Semi-homogeneous joining of silicon nitride with a silicon nitride powder insert
Source abstract
Abstract
Silicon nitride was joined using a silicon nitride powder insert of the same composition as the bulk. The joining was performed at 1600°C for 30 min under a mechanical pressure of 13 MPa. The powder insert was densified to form a joint, but grains in the joint were small and equiaxed. As-joined specimens exhibited an average strength of 859 MPa. During heat treatment at 1800°C for 8 h, grain growth occurred, forming a microstructure with rod-like grains in the joint. The semi-homogeneous joint of the same composition and the similar microstructure consisting of rod-like grains to the bulk was successfully obtained. The average strength of the joined specimen was 947 MPa, which was nearly the same to that of the bulk silicon nitride.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Institute of Advanced Industrial Science and Technology (AIST)
References (10)
Show source-provided references
1. S. Kanzaki and H. Tabata · Yogyo-Kyokai-Shi · 1983 · 91 · 54
2. 10.1007/BF0123311810.1007/BF01233118 ↗
3. 10.1016/j.jeurceramsoc.2010.05.00910.1016/j.jeurceramsoc.2010.05.009 ↗
4. XIE R-J · J. Am. Ceram. Soc. · 2001 · 84 · 47110.1111/j.1151-2916.2001.tb00683.x ↗
5. 5) N. Kondo, H. Hyuga and H. Kita, Ceram. Eng. Sci. Proc., in press.
6. 10.1111/j.1151-2916.1991.tb06872.x10.1111/j.1151-2916.1991.tb06872.x ↗
7. KONDO N · J. Am. Ceram. Soc. · 1999 · 82 · 106710.1111/j.1151-2916.1999.tb01876.x ↗
8. BECHER P F · J. Am. Ceram. Soc. · 1998 · 81 · 282110.1111/j.1151-2916.1998.tb02702.x ↗
9. 10.1016/S0955-2219(97)00081-210.1016/S0955-2219(97)00081-2 ↗
10. J. Am. Ceram. Soc. · 1998 · 81 · 71310.1111/j.1151-2916.1998.tb02395.x ↗