journal article·2017Open access

An optical method for evaluating the degradation mechanism of a developing RuO2 thick film resistor element for power modules

Yoshinobu NAKAMURA, Yuki KITANAKA, Masaru MIYAYAMA, Takeshi ITO, Koichi URANO, Kiyoshi TANAKA, Tomohiko NAKAJIMA, Tetsuo TSUCHIYA

Abstract

We devised a simple and noninvasive method for evaluating the spacial distribution of local electron densities of a thick-film RuO2-based chip resistor using UV–VIS-IR reflectance microscopy. After a long-term durability test for 874 h under an elevated temperature of 623 K, RuO2 resistors were thermally damaged, and their resistance became more than 10% higher. We identified the thermally damaged region by this new method and found that the thermal degradation is mainly due to an increase in the resistance between the Ag electrode and the RuO2 resistor film.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electrical and Thermal Properties of Materials · Transition Metal Oxide Nanomaterials · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Applied Chemistry, Graduate School of Engineering, The University of Tokyo

KOA Corporation

Advanced Coating Technology Research Center, National Institute of Advanced Industrial Science and Technology

References (22)

Show source-provided references
1. 1) J. Millan, P. Godignon, X. Perpina, X. A. Perez-Tomas and J. Rebollo, IEEE Trans. Power Electron., 29, 2155–2163 (2014).10.1109/TPEL.2013.2268900 ↗
2. 2) K. Sheng, IEEE Trans. Electron Dev., 56, 337–342 (2009).10.1109/TED.2008.2010605 ↗
3. 3) P. A. Cox, Transition Metal Oxides —An introduction to their electronic structure and properties—, Oxford University Press, New York, USA (1992) p. 68.
4. 4) KOA, Inc. Online Product Catalog, URL: http://www.koaglobal.com/product/smd-resistor.
5. 5) K. L. Jiao, Q. X. Jia and W. A. Anderson, Thin Solid Films, 227, 59–65 (1993).10.1016/0040-6090(93)90187-T ↗
6. 6) S. Podda, G. C. Cassaneli, F. Fantini and M. Vanzi, Microelectron. Reliab., 44, 1763–1767 (2004).10.1016/j.microrel.2004.07.103 ↗
7. 7) E. H. Stevens, IEEE Trans. Parts Hybrids Packag., 12, 351–356 (1976).10.1109/TPHP.1976.1135152 ↗
8. 8) S. Kasukabe and M. Tanaka, Electrocomponent Sci. Tech. (Paris), 8, 167–174 (1981).10.1155/APEC.8.167 ↗
9. 9) Y. Taketa and M. Haradome, Microelectron. Reliab., 13, 281–289 (1974).10.1016/0026-2714(74)90107-3 ↗
10. 10) E. V. Jelenkovic, K. Y. Tong, W. Y. Cheung and S. P. Wong, Microelectron. Reliab., 43, 49–55 (2003).10.1016/S0026-2714(02)00274-3 ↗
11. 11) M. Tao, B. Ai, O. Dorlanne and A. Loubiere, J. Appl. Phys., 61, 1562–1567 (1987).10.1063/1.338091 ↗
12. 12) A. K. Goel, G. Skorinko and F. R. Pollak, Phys. Rev. B, 24, 7342–7350 (1981).10.1103/PhysRevB.24.7342 ↗
13. 13) H. Ehrenreich and H. R. Philipp, Phys. Rev., 128, 1622–1629 (1962).10.1103/PhysRev.128.1622 ↗
14. 14) J. Si and S. B. Desubakacha, J. Mater. Res., 8, 2644–2648 (1993).10.1557/JMR.1993.2644 ↗
15. 15) A. Belkind, Z. Orban, J. L. Vossen and J. A. Woollam, Thin Solid Films, 207, 242–247 (1992).10.1016/0040-6090(92)90131-T ↗
16. 16) G. Abdurakhmanov, G. S. Vakhidova and L. X. Tursunov, World J. Cond. Mat. Phys., 1, 1–5 (2011).10.4236/wjcmp.2011.11001 ↗
17. 17) A. B. Kuzmenko, Rev. Sci. Instrum., 76, 083108 (2005).10.1063/1.1979470 ↗
18. 18) Comprehensive Inorganic Chemistry, Ed. by J. C. Bailar, H. J. Emeleus, Sir Ronald Nyholmm and A. F. Trotman-Dickenson, Vol. 3, Pergamon Press, Oxford, UK (1973) p. 97.
19. 19) Z. Qu, M. Cheng, W. Huang and X. Bao, J. Catal., 229, 446–458 (2005).10.1016/j.jcat.2004.11.043 ↗
20. 20) A. Nagy and G. Mestl, Appl. Catal., 188, 337–353 (1999).10.1016/S0926-860X(99)00246-X ↗
21. 21) M. M. Steeves and R. J. Lad, J. Vac. Sci. Technol., A28, 906–911 (2009).10.1116/1.3273945 ↗
22. 22) R. Terai and H. Hayami, J. Non-Cryst. Solids, 18, 217–264 (1975).10.1016/0022-3093(75)90022-8 ↗