article·1998-01-01Open access

Preparation of High Fracture Toughness Alumina Sintered Bodies from Bayer Aluminum Hydroxide

Yu‐ichi Yoshizawa, Motohiro Toriyama, Shuzo Kanzaki

Abstract

The mechanical properties of hot-pressed, low-temperature-calcined α-alumina powder made from commercial aluminum hydroxide by seeding of wet grinding abrasion powder were investigated. The microstructure of samples sintered at low temperature is composed of very fine equiaxial grains and its bending strength is higher than 800MPa. As the sintering temperature increases, the grains become large and uniaxially elongated, the bending strength of sintered bodies decreases, and the fracture toughness increases. A sample sintered at 1400°C shows a bending strength of 600MPa and a fracture toughness of 7.9MPa⋅m1/2 (SEPB method). A maximum fracture toughness of 9.0MPa⋅m1/2 is achieved in a sample sintered at 1600°C. This high fracture toughness is caused by a uniform and elongated grain structure, and by increment of grain boundary fracture.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Bauxite Residue and Utilization · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.