Preparation of Dense Negative-Thermal-Expansion Oxide by Rapid Quenching of ZrW2O8 Melt.
Source abstract
Abstract
By rapid quenching of ZrW2O8 melt from 1300°C, dense specimens with few inner pores were successfully prepared. Dilatometry experiments were performed and an abrupt thermal expansion was observed in the range 120-160°C, probably due to removal of internal stress upon the first heating measurement from room temperature to 300°C. The specimen annealed at 200°C for removal of internal stress exhibited a negative average thermal expansion coefficient of -(4-5)×10-6K-1 from room temperature to 250°C, which was smaller than that of sintered ceramic ZrW2O8, (-(6-10)×10-6K-1). X-ray diffraction and secondary electron microscopy measurements revealed that the obtained specimen was a hybrid of ZrO2 and/or WO3 grains with -1μm diameter and ZrW2O8 grains with 10-25μm diameter. The smaller negative thermal expansion could be attributed to this hybridization due to decomposition of ZrW2O8 during the quenching process.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Thermal Expansion and Ionic Conductivity · Thermal and Kinetic Analysis · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.