Pressureless Sintering of TiB2-Al2O3
Source abstract
Abstract
Sintering conditions and mechanical properties of TiB2-Al2O3 composites produced by pressureless sintering at 1600° to 1900°C by using two types of TiB2 powder with different average particle size were investigated. The content of more than 40wt% Al2O3 yielded the composites having relative density of more than 95%. The bending strength of the composite containing coarse TiB2 powder and 60wt% Al2O3 was 300MPa. And that of the composite containing fine TiB2 powder and 50wt% Al2O3 was 450MPa. The Vickers hardness of the composites were about 15GPa. The electrical resistivity increased with increasing amount of Al2O3 and changed drastically from about 10-3Ω·cm to 105Ω·cm for 75wt% to 95wt% addition of Al2O3.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.