journal article·2019-07-01Open access

Rapid reaction sintering of silicon carbide using Nd:YAG laser

Satoshi SUEHIRO, Teiichi KIMURA

Abstract

Reaction sintering of silicon carbide (SiC) using a continuous-wave Nd:YAG laser as a heating source was investigated. The laser was used to irradiate pellets of a stoichiometric powder mixture of Si and C under Ar gas flow. At an appropriate laser power, a dense SiC layer was formed consisting of grains with a size of 100–500 nm; this layer was several micrometers thick. At lower laser power, fine grains of SiC were formed and dispersed in the unreacted Si–C matrix. On the other hand, at higher power, larger faceted SiC grains (1–3 µm) were formed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Research and Development Laboratory, Japan Fine Ceramics Center

References (17)

Show source-provided references
1. 1) R. Naslain, Compos. Sci. Technol., 64, 155–170 (2004).
2. 2) W. J. Clegg, K. Kendall, N. McN. Alford, T. W. Button and J. D. Birchall, Nature, 347, 455–457 (1990).10.1038/347455a0 ↗
3. 3) S. R. Levine, E. J. Opila, M. C. Halbig, J. D. Kiser, M. Singh and J. A. Salem, J. Eur. Ceram. Soc., 22, 2757–2767 (2002).
4. 4) T. Ishikawa, Y. Kohtoku, K. Kumagawa, T. Yamamura and T. Nagasawa, Nature, 391, 773–775 (1998).10.1038/35820 ↗
5. 5) R. Riedel, G. Passing, H. Schönfelder and R. J. Brook, Nature, 355, 714–717 (1992).10.1038/355714a0 ↗
6. 6) S. Suyama, T. Kameda and Y. Itoh, Diamond Relat. Mater., 12, 1201–1204 (2003).
7. 7) W. E. Frazier, J. Mater. Eng. Perform., 23, 1917–1928 (2014).
8. 8) D. Herzog, V. Seyda, E. Wycisk and C. Emmelmann, Acta. Mater., 117, 371–392 (2016).
9. 9) C. Y. Yap, C. K. Chua, Z. L. Dong, Z. H. Liu, D. Q. Zhang, L. E. Loh and S. L. Sing, Appl. Phys Rev., 2, 041101 (2015).10.1063/1.4935926 ↗
10. 10) H. J. Su, J. Zhang, L. Liu, J. Eckert and H. Z. Fu, Appl. Phys. Lett., 99, 221913–222915 (2011).
11. 11) A. Gahler, J. G. Heinrich and J. Günster, J. Am. Ceram. Soc., 89, 3076–3080 (2006).
12. 12) X. Ma, J. Li, Z. Peng, B. Ma, X. Li, W. Pan and L. Qi, Cryst. Growth Des., 15, 5652–5655 (2015).
13. 13) D. Gu, D. Dai, G. Zhang and H. Wang, Appl. Phys. Lett., 101, 171603–171606 (2012).
14. 14) Y. Xiong, J. E. Smugeresky, A. Julie and M. Schoenung, Mat. Sci. Eng. A-Struct., 493, 261–266 (2008).
15. 15) S. Meyers, L. De Leersnijder, J. Vleugels and J.-P. Kruth, J. Eur. Ceram. Soc., 38, 3709–3717 (2018).
16. 16) S. Nakashima and H. Harima, Phys. Status Solidi A, 162, 39–64 (1997).10.1002/1521-396X(199707)162:1<39::AID-PSSA39>3.0.CO;2-L ↗
17. 17) S. Sorieul, J.-M. Costantini, L. Gosmain, L. Thomé and J.-J. Grob, J. Phys. Condens. Matter, 18, 5235–5251 (2006).