Sintering of Si3N4 Ceramics in Air Atmosphere Furnace(Part 2)-Agglomeration of Packing Powder and Deterioration of Al2O3 Crucible-

Shigetaka WADA, Piyaporn CHAIYAPAK, Supatra Jinawath, Thanakorn Wasanapiarnpong, Toyohiko Yano

Abstract

Si3N4 ceramics were sintered at temperature range of 1550-1700°C in an air atmosphere furnace using an Al2O3 crucible, Si3N4 packing powder and Al2O3 filler. Si3N4 packing powder and Al2O3 filler tended to agglomerate. It was found that coarse SN-F2 packing powder was the best candidate when process cost was considered and Al2O3 powder larger than 1-2 μm did not agglomerate even at 1700°C. Additionally, an Al2O3 crucible filled with Si3N4 powder is deteriorated and cracked after only several times using. Nevertheless, Si3N4 ceramic could be sintered to full density reproducibly. However, its mechanical strength was not high enough, and both the strength and the deterioration of crucible should be further improved.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.