Abstract

Cell performance was measured at 773-1073 K for Ni-GDC(Gd-doped ceria) anode-supported GDC film (60 μm thickness) with SrRuO3 cathode using a 3 vol% H2O-containing H2 fuel. Reduction of particle size (< 1 μm) of SrRuO3 cathode was effective to decrease the voltage drop at the cathode because of the increased length of triple phase boundary (GDC electrolyte-SrRuO3 cathode-O2 gas). Open circuit voltage (OCV) of GDC electrolyte in an anode atmosphere without H2 fuel was close to the value calculated by Nernst equation for no electronic conduction. However, the OCV in a H2-containing atmosphere decreased from the values by Nernst equation owing to the increased electronic conduction in a GDC film. This tendency of decrease in OCV became significant for thinner GDC film. This result was interpreted by the dissolution and dissociation of H2 fuel in a GDC film to form protons and electrons (H2 → 2H+ + 2e-).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry, Biotechnology, and Chemical Engineering, Kagoshima University

Fine Particle Processing Group, Nano Ceramics Center, National Institute for Materials Science

References (26)

Show source-provided references
1. 1) M. Nagamori, T. Shimonosono, S. Sameshima, Y. Hirata, N. Matsunaga and Y. Sakka, J. Am. Ceram. Soc., 92[S1], S117-S121 (2009).10.1111/j.1551-2916.2008.02646.x ↗
2. 10.1016/j.ssi.2004.02.02610.1016/j.ssi.2004.02.026 ↗
3. 10.1149/1.209718710.1149/1.2097187 ↗
4. 4) J. Lane, P. H. Middleton, H. Fox, B. C. H. Steel and K. Kilner, "Proceedings of Second International Symposium on Ionic and Mixed Conducting Ceramics," Ed. by T. A. Ramanayanan, W. L. Worrell and H. L. Tuller, The Electrochemical Society Proceeding Series, Pennington, N. J. (1994) pp.489-504.
5. 10.1149/1.183878310.1149/1.1838783 ↗
6. 6) T. Shimonosono, G. Hiramatsu, Y. Hirata, S. Sameshima, N. Matsunaga, T. Doi and T. Horita, Adv. Mater. Res., 26-28, 275-278 (2007).10.4028/www.scientific.net/AMR.26-28.275 ↗
7. 7) S. Sridhar and U. B. Pal, Powd. Tech., 88,173-178 (1996).10.1016/0032-5910(96)03114-2 ↗
8. 10.1007/BF0035665110.1007/BF00356651 ↗
9. 10.1016/S0167-2738(00)00624-X10.1016/S0167-2738(00)00624-X ↗
10. 10.1016/S0167-2738(97)00309-310.1016/S0167-2738(97)00309-3 ↗
11. 10.1016/0167-2738(94)90155-410.1016/0167-2738(94)90155-4 ↗
12. SHIMONOSONO TARO · 2005 · 88 · 211410.1111/j.1551-2916.2005.00401.x ↗
13. SHIMONOSONO T · 2004 · 112 · S616
14. 14) S. Sameshima, Y. Hirata and Y. Ehira, J. Alloys Comp., 408-412, 628-631 (2006).10.1016/j.jallcom.2004.12.072 ↗
15. HIGASHI K · 1999 · 14 · 95710.1557/JMR.1999.0127 ↗
16. SAMESHIMA S · 2000 · 108 · 98510.2109/jcersj.108.1263_985 ↗
17. 10.1016/j.jeurceramsoc.2004.01.01110.1016/j.jeurceramsoc.2004.01.011 ↗
18. OKAWA Y · 2002 · 17 · 226610.1557/JMR.2002.0333 ↗
19. UCHIDA S · 2001 · 109 · 10010.2109/jcersj.109.1266_100 ↗
20. 20) T. Shimonosono, Ph. D. Thesis, Department of Advanced Nanostructured Materials Science and Technology, Kagoshima University, 2008.
21. HIRATA Y · 1990 · 98 · 12610.2109/jcersj.98.126 ↗
22. 10.2109/jcersj2.116.48610.2109/jcersj2.116.486 ↗
23. 10.1016/S0167-2738(99)00192-710.1016/S0167-2738(99)00192-7 ↗
24. 24) G. Hiramatsu, Y. Hirata, S. Sameshima and N. Matsunaga, Mater. Sci. Forum, 544-545, 985-988 (2007).10.4028/www.scientific.net/MSF.544-545.985 ↗
25. 25) Y. Hirata, S. Sameshima and G. Hiramatsu, Proc.23rd Inter. Korea-Japan Seminar on Ceramics (2006) pp. 93-96.
26. 10.1016/0167-2738(92)90102-U10.1016/0167-2738(92)90102-U ↗