article·1994-01-01Open access

Development of Solidification Technique for Recycle of Concrete Wastes by Hydrothermal Hot-Pressing and Its Mechanical Property

Yuji Nakane, Kazushi Sato, Hideaki Takahashi, Nakamichi Yamasaki, Toshiyuki Hashida

Abstract

A new processing method for solidifying pulverized concrete wastes is presented. The objective of this study was to develop a technology to recycle concrete wastes. Concrete wastes were pulverized and then solidified by a hydrothermal hot-pressing method, which is a press-forming technique under hydrothermal conditions using an autoclave. The reaction temperature was in the range of 120 to 300°C, and the reaction time was in the range of 10 to 40min. The tensile strength of the solidified concrete waste was determined by a Brazilian test. It was shown that concrete waste can be solidified under the above reaction conditions. The measured tensile strength increased with increasing temperature, and a steep increase was observed at the reaction temperatures of 150 to 200°C. The tensile strength of 5MPa was achieved above 200°C. The steep increase in the tensile strength was shown to be due to the formation of tobermorite.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycled Aggregate Concrete Performance · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.