journal article·2020-12-01Open access

Strengthening in porcelain reinforced with alumina particles

Takashi AKATSU, Miho TOMIYASU, Takahito SHINGAE, Nobuaki KAMOCHI

Abstract

Alumina has long been known to enhance the strength of porcelain; however, the strengthening mechanism is not sufficiently understood. The strengthening in alumina-strengthened porcelain is examined on the basis of the change in thermal shrinkage of a porcelain matrix upon addition of various amounts of calcined talc. The improvement in flexural strength of the porcelain as a result of the alumina addition is enhanced with increasing difference in the thermal shrinkage between the alumina particle and the matrix. The rate of increase of the flexural strength as a function of the difference in thermal shrinkage is described by the extent to which the compressive prestress on the matrix increases the nominal tensile stress required for the fracture of the porcelain. However, the strengthening due to the internal stress is not sufficient to describe the actual strength of the porcelain. Further strengthening is achieved by the relatively large thermal shrinkage of alumina particles suppressing the formation and extension of microcracks around quartz grains in the glass phase of the porcelain.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Ceramic Research Center of Saga University

Faculty of Art and Regional Design, Saga University

Faculty of Science and Engineering, Saga University

Saga Ceramics Research Laboratory

References (40)

Show source-provided references
1. 1) C. R. Austin, H. Z. Schofield and N. L. Haldy, J. Am. Ceram. Soc., 29, 341–354 (1946).
2. 2) S. I. Warshaw and R. Seider, J. Am. Ceram. Soc., 50, 337–342 (1967).
3. 3) S. K. Khandelwal and R. L. Cook, Am. Ceram. Soc. Bull., 49, 522–526 (1970).
4. 4) Y. Kobayashi, O. Ohira, Y. Ohashi and E. Kato, J. Ceram. Soc. Jpn., 95, 887–892 (1987).
5. 5) Y. Kobayashi, O. Ohira, Y. Ohashi and E. Kato, J. Ceram. Soc. Jpn., 98, 504–509 (1990).
6. 6) Y. Kobayashi, O. Ohira, T. Satoh and E. Kato, J. Ceram. Soc. Jpn., 102, 383–387 (1994).
7. 7) R. Harada, N. Sugiyama, H. Shin and H. Ishida, J. Ceram. Soc. Jpn., 104, 1151–1155 (1996).
8. 8) N. Sugiyama, R. Harada and H. Ishida, J. Ceram. Soc. Jpn., 105, 126–130 (1997).
9. 9) Y. Kobayashi, O. Ohira and H. Isoyama, J. Ceram. Soc. Jpn., 111, 122–125 (2003).
10. 10) Y. Hirata, A. Yoshitomi and S. Sameshima, J. Ceram. Soc. Jpn., 111, 560–566 (2003).
11. 11) Y. Kobayashi, M. Yamada, M. Nakayama, O. Ohira and H. Isoyama, J. Ceram. Soc. Jpn., 111, 872–877 (2003).
12. 12) Y. Kobayashi, M. Mukai, T. Mizuno, O. Ohira and H. Isoyama, J. Ceram. Soc. Jpn., 113, 413–418 (2005).
13. 13) N. Kamochi, K. Nishiyama and H. Katsuki, J. Ceram. Soc. Jpn., 124, 787–790 (2016).
14. 14) H. Marzhal, Ber. Dtsch. Keram. Ges., 32, 203–211 (1955).
15. 15) L. Mattyascvszky-Zsolnay, J. Am. Ceram. Soc., 40, 299–306 (1957).
16. 16) A. Winterling, Ber. Dtsch. Keram. Ges., 38, 9–22 (1961).
17. 17) K. Hamano, Y. H. Wu, Z. Nakagawa and M. Hasegawa, J. Ceram. Soc. Jpn., 99, 153–157 (1991).
18. 18) K. Hamano and M. Hirayama, J. Ceram. Soc. Jpn., 102, 665–669 (1994).
19. 19) N. Yamamoto, Nichigai Review, 25, 17–22 (1962).
20. 20) A. Palatzky and T. Werner, Silikat. Tech., 9, 68–73 (1958).
21. 21) T. Weidmann, Sprechsaal, 92, 2–5 (1959).10.1002/cber.19590921125 ↗
22. 22) J. E. Schroeder, Am. Ceram. Soc. Bull., 57, 526 (1978).
23. 23) K. Niihara, J. Ceram. Soc. Jpn., 99, 974–982 (1991).
24. 24) Y. Wu and D. Wu, Research on the Development of Japanese Ceramics, Atlantis Press (2017).
25. 25) K. Yamamoto, Industrial district of Arita porcelain in southwestern Japan: Its struggle for revitalization under the long-term stagnation of Japanese economy, Kyushu University Economic Association (2016).
26. 26) JCRS203-1996, Testing Method for Flexural Strength of Strengthened Porcelain materials for Tableware, The Ceramic Society of Japan.
27. 27) ISO 14704:2000 Fine ceramics (advanced ceramics, advanced technical ceramics) –Test method for flexural strength of monolithic ceramics at room temperature.
28. 28) ISO 20501:2003 Fine ceramics (advanced ceramics, advanced technical ceramics) –Weibull statistics for strength data.
29. 29) S. N. Luko, SAE Transactions, 108, 398–412 (1999).
30. 30) V. Biasini, M. Dondi, G. Guarini, M. Raimondo, A. Argnani and S. Di Primio, Silic. Ind., 68, 67–73 (2003).
31. 31) R. Gill, Chemical fundamentals of geology and environmental geoscience, Wiley, Blackwell (2014).
32. 32) K. Kihara, Eur. J. Mineral., 2, 63–78 (1990).
33. 33) M. A. Carpenter, E. K. H. Salje, Graeme-Barber, B. Wruck, M. T. Dove and K. S. Knight, Am. Mineral., 83, 2–22 (1998).
34. 34) Y. Ohya, Y. Takahashi, M. Murata, Z. Nakawaga and K. Hamano, J. Am. Ceram. Soc., 82, 445–448 (1999).
35. 35) J. D. Eshelby, Proc. R. Soc. Lon. Ser.-A, 241, 376–396 (1957).
36. 36) T. Mori and K. Tanaka, Acta. Metall. Mater., 21, 571–574 (1973).
37. 37) K. Wakashima and H. Tsukamoto, Mat. Sci. Eng. A-Struct., 146, 291–316 (1991).
38. 38) K. Hamano, Yogyo-Kyokai-shi, 64, 167–179 (1956).10.2109/jcersj1950.64.726_167 ↗
39. 39) I. Takahashi, S. Usami, K. Nakakado, H. Miyata and S. Shida, Yogyo-Kyokai-shi, 93, 186–194 (1985).10.2109/jcersj1950.93.1076_186 ↗
40. 40) R. L. Bertolotti, J. Am. Ceram. Soc., 56, 107–110 (1973).