Abstract

Aluminum nitride nanopowder was fabricated from transition alumina nanopowder by gas reduction–nitridation method. It was sintered by spark plasma sintering with 1 wt % Ca3Al2O6 as a sintering additive in nitrogen. The nanopowder with Ca3Al2O6 was densified up to 3.16 Mg/m3 of density at 1450°C, restraining grain growth. The nanopowder without additive was densified at 1550°C. The sintering temperature for dense aluminum nitride ceramic could be reduced by 1 wt % Ca3Al2O6 as a sintering additive.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Acoustic Wave Resonator Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Institute for Materials Science, Nano-Ceramics Center

Graduate School of Engineering, Hosei University

Department of Chemical Science and Technology, Hosei University

References (20)

Show source-provided references
1. 10.1007/BF0072097410.1007/BF00720974 ↗
2. 10.1063/1.319414810.1063/1.3194148 ↗
3. HOTTA NORIYASU · J. Ceram. Soc. Japan · 1988 · 96 · 73110.2109/jcersj.96.731 ↗
4. 10.1063/1.10111110.1063/1.101111 ↗
5. PANCHU1A M L · J. Am. Ceram. Soc. · 2003 · 86 · 111410.1111/j.1151-2916.2003.tb03433.x ↗
6. PATHAK L C · J. Am. Ceram. Soc. · 1999 · 82 · 25710.1111/j.1151-2916.1999.tb01757.x ↗
7. 10.1016/j.msea.2008.05.02710.1016/j.msea.2008.05.027 ↗
8. 10.1111/j.1151-2916.2003.tb03420.x10.1111/j.1151-2916.2003.tb03420.x ↗
9. 10.1111/j.1551-2916.2005.00715.x10.1111/j.1551-2916.2005.00715.x ↗
10. 10) T. Suehiro, N. Hirosaki and K. Komeya, Nanotechnology, 14, 487–491 (2003).10.1088/0957-4484/14/5/301 ↗
11. PANCHU1A M L · J. Am. Ceram. Soc. · 2003 · 86 · 112110.1111/j.1151-2916.2003.tb03434.x ↗
12. 12) K. Komeya, H. Inoue and A. Tsuge, J. Ceram. Soc. Japan, 88, 330–336 (1981).10.2109/jcersj1950.89.1030_330 ↗
13. 10.1111/j.1151-2916.1996.tb08024.x10.1111/j.1151-2916.1996.tb08024.x ↗
14. 14) C.-F. Yang, C.-M. Cheng, H.-H. Chung and C.-C. Chan, Key Eng. Mater., 336–338, 1868–1871 (2007).10.4028/www.scientific.net/KEM.336-338.1868 ↗
15. 15) Y. Xiong, Z. Fu and H. Wang, Key Eng. Mater., 368–372, 970–972 (2008).10.4028/www.scientific.net/KEM.368-372.970 ↗
16. 16) H. S. Zhao, L. Chen, N.-Z. Gao, K. H. Zhang and Z.-Q. Li, J. Zhejiang Univ., Sci., A, 10, 109–113 (2009).10.1631/jzus.A0820397 ↗
17. T. Honma, Y. Kuroki, T. Okamoto, M. · Ceram. Int. · 2008 · 34 · 94310.1016/j.ceramint.2007.09.062 ↗
18. 10.1088/1468-6996/10/5/05300110.1088/1468-6996/10/5/053001 ↗
19. 10.2109/jcersj2.116.78110.2109/jcersj2.116.781 ↗
20. 20) E. M. Levin, C. R. Robbins and H. F. McMurdie, “Phase Diagram for Ceramists,” Ed. and Publ. by The American Ceramic Society (1964) p. 102.