We have for the first time fabricated the textured ceramics of doped lanthanum silicate oxyapatite (LSO) by templated grain growth method. Tabular template particles of K2O- and F-doped LSO with well-developed {001} faces were grown by KF flux method, and aligned in BaO-doped LSO matrix by tape casting. The tapes were punched out into disk-shaped pieces, stacked in two layers, and sintered at 1873 K for 50 h. We obtained a disk-shape K2O- and BaO-doped LSO polycrystal aligned in the c-axis with small amounts of two types of interstitial materials. The texture fraction of apatite {0 0 l} planes was 0.45. The doped LSO was characterized by the heterogeneous distribution of K2O, the component of which originated from the template particles, within the crystal grains. The chemical formula of the doped LSO was derived from the average composition to be (La8.43K0.03Ba1.43□0.11)Σ=10(Si5.96□0.04)Σ=6O26, where □ denotes vacancies in La and/or Si sites. One type of the interstitial materials was composed mainly of BaO and La2O3, and the other was rich in SiO2. As the temperature increased from 773 to 1023 K, the bulk oxide-ion conductivity (σ) steadily increased from 1.89 × 10−4 to 2.48 × 10−3 S cm−1, with the activation energy of conduction (Ea) being 0.78 eV. The σ-values of randomly oriented polycrystal with the same bulk chemical composition steadily increased from 3.89 × 10−5 to 4.99 × 10−4 S cm−1 with increasing temperature from 773 to 1023 K (Ea = 0.78 eV). When the σ-values were compared at the same temperatures, they were 6.7 (973 K)–8.2 (923 K) times higher for the former polycrystal than for the latter. The larger σ-values of the c-axis-aligned polycrystal would be principally induced by the substantially higher oxide-ion conductivity along the c-axis than along the other directions in K2O- and BaO-doped LSO.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Ferroelectric and Piezoelectric Materials · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Life Science and Applied Chemistry, Nagoya Institute of Technology
Department of Earth and Planetary Science, Graduate School of Science, The University of Tokyo
References (28)
Show source-provided references
1. 1) S. Nakayama, T. Kageyama, H. Aono and Y. Sadaoka, J. Mater. Chem., 5, 1801–1805 (1995).
2. 2) S. Nakayama and M. Sakamoto, J. Eur. Ceram. Soc., 18, 1413–1418 (1998).
3. 3) S. Nakayama and H. Highchi, J. Mater. Sci. Lett., 20, 913–915 (2001).
4. 4) S. Beaudet-Savignat, A. Vincent, S. Lambert and F. Gervais, J. Mater. Chem., 17, 2078–2087 (2007).
5. 5) K. Fukuda, T. Asaka, S. Hara, M. Oyabu, A. Berghout, E. Béchade, O. Masson, I. Julien and P. Thomas, Chem. Mater., 25, 2154–2162 (2013).
6. 6) K. Fukuda, R. Watanabe, M. Oyabu, R. Hasegawa, T. Asaka and H. Yoshida, Cryst. Growth Des., 16, 4519–4525 (2016).
7. 7) K. Fukuda, T. Asaka, R. Hamaguchi, T. Suzuki, H. Oka, A. Berghout, E. Béchade, O. Masson, I. Julien, E. Champion and P. Thomas, Chem. Mater., 23, 5474–5483 (2011).
8. 8) K. Fukuda, T. Asaka, S. Hara, A. Berghout, E. Béchade, O. Masson, J. Jouin and P. Thomas, Cryst. Growth Des., 15, 3435–3441 (2015).
9. 9) R. Hasegawa, M. Okabe, T. Asaka, N. Ishizawa and K. Fukuda, J. Solid State Chem., 229, 252–259 (2015).
10. 10) K. Fukuda, S. Hasegawa, E. Hasegawa, D. Urushihara and T. Asaka, J. Ceram. Soc. Jpn., 127, 150–157 (2019).
11. 11) G. L. Messing, S. Trolier-McKinstry, E. M. Sabolsky, C. Duran, S. Kwon, B. Brahmaroutu, P. Park, H. Yilmaz, P. W. Rehrig, K. B. Eitel, E. Suvaci, M. Seabaugh and K. S. Oh, Crit. Rev. Solid State Mater. Sci., 29, 45–96 (2004).
12. 12) T. Kimura, J. Ceram. Soc. Jpn., 114, 15–25 (2006).
13. 13) M. Hillert, Acta Metall., 13, 227–238 (1965).
14. 14) M. M. Seabaugh, I. H. Kerscht and G. L. Messing, J. Am. Ceram. Soc., 80, 1181–1888 (1997).
15. 15) K. Fukuda, Y. Tsunoda, D. Urushihara, T. Asaka and H. Yoshida, J. Ceram. Soc. Jpn., 127, 143–149 (2019).
16. 16) S.-J. L. Kang, Sintering: Densification, Grain Growth, and Microstructure. Elsevier Butterworth-Heinemann (2005).
17. 17) I.-J. Bae and S. Baik, J. Am. Ceram. Soc., 80, 1149–1156 (1997).
18. 18) A. Le Bail, H. Duroy and J. L. Fourquet, Mater. Res. Bull., 23, 447–452 (1988).
19. 19) F. Izumi and K. Momma, Solid State Phenom., 130, 15–20 (2007).
20. 20) H. Okudera, Y. Masubuchi, S. Kikkawa and A. Yoshiasa, Solid State Ionics, 176, 1473–1478 (2005).10.1016/j.ssi.2005.02.014 ↗
21. 21) F. K. Lotgering, J. Inorg. Nucl. Chem., 9, 113–123 (1959).
22. 22) H. Sumi, H. Shimada, Y. Yamaguchi, T. Yamaguchi and Y. Fujishiro, Electrochim. Acta, 339, 135913 (2020).10.1016/j.electacta.2020.135913 ↗
23. 23) D. Johnson, ZView Program (Version 2.9b), Scribner Associ-ates Inc., Southern Pines, NC (1990).
24. 24) W. S. Rasband, ImageJ Program, U. S. National Institutes of Health, Bethesda, Maryland, USA, https://imagej.nih.gov/ij/, 1997–2018.
25. 25) E. M. Levin, C. R. Robbins and H. F. McMurdie, eds. Phase Diagrams for Ceramists, Vol. I, Fig. 209. The American Ceramic Society, Columbus, OH (1964).
26. 26) N. A. Toropov, I. A. Bondar and F. Y. Galakhov, Trans. Int. Ceram. Congr., 8th, Copenhagen, Denmark (1962) pp. 85–103.
27. 27) J. T. S. Irvine, D. C. Sinclair and A. R. West, Adv. Mater., 2, 132–138 (1990).
28. 28) X. Vendrell and A. R. West, J. Electrochem. Soc., 165, F966–F975 (2018).10.1149/2.0881811jes ↗