journal article·2010Open access

One-step realization of open-ended TiO2 nanotube arrays by transition of the anodizing voltage

Shiqi LI, Gengmin ZHANG

Journal of the Ceramic Society of Japan· Volume 118· Issue 1376

Abstract

Free-standing TiO2 nanotubes with both their ends open are required in many applications. This article reports the authors’ latest progress in meeting these requirements. Elevating the voltage at the end of an anodization process can break the adhesion of the TiO2 nanotube layer to the underlying Ti substrate and simultaneously open their bottoms. Furthermore, by modulating the value and duration of the elevated voltage, the bottom morphology of the nanotubes can also be effectively tailored. Compared with most of the related work, in which obtaining free-standing TiO2 nanotube layers and opening their bottom ends are often performed in two separate procedures, this newly-developed route features a simple one-step solution and also good controllability. Both the detachment of the nanotubes from the Ti substrate and the tailoring of their bottom ends are ascribable to the local acidification and gas evolution induced by the sudden voltage transition.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · TiO2 Photocatalysis and Solar Cells · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory for the Physics and Chemistry of Nanodevices and Department of Electronics, Peking University

References (24)

Show source-provided references
1. 10.1038/353737a010.1038/353737a0 ↗
2. 10.1002/adma.20070161910.1002/adma.200701619 ↗
3. 10.1021/nl070264k10.1021/nl070264k ↗
4. 10.1016/j.jphotochem.2005.05.02310.1016/j.jphotochem.2005.05.023 ↗
5. 10.1021/ja810130h10.1021/ja810130h ↗
6. 10.1557/JMR.2001.045710.1557/JMR.2001.0457 ↗
7. 7) K. Kant and D. Losic, Phys. Status Solidi RRL, 3, 139 (2009).10.1002/pssr.200903087 ↗
8. 10.1021/jp811201x10.1021/jp811201x ↗
9. 9) Q. W. Chen, D. S. Xu, Z. Y. Wu and Z. F. Liu, Nanotechnology, 19, 365708 (2008).10.1088/0957-4484/19/36/365708 ↗
10. 10.1021/jp900336e10.1021/jp900336e ↗
11. A. Ghicov, S. P. Albu, J. M. Macak · Small · 2008 · 4 · 106310.1002/smll.200701244 ↗
12. 10.1002/adma.20080081510.1002/adma.200800815 ↗
13. 10.1016/j.memsci.2008.03.05010.1016/j.memsci.2008.03.050 ↗
14. 10.1021/jp075258r10.1021/jp075258r ↗
15. C. J. Lin, W. Y. Yu, Y. T. Lu and S · Chem. Commun. (Camb.) · 2008 · 45 · 6031
16. 10.1021/jp070273h10.1021/jp070273h ↗
17. 10.1021/cm702891710.1021/cm7028917 ↗
18. 10.1021/jp903037f10.1021/jp903037f ↗
19. 10.1021/nl801422w10.1021/nl801422w ↗
20. ZHANG GUOGE · Electrochem. Commun. · 2007 · 9 · 285410.1016/j.elecom.2007.10.014 ↗
21. 10.1007/s10853-007-2418-810.1007/s10853-007-2418-8 ↗
22. J. M. Macak, H. Tsuchiya, A. Ghicov · Curr. Opin. Solid State Mater. Sci. · 2007 · 11 · 310.1016/j.cossms.2007.08.004 ↗
23. 10.1016/j.electacta.2006.11.02310.1016/j.electacta.2006.11.023 ↗
24. 24) Y. Shin and S. Lee, Nanotechnology, 20, 105301 (2009).10.1088/0957-4484/20/10/105301 ↗