature (900–1100 °C). The present results showed that a shorter nucleation time with annealing at 900 °C for crystal growth gave rise to higher conductivities of 5 × 10−2 S cm−1 at representative temperatures of 300 °C and 3 × 10−3 S cm−1 at 150 °C, respectively. Those results were attributed to the microstructures of glass-ceramics and the conductivities of a whole glass-ceramic were considered to be dominated by those of grains at 300 °C and, on the other hand, strongly influenced by those of grain boundaries at 150 °C. It was found that the dependence of a whole conductivity on the apparent number of grain boundaries calculated as the ratio of a whole thickness to an average grain diameter was stronger in the measurements at 150 °C than at 300 °C. Considering the result, we propose the use of largely grained glass-ceramics for both higher and lower temperature uses.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Applied Chemistry, School of Advanced Engineering, Kogakuin University

Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University

Advanced Central Research Organization, Teikyo University

References (39)

Show source-provided references
1. 1) A. Hayashi, K. Noi, A. Sakuda and M. Tatsumisago, Nat. Commun., 3, 1–5 (2012).10.1038/ncomms1843 ↗
2. 2) M. Tatsumisago and A. Hayashi, Int. J. Appl. Glass Sci., 5, 226–235 (2014).10.1111/ijag.12084 ↗
3. 3) N. Tanibata, M. Deguchi, A. Hayashi and M. Tatsumisago, Chem. Mater., 29, 5232–5238 (2017).10.1021/acs.chemmater.7b01116 ↗
4. 4) K. Noi, Y. Nagata, T. Hakari, K. Suzuki, S. Yabuchi, Y. Ito, A. Sakuda, A. Hayashi and M. Tatsumisago, ACS Appl. Mater. Inter., 10, 19605–19614 (2018).10.1021/acsami.8b02427 ↗
5. 5) T. Honma, T. Togashi, N. Ito and T. Komatsu, Ceram. Eng. Sci. Proc., 34, 33–40 (2013).10.1002/9781118807934.ch4 ↗
6. 6) T. Honma, A. Sato, N. Ito, T. Togashi, K. Shinozaki and T. Komatsu, J. Non-Cryst. Solids, 404, 26–31 (2014).10.1016/j.jnoncrysol.2014.07.028 ↗
7. 7) T. Honma, M. Okamoto, T. Togashi, N. Ito, K. Shinozaki and T. Komatsu, Solid State Ionics, 269, 19–23 (2015).10.1016/j.ssi.2014.11.009 ↗
8. 8) H. Wang, K. Okubo, M. Inada, G. Hasegawa, N. Enomoto and K. Hayashi, Solid State Ionics, 322, 54–60 (2018).10.1016/j.ssi.2018.04.025 ↗
9. 9) Y. Uchida, G. Hasegawa, K. Shima, M. Inada, N. Enomoto, H. Akamatsu and K. Hayashi, ACS Appl. Energy Mater., 2, 2913–2920 (2019).10.1021/acsaem.9b00250 ↗
10. 10) H. Yamauchi, J. Ikejiri, F. Sato, H. Oshita, T. Honma and T. Komatsu, J. Am. Ceram. Soc., 102, 6658–6667 (2019).10.1111/jace.16607 ↗
11. 11) S. Komaba, N. Yabuuchi, T. Nakayama, A. Ogata, T. Ishikawa and I. Nakai, Inorg. Chem., 1, 6211–6220 (2012).10.1021/ic300357d ↗
12. 12) N. Yabuuchi, K. Kubota, M. Dahbi and S. Komaba, Chem. Rev., 1, 11636–11682 (2014).10.1021/cr500192f ↗
13. 13) N. Yabuuchi, I. Ikeuchi, K. Kubota and S. Komaba, ACS Appl. Mater. Inter., 8, 32292–32299 (2016).10.1021/acsami.6b09280 ↗
14. 14) M. Tanabe, T. Honma and T. Komatsu, J. Asian Ceram. Soc., 5, 209–215 (2017).10.1016/j.jascer.2017.04.009 ↗
15. 15) C. R. Peters, M. Bettman, J. W. Moore and M. D. Glick, Acta Crystallogr. B, 27, 1826–1834 (1971).10.1107/S0567740871004862 ↗
16. 16) H. Y.-P. Hong, Mater. Res. Bull., 11, 173–182 (1976).10.1016/0025-5408(76)90073-8 ↗
17. 17) J. B. Goodenough, H. Y.-P. Hong and J. A. Kafalas, Mater. Res. Bull., 11, 203–220 (1976).10.1016/0025-5408(76)90077-5 ↗
18. 18) R. D. Shannon, B. E. Taylor, T. E. Gier, H. Y. Chen and T. Berzins, Inorg. Chem., 17, 958–964 (1978).10.1021/ic50182a033 ↗
19. 19) H. U. Beyeler and T. Hibma, Solid State Commun., 27, 641–643 (1978).10.1016/0038-1098(78)90461-1 ↗
20. 20) M. A. Evstigneeva, V. B. Nalbandyan, A. A. Petrenko, B. S. Medvedev and A. A. Kataev, Chem. Mater., 23, 1174–1181 (2011).10.1021/cm102629g ↗
21. 21) J. Wua, Z. Yu, Q. Wang and X. Guo, Energy Stor. Mater., 24, 467–471 (2020).10.1016/j.ensm.2019.07.012 ↗
22. 22) X. Li, F. Bianchini, J. Wind, C. Pettersen, D. S. Wragg, P. Vajeeston and H. Fjellva, ACS Appl. Mater. Inter., 12, 28188–28198 (2020).10.1021/acsami.0c05863 ↗
23. 23) T. Okura, T. Takahashi, H. Monma and K. Yamashita, Solid State Ionics, 179, 1291–1295 (2008).10.1016/j.ssi.2008.04.017 ↗
24. 24) K. Yamashita, T. Nojiri, T. Umegaki and T. Kanazawa, Solid State Ionics, 35, 299–306 (1989).10.1016/0167-2738(89)90312-3 ↗
25. 25) K. Yamashita, T. Nojiri, T. Umegaki and T. Kanazawa, Solid State Ionics, 40–41, 48–52 (1990).10.1016/0167-2738(90)90284-X ↗
26. 26) K. Yamashita, S. Okura, T. Umegaki and T. Kanazawa, Solid State Ionics, 26, 279–286 (1988).10.1016/0167-2738(88)90255-X ↗
27. 27) K. Yamashita, S. Ohkura, T. Umegaki and T. Kanazawa, J. Ceram. Soc. Jpn., 96, 967–972 (1988).10.2109/jcersj.96.967 ↗
28. 28) K. Yamashita, T. Umegaki, M. Tanaka, T. Kakuta and T. Nojiri, J. Electrochem. Soc., 143, 2180–2186 (1996).10.1149/1.1836978 ↗
29. 29) K. Yamashita, M. Matsuda and T. Umegaki, J. Mater. Res., 13, 3361–3364 (1998).10.1557/JMR.1998.0456 ↗
30. 30) T. Okura, M. Tanaka, H. Kanzawa and G. Sudoh, Solid State Ionics, 86–88, 511–516 (1996).10.1016/0167-2738(96)00335-9 ↗
31. 31) K. Yamashita, M. Tanaka, T. Kakuta, M. Matsuda and T. Umegaki, J. Alloy. Compd., 193, 283–285 (1993).10.1016/0925-8388(93)90372-T ↗
32. 32) T. Okura, K. Kawada, N. Yoshida, H. Monma and K. Yamashita, Solid State Ionics, 225, 367–370 (2012).10.1016/j.ssi.2012.05.010 ↗
33. 33) T. Okura, K. Kawada, N. Yoshida, H. Monma and K. Yamashita, Solid State Ionics, 262, 604–608 (2014).10.1016/j.ssi.2013.10.043 ↗
34. 34) K. Kawada, K. Yamashita and T. Okura, J. Non-Cryst. Solids, 545, 1–9 (2020).10.1016/j.jnoncrysol.2020.120236 ↗
35. 35) K. Kawada, K. Yamashita and T. Okura, J. Ceram. Soc. Jpn., 128, 375–380 (2020).10.2109/jcersj2.20083 ↗
36. 36) T. Okura, M. Saimaru, H. Monma and K. Yamashita, Solid State Ionics, 180, 537–540 (2009).10.1016/j.ssi.2008.12.032 ↗
37. 37) K. Matusita, T. Komatsu and R. Yokota, J. Mater. Sci., 19, 291–296 (1984).10.1007/BF02403137 ↗
38. 38) I. W. Donald, J. Mater. Sci., 30, 904–915 (1995).10.1007/BF01178424 ↗
39. 39) Y. M. Sung, J. Mater. Sci., 31, 5421–5427 (1996).10.1007/BF01159312 ↗