Corrosion Behavior of Silicon Nitride Ceramics in Aqueous Solutions (Part 3)

Satoshi Iio, Akira Okada, Tetsuo Asano, Masahiro Yoshimura

Abstract

Corrosion behavior of gas pressure sintered silicon nitride ceramics was investigated in sulfuric acid solution with respect to the effect of solution temperature and to the microstructure of corroded layer. Weight loss of samples after corrosion test was severe in boiling solution as compared with in 90°C solution. Nevertheless strength degradation occurred similarly in each solution. The gradual growth of corrosion is considered to be controlled by the dissolution reaction of grain boundary phase of silicon nitride ceramics in sulfuric acid solution. The drastic strength degradation at initial stage is considered to be ascribed to the relaxation of the residual compressive stress during corrosion which was introduced on surfaces of specimens by machining.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.