Synthesis of Zinc Gallate Spinel Nanoparticles by Hydrothermal Method in the Presence of Urea and Their Sintering.
Source abstract
Abstract
Nanometer-sized particles of zinc gallate (ZnGa2O4) spinel solid solutions over wide compositional range (Zn/Ga molar ratio = 0.341-0.499) were directly synthesized from aqueous solutions of gallium and zinc sulfates (Zn/Ga = 0.5-2.0) in the presence of urea under hydrothermal conditions at 120 to 240°C. Under almost neutral conditions in the presence of urea (pH = 7.65), zinc gallate spinel was hydrothermally formed over 200°C, although ZnCO3 and GaO(OH) were formed at 120°C. The synthesized temperature of zinc gallate spinel was able to decrease from 240 to 120°C, with the increase of the concentration of urea from 0.8 to 2.4 mol·dm-3. Zinc gallate spinel with almost stoichiometric composition (Zn/Ga = 0.499) was synthesized from the solution with Zn/Ga = 2 at 240°C. The obtained zinc gallate spinel powder was fully densified by sintering over 1200°C for 1 h.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Pigment Synthesis and Properties · ZnO doping and properties · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.