Electrode properties of doped Pr2NiO4-based oxide cathode for intermediate-temperature SOFCs

Takeshi NOMURA, Shunsuke NISHIMOTO, Yoshikazu KAMESHIMA, Michihiro MIYAKE

Journal of the Ceramic Society of Japan· Volume 120· Issue 1407

Abstract

K2NiF4-type Pr2NiO4 doped with Cu, Cu–Ga, or Co (Pr2Ni0.9Cu0.1O4, Pr2Ni0.75Cu0.25O4, Pr1.91Ni0.71Cu0.24Ga0.05O4, or Pr2Ni0.9Co0.1O4) were synthesized by a solid-state reaction for use as cathodes in an intermediate-temperature (500–700°C) solid oxide fuel cell (IT-SOFC). Pr2NiO4, Pr2Ni0.9Cu0.1O4, Pr2Ni0.75Cu0.25O4, Pr1.91Ni0.71Cu0.24Ga0.05O4, and Pr2Ni0.9Co0.1O4 crystallize in the space group Bmab. Single test cells with samarium oxide doped ceria (SDC) as the electrolyte, Ni-SDC cermet as the anode, and the above-mentioned cathode material were fabricated for cell performance measurements at 700°C. Current interruption measurements and electrochemical impedance spectroscopic analysis revealed that the cathode properties of Pr2NiO4, Pr2Ni0.9Cu0.1O4, Pr2Ni0.75Cu0.25O4, and Pr1.91Ni0.71Cu0.24Ga0.05O4 were comparable to that of La0.6Sr0.4Co0.2Fe0.8O3 (LSCF) and the cathode properties of Pr2NiO4 were improved by doping with Cu or Cu–Ga at the Ni site of Pr2NiO4.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Material and Energy Science, Graduate School of Environmental and Life Science, Okayama University

References (23)

Show source-provided references
1. 10.1016/S0920-5861(03)00234-710.1016/S0920-5861(03)00234-7 ↗
2. 10.1016/S0955-2219(01)00120-010.1016/S0955-2219(01)00120-0 ↗
3. 10.1016/S0955-2219(03)00561-210.1016/S0955-2219(03)00561-2 ↗
4. 10.1016/S0022-4596(03)00261-510.1016/S0022-4596(03)00261-5 ↗
5. 10.1039/b102678j10.1039/b102678j ↗
6. 10.1016/S1293-2558(03)00091-810.1016/S1293-2558(03)00091-8 ↗
7. 7) J. A. Kilner and C. K. M. Shaw, Solid State Ionics, 154–155, 523–527 (2002).10.1016/S0167-2738(02)00506-4 ↗
8. 10.1006/jssc.1994.114610.1006/jssc.1994.1146 ↗
9. 10.1016/j.ssi.2006.05.00510.1016/j.ssi.2006.05.005 ↗
10. 10.1007/s10008-006-0127-x10.1007/s10008-006-0127-x ↗
11. 10.1016/j.jpowsour.2008.05.00110.1016/j.jpowsour.2008.05.001 ↗
12. 10.1016/j.ssi.2008.06.01910.1016/j.ssi.2008.06.019 ↗
13. 13) F. Mauvy, C. Lalanne, J. M. Bassat, J. C. Grenier, H. Zhao, L. Huo and P. Stevens, J. Electrochem. Soc., 153, A1547–A1553 (2006).10.1149/1.2207059 ↗
14. 10.1016/j.ssi.2005.06.03310.1016/j.ssi.2005.06.033 ↗
15. 10.1016/j.jeurceramsoc.2005.03.12010.1016/j.jeurceramsoc.2005.03.120 ↗
16. 10.1007/s10008-009-0932-010.1007/s10008-009-0932-0 ↗
17. 18) S. Miyoshi, T. Furuno, H. Matsumoto and T. Ishihara, Solid State Ionics, 177, 2269–2273 (2006).10.1016/j.ssi.2006.01.042 ↗
18. 19) T. Ishihara, S. Miyoshi, T. Furuno, O. Sanguanruang and H. Matsumoto, Solid State Ionics, 177, 3087–3091 (2006).10.1016/j.ssi.2006.08.013 ↗
19. 10.1016/j.ssi.2007.11.01910.1016/j.ssi.2007.11.019 ↗
20. 22) A. V. Kovalevsky, V. V. Kharton, A. A. Yaremchenko, Y. V. Pivak, E. V. Tsipis, S. O. Yakovlev, A. A. Markov, E. N. Naumovich and J. R. Frade, J. Electroceram., 18, 205–218 (2007).
21. 10.1006/jssc.1997.740210.1006/jssc.1997.7402 ↗
22. 10.1149/1.210026710.1149/1.2100267 ↗
23. 10.1111/j.1551-2916.2010.03743.x10.1111/j.1551-2916.2010.03743.x ↗