Effect of sintering temperature and time on microwave dielectric properties of Nd2WO6 ceramics
Source abstract
Abstract
The microwave dielectric properties of Nd2WO6 ceramics were investigated with a view to their application in mobile communication. Nd2WO6 ceramics were prepared by the conventional solid–state method with various sintering temperatures and sintering times. A maximum density of 7.45 g/cm3 and an open porosity of 2.1% were obtained for Nd2WO6 ceramic, sintered at 1500°C for 4 h. A dielectric constants (εr) of 15.6, a quality factor (Q×f) of 50,600 GHz, and a temperature coefficient of resonant frequency (τf) of −65 ppm/°C were obtained when Nd2WO6 ceramics that were sintered at 1500°C for 4 h.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Electrical Engineering, Lunghua University of Science and Technology
References (15)
Show source-provided references
1. 1) Y. B. Chen, J. Ceram. Soc. Japan, 123, 374–377 (2015).
2. 2) Y. B. Chen, J. Ceram. Soc. Japan, 122, 708–713 (2014).
3. 3) Y. B. Chen, J. Ceram. Soc. Japan, 122, 955–958 (2014).
4. 4) F. De Smet, M. Devillers, C. Poleunis and P. Bertrand, J. Chem. Soc., Faraday Trans., 94, 941–947 (1998).10.1039/a707883h ↗
5. 5) F. De Smet, P. Ruiz, B. Delmon and M. Devillers, J. Phys. Chem. B, 105, 12355–12363 (2001).10.1021/jp0124600 ↗
6. 6) Y. C. Chen and M. Z. Weng, J. Mater. Sci.: Mater. Electron., 26, 853–859 (2015).
7. 7) E. S. Kim, B. S. Chun, R. Freer and R. J. Cernik, J. Eur. Ceram. Soc., 30, 1731–1736 (2010).10.1016/j.jeurceramsoc.2009.12.018 ↗
8. 8) B. W. Hakki and P. D. Coleman, IRE. Trans. Microwave Theory Tech., 8, 402–410 (1960).10.1109/TMTT.1960.1124749 ↗
9. 9) Y. Kobayashi and M. Katoh, IEEE Trans. Microwave Theory Tech., 33, 586–592 (1985).10.1109/TMTT.1985.1133033 ↗
10. 10) Y. Tohdo, K. Kakimoto, H. Ohsato, H. Yamada and T. Okawa, J. Eur. Ceram. Soc., 26, 2039–2043 (2006).10.1016/j.jeurceramsoc.2005.09.098 ↗
11. 11) R. D. Shannon, J. Appl. Phys., 73, 348–366 (1993).10.1063/1.353856 ↗
12. 12) C. Veneis, P. K. Davies, T. Negas and S. Bell, Mater. Res. Bull., 31, 431–437 (1996).10.1016/S0025-5408(96)00028-1 ↗
13. 13) B. D. Silverman, Phys. Rev., 125, 1921–1930 (1962).10.1103/PhysRev.125.1921 ↗
14. 14) W. S. Kim, T. H. Hong, E. S. Kim and K. H. Yoon, Jpn. J. Appl. Phys., 37, 3567–3571 (1998).
15. 15) A. J. Bosman and E. E. Havinga, Phys. Rev., 129, 1593–1600 (1963).10.1103/PhysRev.129.1593 ↗