article·1997-01-01Open access

Strengthening of Hydrothermal Hot-Pressed Concrete Waste by the Addition of Slag

Kazuhiko Sato, Toshiyuki Hashida, Hideaki Takahashi, Nakamichi Yamasaki

Abstract

This paper discusses the effect of addition of granulated blast furnace slag on the tensile strength of solidified concrete wastes using a hydrothermal hot-pressing method. Blast furnace slag of 0-100mass% was added to the concrete waste and NaOH solution was used as alkali-activator. Hydrothermal hot-pressing tests were carried out at 250°C with the water content of 10-30mass% under the pressure of 20MPa, The tensile strength of solidified bodies was determined by Brazilian test. It was shown that the formation of tobermorite and C-S-H compound improved the strength. The tensile strength reached at 13MPa under the following conditions; slag content: 50mass%, water content: 20mass%, NaOH addition: 1.75mass%.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Recycled Aggregate Concrete Performance · Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.