journal article·2017Open access

Effects of pitch addition on the properties of environmental-friendly tap-hole clay

Lingyun WANG, Yucheng YIN, Wendong QIU, Yonghe LIANG, Guozhi RUAN, Lei ZHAO

Abstract

An environmentally friendly tap-hole clay that contains almost no benzo[a]pyrene was developed using resin and pitch as binder. The effects of the pitch addition on the tap-hole clay were investigated through evaluating the physical and chemical properties together with the microstructure, phase compositions and thermal analysis. The plasticity of the tap-hole clay is significantly improved with increasing pitch addition. However, the bulk density of tap-hole clay decreases gradually with increasing pitch content after treatment at different temperatures, while the apparent porosity increases due to the evaporation of pitch components and relatively low solid components. Also, this phenomenon is the main reason for the poor volume stability of tap-hole clay after heat treatment at different temperatures, although mullite formation has negated some of the shrinkage. Mechanical-strength evolution of the tap-hole clay is closely related to the carbonization process of the resin and pitch at high temperatures. Oxidation resistance could be significantly improved with 2 wt % of the pitch, but there is almost no change with much more than 2 wt %. However, the higher pitch content corresponds to better slag resistance. In terms of the comprehensive performance of the tap-hole clay, 4 wt % of the pitch would be better.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Natural Fiber Reinforced Composites · Dental materials and restorations · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology

Shanghai Baosteel Industry Technological Service Co.Ltd.

References (18)

Show source-provided references
1. 1) M. Swartling, B. Sundelin, A. Tilliander and P. Jönsson, Steel Res. Int., 81, 724–734 (2010).10.1002/srin.201000035 ↗
2. 2) I. F. Kurunov, V. N. Loginov and D. N. Tikhonov, Metallurgist, 50, 605–613 (2006).10.1007/s11015-006-0131-5 ↗
3. 3) M. Kitamura, R. Nakamura and H. Sumimura, Taikabutsu Overseas, 22, 277 (2002).
4. 4) S. Yang, J. Zhang, Y. Dong, S. Sun and P. Cui, Advanced Materials Research, 79–82, 2099–2102 (2009).10.4028/www.scientific.net/AMR.79-82.2099 ↗
5. 5) S. Tao, B. Li, Y. Zhang and H. Yuan, Environmental Science&Technology, 40, 702–708 (2006).10.1021/es0517062 ↗
6. 6) R. B. Finkelman and P. M. K. Gross, Int. J. Coal Geol., 40, 91–101 (1999).10.1016/S0166-5162(98)00061-5 ↗
7. 7) M. Pufulete, J. Battershill, A. Boobis and R. Fielder, Regulatory Toxicology and Pharmacology, 40, 54–66 (2004).10.1016/j.yrtph.2004.04.007 ↗
8. 8) C. E. Boström, P. Gerde, A. Hanberg, B. Jernström, C. Johansson, T. Kyrklund, A. Rannug, M. Törnqvist, K. Victorin and R. Westerholm, Environmental Health Perspectives, 110, 451–488 (2002).10.1289/ehp.110-1241197 ↗
9. 9) K. Straif, R. Baan, Y. Grosse, B. Secretan, F. E. Ghissassi and V. Cogliano, Lancet Oncol., 6, 931–932 (2005).10.1016/S1470-2045(05)70458-7 ↗
10. 10) G. Xu, W. Yue, M. He and H. Zhang, China’s Refractories, 20, 16–21 (2011).
11. 11) K. Curran, M. Underhill, L. T. Gibson and M. Strlic, Microchem. J., 124, 909–918 (2016).10.1016/j.microc.2015.08.027 ↗
12. 12) S. Masala, C. Bergvall and R. Westerholm, Sci. Total Environ., 432, 97–102 (2012).10.1016/j.scitotenv.2012.05.081 ↗
13. 13) F. Wang, L. Zhao, W. Fang, F. Liang, H. Chen, H. Chen and X. Du, Int. J. Appl. Ceram. Technol., 13, 133–139 (2016).10.1111/ijac.12426 ↗
14. 14) I. C. Lewis, New Carbon Materials, 5, 32–36, (1989).
15. 15) Y. Cheng, C. Fang and J. Su, Journal of Analytical and Applied Pyrolysis, 109, 90–97 (2014).10.1016/j.jaap.2014.07.009 ↗
16. 16) D. Cho, J. M. Kim and D. Kim, Mater. Lett., 104, 24–27 (2013).10.1016/j.matlet.2013.03.132 ↗
17. 17) N. Li, H. Gu and H. Zhao, “NAIHUOCAILIAOXUE (in chinese)”, Ed. by S. Cao, Metallurgical industry press, Beijing (2010) pp. 147–154.
18. 18) Y. Yin, Y. Liang, S. Ge, Z. Liu, J. Nie and J. Lu, Journal of Ceramic Society of Japan, 121, 873–879 (2013).10.2109/jcersj2.121.873 ↗