Cohesive Energy of Interfaces and Toughness of Fluorine-Doped Si3N4/SiC Composites
Source abstract
Abstract
Fracture mechanics and electron microscopy studies were systematically conducted on a dense Si3N4 material reinforced with high-aspect-ratio SiC platelets. This model system contained only an amorphous SiO2 phase at the multigrain pockets and along the internal interfaces. Two different procedures (and their empirical combination) were followed to gradually weaken the grain interfaces and, hence, deliberately change the fraction of intergranular fracture within the material upon crack propagation. These procedures were: 1) the gradual addition of a fluorine impurity, which remains segregated at the grain boundaries after sintering, and 2) the adoption of a “quenching” process under high pressure. Quantitative high-resolution and analytical electron microscopy provided fundamental insight into the internal structure of the intergranular SiO2 phase doped with fluorine and the corresponding microcracking processes. Quantitative fractography allowed to estimate the apparent cohesive energy of the internal interfaces of the composite and to relate it to the macroscopic material toughness.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.