Corrosion and oxidation behaviour of .BETA.-SiAlON ceramics via different processing route
Source abstract
Abstract
The corrosion resistance of β-SiAlON based advanced ceramic materials in molten aluminum, equimolar NaCl-KCl melt and also in the melted mixture of NaF and AlF3 (molar ratio 1 : 1.163) were investigated. Two kinds of β-SiAlONs were tested; β-SiAlON prepared from powder precursors produced by carbothermal reduction and nitridation (CRN) of pyrophyllite and β-SiAlON made from commercial powders (AlN, Al2O3 and Si3N4). Corrosion tests were realized at 760°C for 7, 36 and 72 h under nitrogen atmosphere by dip-finger test method. All types of β-SiAlONs have great corrosion resistance against molten aluminum and NaCl-KCl melt at these conditions. The results of corrosion test were different for the β-SiAlONs in molten fluorides. While the corroded zone was only about 100 μm deep after 72 h corrosion test in reference β-SiAlON prepared from synthetic powders (SiAlON-R), in sample prepared from CRN pyrophyllite (SiAlON-P) it was almost 230 μm thick. Additionally, the oxidation resistance of β-SiAlONs was tested. The results showed that both SiAlON-P and reference SiAlON-R have comparable good oxidation resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Inorganic Chemistry, Slovak Academy of Sciences
VOP-026 Sternberk, s. p., Division VTUO Brno
Institute of Science and Technology for Ceramics, National Research Council
References (22)
Show source-provided references
1. 1) F. L. Riley, Key Eng. Mater., 113, 1-14 (1996).10.4028/www.scientific.net/KEM.113.1 ↗
2. 10.1016/0955-2219(92)90101-I10.1016/0955-2219(92)90101-I ↗
3. 10.1016/0955-2219(94)90006-X10.1016/0955-2219(94)90006-X ↗
4. 4) L. Mouradoff, P. Tristant, J. Desmaison, J. C. Labbe, M. Desmaison-Brut and R. Rezakhanlou, Key Eng. Mater., 113, 177-186 (1996).10.4028/www.scientific.net/KEM.113.177 ↗
5. 10.1016/j.jeurceramsoc.2004.03.02110.1016/j.jeurceramsoc.2004.03.021 ↗
6. 6) C. Santos, S. Ribeiro, K. Strecker, D. Rodrigues Jr. and C. R. M. Silva , J. Mater. Process. Tech., 184, 108-114 (2007).10.1016/j.jmatprotec.2006.11.012 ↗
7. 7) L. T. Dower and K. Coley, Key Eng. Mater., 113, 167-176 (1996).10.4028/www.scientific.net/KEM.113.167 ↗
8. 1986 · 85 · 161
9. 10.1007/BF0035680810.1007/BF00356808 ↗
10. 1988 · 3 · 36910.1111/j.1551-2916.1988.tb00236.x ↗
11. 10.1007/BF0054049710.1007/BF00540497 ↗
12. 10.1007/BF0054465110.1007/BF00544651 ↗
13. 13) G. Sucik, T. Kuffa and D. Hrsak, Metalurgija, 43, 93-95 (2004).
14. 10.1016/S0955-2219(03)00335-210.1016/S0955-2219(03)00335-2 ↗
15. 15) A. Solheim and A. Sterten, Proceedings of the Ninth International Symposium on Light Metals, Trondheim, Norway, 225-234 (1997).
16. 16) M. Takeuchi, T. Kato, K. Hanada, T. Koizumi and S. Aose, J. Phys. Chem. Solids, 66, 521-525 (2005).10.1016/j.jpcs.2004.06.046 ↗
17. 10.1016/j.jeurceramsoc.2006.08.01210.1016/j.jeurceramsoc.2006.08.012 ↗
18. 18) E. Jorge, O. Marguin, L. Moitrier and O. Citti, USPTO Applicaton No. 20080234122 - Class: 501 92, (2008).
19. 19) P. A. Foster, J. Am. Ceram. Soc., 58, 288-291 (1975).10.1111/j.1151-2916.1975.tb11477.x ↗
20. 10.1016/0955-2219(94)90026-410.1016/0955-2219(94)90026-4 ↗
21. 21) R. Ramesh, P. Byrne and M. J. Pomeroy, J. Mater. Process. Tech., 56, 600-608 (1996).10.1016/0924-0136(95)01874-3 ↗
22. 10.1016/j.jeurceramsoc.2007.09.04110.1016/j.jeurceramsoc.2007.09.041 ↗