journal article·2014Open access

Ferrite multiphase/carbon nanotube composites sintered by spark plasma sintering

Xiaobing ZHOU, Young-Hwan HAN, Yongqiang ZHANG, Qian WANG, Jie ZHOU, Lu SHEN, Tongming HUANG, Weiming PAN, Changshu XIANG, Huiping TANG, Jaehyung LEE, So Ik BAE, Dong-Yeon LEE, Qing HUANG

Journal of the Ceramic Society of Japan· Volume 122· Issue 1429

Abstract

Ni-Carbon nanotube (CNT)-Ni0.5Zn0.5Fe2O4 multiphase composites were sintered by spark plasma sintering (SPS) technique. Ni nanoparticles were in-situ formed due to the localized carbothermal reduction by CNTs and well distributed between grain boundaries in the composites. The electrical conductivity of the resultant multiphase composites was strongly dependent on the weight percentage of CNTs. In the SPS process, CNTs acted as “heating source” and improved the consolidation of the composites. The results indicate that the introduction of the CNTs can promote the sintering kinetics of the ferrite ceramics. However, the grain growth kinetics has been inhibited by SPS and the grain size becomes finer.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electromagnetic wave absorption materials · Magnetic Properties and Synthesis of Ferrites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences

School of Materials Science and Engineering, Yeungnam University

Institute of High Energy Physics Chinese Academy of Sciences

State Key Laboratory of Porous Metal Materials, Northwest Institute for Nonferrous Metal Research

School of Mechanical Engineering, Yeungnam University

References (19)

Show source-provided references
1. 1) A. Verma and D. C. Dube, J. Am. Ceram. Soc., 88, 519–523 (2005).10.1111/j.1551-2916.2005.00098.x ↗
2. 2) J. Azadmanjiri, Mater. Chem. Phys., 109, 109–112 (2008).10.1016/j.matchemphys.2007.11.001 ↗
3. 3) M. P. Reddy, W. Madhuri, N. R. Reddy, K. S. Kumar, V. Murthy and R. R. Reddy, J. Electroceram., 28, 1–9 (2012).10.1007/s10832-011-9670-7 ↗
4. 4) A. Costa, E. Tortella, M. Morelli, M. Kaufman and R. Kiminami, J. Mater. Sci., 37, 3569–3572 (2002).10.1023/A:1016528302082 ↗
5. 5) A. S. Albuquerque, J. D. Ardisson, W. A. A. Macedo and M. Alves, J. Appl. Phys., 87, 4352–4357 (2000).10.1063/1.373077 ↗
6. 6) S. Iijima, Nature, 354, 56–58 (1991).10.1038/354056a0 ↗
7. 7) L. Jiang and L. Gao, Chem. Mater., 15, 2848–2853 (2003).10.1021/cm030007q ↗
8. 8) Q. Huang and L. Gao, Appl. Phys. Lett., 86, 123104 (2005).10.1063/1.1884763 ↗
9. 9) X. B. Zhou, L. Shen, L. Li, S. H. Zhou, T. M. Huang, C. F. Hu, W. M. Pan, X. H. Jing, J. Sun and L. Gao, J. Eur. Ceram. Soc., 33, 2119–2126 (2013).10.1016/j.jeurceramsoc.2013.03.017 ↗
10. 10) E. T. Thostenson, Z. Ren and T. W. Chou, Compos. Sci. Technol., 61, 1899–1912 (2001).10.1016/S0266-3538(01)00094-X ↗
11. 11) Y. Q. Liu and L. Gao, Carbon, 43, 47–52 (2005).10.1016/j.carbon.2004.08.019 ↗
12. 12) M. Han and L. Deng, Appl. Phys. Lett., 90, 011108 (2007).10.1063/1.2429020 ↗
13. 13) J. Snoek, Physica, 14, 207–217 (1948).10.1016/0031-8914(48)90038-X ↗
14. 14) V. B. Bregar, IEEE Trans. Magn., 40, 1679–1684 (2004).10.1109/TMAG.2004.826622 ↗
15. 15) X. F. Zhang, X. L. Dong, H. Huang, Y. Y. Liu, W. N. Wang, X. G. Zhu, B. Lv and J. P. Lei, Appl. Phys. Lett., 89, 53115 (2006).10.1063/1.2236965 ↗
16. 16) J. J. Sun, J. B. Li, G. L. Sun and W. G. Qu, Ceram. Int., 28, 855–858 (2002).10.1016/S0272-8842(02)00064-0 ↗
17. 17) Q. Huang, D. Jiang, I. Ovid’Ko and A. Mukherjee, Scr. Mater., 63, 1181–1184 (2010).10.1016/j.scriptamat.2010.08.030 ↗
18. 18) G. D. Zhan, J. D. Kuntz, J. E. Garay and A. K. Mukherjee, Appl. Phys. Lett., 83, 1228–1230 (2003).10.1063/1.1600511 ↗
19. 19) F. Inam, H. Yan, D. D. Jayaseelan, T. Peijs and M. J. Reece, J. Eur. Ceram. Soc., 30, 153–157 (2010).10.1016/j.jeurceramsoc.2009.05.045 ↗