article·1993-01-01Open access

Microstructure and Mechanical Strength of TiO2-Doped Al2O3 Ceramics Fired in Vacuum Atmosphere

Chii-Shyang Hwang, Zenbe-e NAKAGAWA, Kenya HAMANO

Abstract

Microstructure and mechanical strength of Al2O3-TiO2 ceramics fired in vacuum were studied by X-ray powder diffractometry, scanning electron microscopy, and bending test method. Alumina powder compacts containing 0-4wt% TiO2 were sintered at 1500-1700°C in vacuum (10-3-10-4Pa) and then annealed at 1300°C in air. The solid solubility of TiO2 into Al2O3 increased with an increase in temperature in vaccum. Beyond the solid solubility limit, TiO2 or Al2TiO5 existed in alumina matrix and restrained the grain growth of alumina. Vacuum-sintered bodies which had high solubilities of Ti were annealed in air. Excess Ti ion existing in Al2O3 grains diffused to the grain boundary, and then to the surface of the sintered body, and the annealing treatment slightly decreased the bending strength of sintered bodies.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Additive Manufacturing and 3D Printing Technologies · Material Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.