article·1992-01-01Open access

Preparation and Thermal Expansion Behavior of Excess SiO2 Pollucite Powders

Hidehiko Kobayashi, Toshihiro Terasaki, Toshiyuki Mori, Hiroshi Yamamura, Takashi MITAMURA

Abstract

Pollucite powders of single phase containing excess SiO2 have been prepared from CsNO3, Al2O3 sol and SiO2 sol by a sol-gel processing. Behaviors of the thermal expansion of these powders have been also studied. As a result of the research for synthesis of the pollucite powders (Cs2O:SiO2:Al2O3 (molar ratio)=1:4.5-5:1), the two-stage heat treatment was the most effective: after the dried samples prepared by the solgel process were heated at 600°C for 24h and were subsequently heated at 750°C for 10h, then the powders were calcined at 1000°C for 50h. The synthesized pollucite powders of single phase containing excess SiO2 showed a low thermal expansion from room temperature to 200°C. Furthermore, it is revealed that the range of temperature showing the thermal expansion less than 0.1% was extended up to 600°C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Zeolite Catalysis and Synthesis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.