journal article·2020-05-01Open access

Fabrication and microstructures improvement of porous mullite ceramics based on sol-treated sawdust

Zhiyong HE

Abstract

Calcined flint clay has a large reserve in China. In this paper, porous mullite ceramics are prepared by calcined flint clay, while the sawdust is pretreated with different concentrations of silica sol. Effects of sintering temperature and silica sol concentrations on physical properties and microstructures of the porous mullite ceramics are studied. Residual skeleton structure cross pores are clearly observed in the scanning electron microscope images, which is established as a key factor in improving the properties of specimens. With the pretreatment of silica sol on sawdust, mechanical properties are enhanced and thermal conductivities could be optimized. Under the firing temperature of 1350 °C, the compressive strength of specimens with sawdust pretreated in 5 wt % concentration of silica sol is 2.4 MPa.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Central Iron & Steel Research Institute Group

References (22)

Show source-provided references
1. 1) A. Noor, F. Mahtab, M. Khan and G. Saeed, J. Clean. Prod., 129, 491–495 (2016).
2. 2) X. M. Li and M. J. Gao, Appl. Clay Sci., 132–133, 161–166 (2016).10.1016/j.clay.2016.05.029 ↗
3. 3) R. L. Fei and B. Q. Lin, Energy, 135, 865–875 (2017).10.1016/j.energy.2017.06.173 ↗
4. 4) C. N. Djangang, E. Kamseu, M. K. Ndikontar, L. N. Gisèle, J. Soro, U. C. Melo, A. Elimbi, P. Blanchart and D. Daniel Njopwouo, Mat. Sci. Eng. A-Struct., 528, 8311–8318 (2011).
5. 5) D. O. Obada, D. Dodoo-Arhin, M. Daud, F. O. Anafi, A. S. Ahmed and O. A. Ajayi, Appl. Clay Sci., 132–133, 194–204 (2016).10.1016/j.clay.2016.06.006 ↗
6. 6) H. Zouaoui and J. Bouaziz, Appl. Clay Sci., 150, 131–137 (2017).
7. 7) F. D. Santos, L. R. V. da Conceição, R. V. C. Leyvison, C. de Annie and F. Heizir, Appl. Clay Sci., 149, 41–50 (2017).
8. 8) M. Baptista, A. Kovalevsky, A. R. Sarabando, M. C. Ferro, I. Capela and J. R. Frade, Mater. Lett., 237, 41–44 (2019).
9. 9) N. N. Xu, S. J. Li, Y. B. Li, Z. L. Xue, L. Yuan, J. L. Zhang and L. Wang, Ceram. Int., 41, 5807–5811 (2015).
10. 10) P. Giorgio, L. G. Magdalena, C. Ludovica, P. Paola, D. Francesco and S. Cristina, Ceram. Int., 44, 16992–16998 (2018).
11. 11) M. M. Hoog Antink, L. Röpke and J. Bartels, Ceram. Int., 44, 16561–16571 (2018).
12. 12) M. Branko, B. Biljana, E. Adela, R. M. Ana, L. Vesna, S. Aleksandra and B. Snezana, Mater. Manuf. Process., 24, 1109–1113 (2009).
13. 13) K. N. Rafael, L. R. Priscila, G. N. Q. Mara and H. Dachamir, J. Eur. Ceram. Soc., 38, 988–1001 (2018).
14. 14) W. Cao, X. D. Cheng, L. L. Gong, Y. Li, R. F. Zhang and H. P. Zhang, Mater. Lett., 139, 66–69 (2015).
15. 15) I. Yakub, J. Du and W. O. Soboyejo, Mat. Sci. Eng. A-Struct., 558, 21–29 (2012).
16. 16) W. Yan, N. Li, B. Q. Han, J. Liu and G. P. Liu, T. Indian Ceram. Soc., 70, 65–69 (2013).
17. 17) Z. P. Wei, S. J. Li, Y. B. Li, X. S. Li, R. F. Xiang and N. N. Xu, Ceram. Int., 44, 22616–22621 (2018).
18. 18) M. Mizutani, H. Takase, N. Adachi, T. Ota, K. Daimon and Y. Hikichi, Sci. Technol. Adv. Mater., 6, 76–83 (2005).
19. 19) B. Francesco, Mater. Lett., 212, 12–15 (2018).
20. 20) Z. Li, K. F. Wang, B. L. Wang and S. L. Guo, Ceram. Int., https: //doi.org/10.1016/j.ceramint.2018.11.083.
21. 21) T. Ohji and M. Fukushima, Int. Mater. Rev., 57, 115–131 (2012).
22. 22) A. Pyzik, R. Ziebarth, C. H. Han and K. Yang, Int. J. Appl. Ceram. Tec., 8, 1059–1066 (2011).