Mechanical Properties of SiC Whisker-Reinforced TiB2 Composites Fabricated by Hot-Pressing
Source abstract
Abstract
SiC whisker reinforced TiB2 matrix composites containing 10 to 30vol% whisker were prepared by hotpressing at 1600 to 1900°C. The flexural strength of 867±77MPa and KIC of 5.8±0.12MPa√m were obtained for the 1800°C hot-pressed samples containing 10vol% whisker. No significant increase in KIC was observed by the whisker reinforcement because of the chemical reaction between matrix and whisker, which enhanced strong interfacial bonding and whisker agglomeration.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.