Novel co-precipitation derived nanostructured LSM-YSZ cathode for intermediate temperature solid oxide fuel cells
Source abstract
Abstract
Strontium doped lanthanum manganite ((La0.85Sr0.15)0.98MnO3; LSM)/yttria-stabilized zirconia (YSZ) nanocomposite particles were synthesized through a novel co-precipitation method using YSZ nanoparticles with the average size of 3 nm as seed crystals. Phase evolution studies indicated that crystalline LSM/YSZ phases were obtained by calcining the co-precipitated precursor above 700°C. The nanocomposite particles calcined at 1000°C were screen printed on YSZ dense electrolytes and then sintered at 1100°C for cathode fabrication. The resulting cathode had a uniform porous structure consisting of fine grains ∼100 nm in size, and exhibited low polarization resistance of 2.82, 1.18, 0.48 and 0.25 Ω·cm2 at 650, 700, 750 and 800°C, respectively under air atmosphere. These results indicated that the present nanostructured cathode may be applicable for intermediate temperature solid oxide fuel cells.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Joining and Welding Research Institute, Osaka University
New Technology Research Laboratory, Sumitomo Osaka Cement Co., Ltd
References (21)
Show source-provided references
1. 10.1023/A:100488182571010.1023/A:1004881825710 ↗
2. 10.1016/0167-2738(92)90161-H10.1016/0167-2738(92)90161-H ↗
3. 10.1149/1.183647610.1149/1.1836476 ↗
4. 4) F. H. van Heuveln, H. J. M. Bouwmeester and F. P. F. van Berkel, J. Electrochem. Soc., 144, 126-133 (1996).10.1149/1.1837374 ↗
5. 10.1016/j.ssi.2007.05.00510.1016/j.ssi.2007.05.005 ↗
6. 10.1016/j.jpowsour.2003.09.05510.1016/j.jpowsour.2003.09.055 ↗
7. 10.1023/A:101795322885410.1023/A:1017953228854 ↗
8. 10.1007/s10008-007-0317-110.1007/s10008-007-0317-1 ↗
9. 10.1021/ja027881p10.1021/ja027881p ↗
10. 10.1016/j.jpowsour.2008.12.03810.1016/j.jpowsour.2008.12.038 ↗
11. 10.1016/j.jeurceramsoc.2008.07.05010.1016/j.jeurceramsoc.2008.07.050 ↗
12. 10.1016/j.scriptamat.2005.02.02010.1016/j.scriptamat.2005.02.020 ↗
13. 10.1016/S0167-2738(98)00195-710.1016/S0167-2738(98)00195-7 ↗
14. SHINOHARA N · 2000 · 83 · 163310.1111/j.1151-2916.2000.tb01442.x ↗
15. 10.1016/j.jallcom.2007.02.09210.1016/j.jallcom.2007.02.092 ↗
16. 10.1016/j.ceramint.2008.06.01810.1016/j.ceramint.2008.06.018 ↗
17. 10.1016/S0167-2738(01)00877-310.1016/S0167-2738(01)00877-3 ↗
18. 10.1111/j.1151-2916.1989.tb06209.x10.1111/j.1151-2916.1989.tb06209.x ↗
19. 19) W. D. Kingery and B. Francois, "Sintering and Related phenomena," Ed. by G. C. Kuczynski, N. A. Hooton and G. N. Gibbon, Gordon and Breach, New York (1967) pp. 471-498.
20. 10.1023/B:JACH.0000016627.29374.2410.1023/B:JACH.0000016627.29374.24 ↗
21. 10.1016/S0167-2738(98)00142-810.1016/S0167-2738(98)00142-8 ↗