journal article·2008Open access

Borosilicate glasses with high softening points for glass-ceramic/copper multilayer substrates

Masahide OKAMOTO, Hirayoshi TANEI, Shoichi IWANAGA, Masato NAKAMURA, Shosaku ISHIHARA, Fumikazu TAGAMI, Kazuo SHINOZAKI

Journal of the Ceramic Society of Japan· Volume 116· Issue 1352

Abstract

We have developed borosilicate glasses with high softening points for glass-ceramic / copper multilayer substrates. The softening points of this glass ranged from 900°C to 1000°C. Glass-ceramics made using this glass barely sintered below 850°C, but sintered compactly at temperatures just below 1050°C. Green sheets made using this glass-ceramics could be fired around 850°C to remove the binder. Binder removal was caused very fast at this temperature. The glass-ceramics could be co-sintered with copper and had various advantages, such as easy binder removal, a coefficient of thermal expansion approximately equal to that of silicon, a low dielectric constant, sufficient flexural strength, and high water durability. These advantages helped make the manufacturing process of the substrate more productive.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Production Engineering Research Laboratory, Hitachi Ltd.

Industrial Property Cooperation Center

Hitachi Global Storage Technologies

Department of Metallurgy and Ceramics Science, Tokyo Institute of Technology

References (12)

Show source-provided references
1. 10.1111/j.1151-2916.1991.tb04320.x10.1111/j.1151-2916.1991.tb04320.x ↗
2. 2) A. H. Kumar, S. Knickerbocker and R. R. Tummala, Proceedings of 42nd Electronic Components & Technology Conference, 678-681 (1992).
3. 3) R. N. Master, L. W. Herron and R. R. Tummala, IEEE Trans. On Comp., Hybrid & Manuf. Tech., 14[4], 780-783 (1991).10.1109/33.105133 ↗
4. 4) S. H. Kinckerbocker, A. H. Kumar and L. W. Herron, Am Ceram Soc Bull, 72[1], 90-95 (1993).
5. 5) K. Niwa, N. Kamehara, K. Yokouchi and Y. Imanaka, Advanced Ceramic Materials, 2, No. 4, October, 832-835 (1987).10.1111/j.1551-2916.1987.tb00157.x ↗
6. 6) K. Niwa, N. Kamehara, H. Yokoyama, K. Yokouchi and Y. Imanaka, Advanced in Ceramics, 19, 41-47 (1987).
7. 7) K. Niwa, Y. Imanaka, N. Kamehara and S. Aoki, Advances in Ceramics, 26, 323-337 (1989).
8. 8) N. Kamehara, Y. Imanaka and K. Niwa, Denshi Tokyo, 26, 143-148 (1987).
9. 9) Y. Shimada, K. Utsumi, M. Suzuki and H. Takamizawa, Electron Compon Conf, 33, 314-319 (1983).
10. 10) J. H. Jean, Jpn. J. Appl. Phys., 35, L429-L431 (1996).10.1143/JJAP.35.L429 ↗
11. 11) P. B. Adams and D. D. Evans, Mater. Sci. Res., 12, 525-537 (1978).10.1007/978-1-4684-3357-9_28 ↗
12. 12) B. C. Bunker, D. R. Tallant and T. J. Headley et al., Phys. and Chem. of Glasses, 29[3], 106-120 (1988).