The Influence of Grain Size and Secondary Phase on the Fracture Toughness of Sintered MgO Bodies (Part 1)
Source abstract
Abstract
The influence of grain size and secondary phase on the fracture toughness KIC of sintered MgO bodies was investigated. Sintered MgO bodies doped with 1-10wt% Al2O3 were made by hot-pressing. The grain size was changed by annealing. The fracture toughness KIC was measured by a chevron-notched beam method. The fracture toughness of sintered MgO bodies doped with Al2O3 was independent of the grain size and the amount of Al2O3, and indicated a constant value of 2.2MPa√m, 20% larger than that of pure MgO. The fractography revealed that the toughening of Al2O3-doped MgO bodies corresponded to the increase in the fraction of stepwise transgranular fracture on the fracture surfaces. It was considered that the change in fracture mode resulted from residual thermal stresses generated near secondary phase particles (MgAl2O4).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.