Sintering of CaO-ZrO2 Composite and Its Property of Slaking Resistance.

Min Chen, Akira Yamaguchi

Abstract

CaO-ZrO2 composite was sintered at 1500°C by addition of ZrO2 to 20 mol%. ZrO2 reacted with CaO to form CaZrO3 that promoted densification of the clinker by restraining growth of CaO grains. The formed CaZrO3 was mainly located within CaO grains when a small amount of ZrO2 was doped, while it localized at CaO boundaries with increasing the amount of added ZrO2. Protective layer, consisting of CaZrO2 crystalline that encompassed most of CaO grains, formed when the content of ZrO2 was increased to 20 mol%. The slaking resistance was effectively increased owing to the promotion of densification when a small amount of ZrO2 was added, and it was increased further by conversion of free CaO into CaZrO3 with increasing the content of ZrO2. Especially when a protective layer was formed, the slaking resistance of the clinker increased significantly. The mass gain of CaO clinker without ZrO2 was 5.8% which decreased to 0.4% by increasing ZrO2 content to 20 mol% after slaking for 96h at 70°C in 90% humidity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.